The effects of phase transformation on the structure and mechanical properties of TiSiCN nanocomposite coatings deposited by PECVD method
Source abstract
Abstract
Abstract In the present study, the effects of phase transformations on the structure and mechanical properties of TiSiCN coatings were investigated. TiSiCN nanocomposite coatings were deposited on AISI H13 hot-work tool steel by a pulsed direct current plasma-enhanced chemical vapor deposition process at 350 or 500 °C, using TiCl4 and SiCl4 as the precursors of Ti and Si, respectively, in a CH4/N2/H2/Ar plasma as the source of carbon and nitrogen and reducing environment. Some samples deposited at 350 °C were subsequently annealed at 500 °C under Ar atmosphere. Super hard self-lubricant TiSiCN coatings, having nanocomposite structure consisting of TiCN nanocrystals and amorphous carbon particles embedded in an amorphous SiCNx matrix, formed through spinodal decomposition in the specimens deposited or annealed at 500 °C. In addition, it was revealed that either uncomplete or relatively coarse phase segregation of titanium compounds was achieved during deposition at 350 °C and 500 °C, respectively. On the contrary, by deposition at 350 °C followed by annealing at 500 °C, a finer structure was obtained with a sensible improvement of the mechanical properties of coatings. Accordingly, the main finding of this work is that significant enhancement in key properties of TiSiCN coatings, such as hardness, adhesion and friction coefficient, can be obtained by deposition at low temperature and subsequent annealing at higher temperature, thanks to the formation of a fine grained nanocomposite structure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Transition metal nitride-based nanolayered multilayer coatings and nanocomposite coatings as novel superhard materials
2. Hard nanocomposite coatings: thermal stability, oxidation resistance and toughness10.1016/j.surfcoat.2012.05.073 ↗
3. Mechanical and tribological properties of nanocomposite TiSiN coatings10.1016/j.surfcoat.2009.11.034 ↗
4. Influence of Si content on Nano-structured Ti–Si–N films coated by pulsed-dc plasma enhanced CVD10.1016/j.surfcoat.2003.10.057 ↗
5. Improving the wear and corrosion resistance of Ti–6Al–4V alloy by deposition of TiSiN nanocomposite coating with pulsed-DC PACVD10.1016/j.wear.2017.07.009 ↗
6. Microstructure and mechanical properties of Ti-Si-CN films synthesized by plasma-enhanced chemical vapor deposition10.1016/j.surfcoat.2007.05.073 ↗
7. Ternary and quarternary TiSiN and TiSiCN nanocomposite coatings obtained by chemical vapor deposition10.1016/j.surfcoat.2012.10.067 ↗
8. Synthesis and characterization of super hard, self-lubricating Ti–Si–C–N nanocomposite coatings10.1016/j.actamat.2007.07.046 ↗
9. On the oxidation resistance of superhard Ti–Si–C–N coatings10.1557/jmr.2008.0293 ↗
10. Effect of ion bombardment on structural, mechanical, erosion and corrosion properties of Ti–Si–C–N nanocomposite coatings10.1016/j.surfcoat.2014.09.006 ↗
11. Development and evaluation of low friction TiSiCN nanocomposite coatings for piston ring applications10.1016/j.surfcoat.2016.04.061 ↗
12. A concept for the design of novel superhard coatings10.1016/0040-6090(95)06695-0 ↗
13. Different approaches to superhard coatings and nanocomposites10.1016/j.tsf.2004.10.053 ↗
14. Avoiding the high-temperature decomposition and softening of (Al1−xTix) N coatings by the formation of stable superhard nc-(Al1−xTix)N/a-Si3N4 nanocomposite10.1016/j.msea.2003.08.052 ↗
15. Study of the structural and mechanical properties of nanocrystalline TiAlSiN gradient coatings10.4028/www.scientific.net/JNanoR.27.15 ↗
16. Plasma-enhanced chemical vapor deposition of functional coatings
17. Thermal stability of diamond-like carbon films with added silicon10.1016/S0257-8972(98)00719-1 ↗
18. Relative hydrogen content in plasma-enhanced CVD silicon nitride films: substrate temperature dependence and effect of thermal annealing10.1002/pssa.2210890154 ↗
19. Voevodin · 2006
20. Single-step, rapid low-temperature synthesis of Si quantum dots embedded in an amorphous SiC matrix in high-density reactive plasmas10.1016/j.actamat.2009.09.034 ↗
21. Synthesis of tubular silicon carbide (SiC) from a carbon–silica material by using a reactive replica technique: mechanism of formation of SiC10.1016/j.actamat.2003.12.033 ↗
22. Structural and optical properties of amorphous hydrogenated silicon carbonitride films produced by PECVD10.1016/j.apsusc.2005.10.017 ↗
23. Ultrathin TiSiN overcoat protection layer for magnetic media10.1116/1.3607423 ↗
24. XRD and FTIR analysis of Ti–Si–C–ON coatings for biomedical applications10.1016/j.surfcoat.2008.06.121 ↗
25. Physical deposition of carbon doped titanium nitride film by DC magnetron sputtering for metallic implant coating use10.1016/j.apsusc.2014.01.010 ↗
26. Diamond-like amorphous carbon10.1016/S0927-796X(02)00005-0 ↗
27. Raman spectroscopy as a tool to study cubic Ti–C–N CVD coatings10.1016/j.surfcoat.2009.05.029 ↗
28. Structural transformations in TiAlSiCN coatings in the temperature range 900–1600 °C10.1016/j.actamat.2014.10.007 ↗
29. A comparative study of salt-bath nitrocarburizing and gas nitriding followed by post-oxidation used as surface treatments of H13 hot forging dies10.1016/j.surfcoat.2016.08.003 ↗
30. The formation and role of interfaces in superhard nc-MenN/a-Si3N4 nanocomposites10.1016/j.surfcoat.2006.08.112 ↗
31. On the spinodal nature of the phase segregation and formation of stable nanostructure in the Ti–Si–N system10.1016/j.msea.2006.03.017 ↗
32. Effect of substrate temperature and input power on TiN film deposition by low-frequency (60 Hz) PECVD
33. Orhing · 2001
34. Porter · 2009