journal article·2021-12

Mechanical properties evolution of SiCf/SiC composites with a BN/SiC multilayer interface oxidized at elevated temperature

Guang-Yuan Cui, Rui-Ying Luo, Lian-Yi Wang, Peng Huang, Jia-Qi Song, Jin-Sen Wang

Publisher page

Abstract

Abstract In this study, the mechanical properties of SiCf/SiC composites with a BN/SiC multilayer interface was evaluated after oxidized at 800 °C, 1100 °C and 1400 °C for 200 h. The damage evolution of the fabricated and oxidized composites were analyzed by acoustic emission techniques. The chemical composition and structural evolution of the SiCf/SiC composites after oxidation were observed by X-ray diffraction, X-ray photoelectron spectroscopy, scanning electron microscopy and energy dispersive spectroscopy. Significant temperature-dependent strength degradation of the SiCf/SiC composites was observed. The results indicated that the interfacial microstructure change caused by oxidation had a significant impact on the damage process of the composites, and two different degradation mechanisms for oxidized composites are discussed. The toughening mechanism of crack deflection and fiber pull out failed after oxidation at 800 °C. The degradation of the mechanical properties after oxidation at 1100 and 1400 °C was attributed to the hysteresis of fiber breakage caused by weak interface bonding. This work could predict the service life of SiCf/SiC composites and contribute to their early application in aerospace.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Development of high tensile strength silicon carbide fibre using an organo-silicon polymer precursor: Yajima, S., Hasegawa, Y., Okamura, K. and Matsuzawa, T. Nature Vol 273 (15 June 1978) p 525, Composites 10(1) (1979) 45.10.1016/0010-4361(79)90363-X ↗
2. SiC-Matrix Composites: Nonbrittle Ceramics for Thermo-Structural Application10.1111/j.1744-7402.2005.02009.x ↗
3. Enhanced oxidation resistance of SiC/SiC minicomposites via slurry infiltration of oxide layers10.1016/j.jeurceramsoc.2017.03.065 ↗
4. Microstructural evolution and mechanical property of a SiCf/SiC composite/Ni-based superalloy joint brazed with an Au-Cu-Ti filler10.1016/j.jeurceramsoc.2020.08.065 ↗
5. Degradation of a SiC-SiC composite in water vapor environments10.1111/jace.16838 ↗
6. Cyclic-Dependent Damage Evolution in Self-Healing Woven SiC/[Si-B-C] Ceramic-Matrix Composites at Elevated Temperatures10.3390/ma13061478 ↗
7. Fracture mechanisms for SiC fibers and SiC/SiC composites under stress-rupture conditions at high temperatures
8. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
9. Toughness assessment of ceramic matrix composites10.1016/0266-3538(90)90102-B ↗
10. A.G. Evans, D.B. Marshall, Overview no. 85 The mechanical behavior of ceramic matrix composites, Acta Metallurgica 37(10) (1989) 2567-2583.10.1016/0001-6160(89)90291-5 ↗
11. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
12. Influences of the dip-coated BN interface on mechanical behavior of PIP-SiC/SiC minicomposites
13. Microstructure and mechanical performance of SiCf/BN/SiC mini-composites oxidized at elevated temperature from ambient temperature to 1500 °C in air10.1016/j.jeurceramsoc.2019.04.013 ↗
14. Oxidation resistance of NITE-SiC/SiC composites with/without CVD-SiC environmental barrier coating10.1016/j.ceramint.2018.06.194 ↗
15. Effect of interface type on the static and dynamic mechanical properties of 3D braided SiCf/SiC composites10.1016/j.msea.2016.05.080 ↗
16. SiC/SiC minicomposites with structure-graded BN interphases10.1016/S0955-2219(00)00064-9 ↗
17. Oxidation behavior and protection of carbon/carbon composites10.1016/0008-6223(87)90197-7 ↗
18. Oxidation resistance of SiCf/SiC composites with a PyC/SiC multilayer interface at 500 °C to 1100°C10.1016/j.corsci.2020.108522 ↗
19. High-Temperature Oxidation of Boron Nitride: I, Monolithic Boron Nitride10.1111/j.1551-2916.1999.tb20075.x ↗
20. Tensile Stress Rupture of SiCf/SiCmMinicomposites with Carbon and Boron Nitride Interphases at Elevated Temperatures in Air10.1111/j.1151-2916.1997.tb03087.x ↗
21. Boron Nitride Interphase in Ceramic-Matrix Composites10.1111/j.1151-2916.1991.tb06789.x ↗
22. J. Dai, Y. Wang, Z. Xu, R. Mu, W. Liu, L. He, Effect of BN/SiC interfacial coatings on the tensile properties of SiC/SiC minicomposites fabricated by PIP, Ceramics International 46(16, Part A) (2020) 25058-25065.10.1016/j.ceramint.2020.06.292 ↗
23. Mechanical properties of SiCf/SiC composites with alternating PyC/BN multilayer interfaces10.1080/17436753.2017.1339517 ↗
24. Effects of BN/SiC dual-layer interphase on mechanical and dielectric properties of SiCf/SiC composites10.1016/j.ceramint.2013.09.091 ↗
25. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
26. Microstructure and damage evolution of SiCf/PyC/SiC and SiCf/BN/SiC mini-composites: A synchrotron X-ray computed microtomography study10.1016/j.ceramint.2019.03.004 ↗
27. Oxidation and microstructure of SiCf/SiC composites in moist air up to 1600°C by X-ray tomographic characterization10.1111/ijac.13450 ↗
28. A novel strategy to prepare BN interface and its effects on microstructure and properties of SiCw/BN/SiC composites10.1016/j.jallcom.2020.158218 ↗
29. Oxidation of BN/Nicalon Fiber Interfaces in Ceramic-Matrix Composites and Its Effect on Fiber Strength10.1111/j.1151-2916.1999.tb02271.x ↗
30. Effect of oxidation treatment on KD–II SiC fiber–reinforced SiC composites10.1016/j.ceramint.2017.05.001 ↗
31. Mechanical and dielectric properties of SiCf/BN/SiBCN composites via different synthesis technologies10.1016/j.jeurceramsoc.2019.05.033 ↗
32. Borosilicate Glass-Induced Fiber Degradation of SiC/BN/SiC Composites Exposed in Combustion Environments10.1111/ijac.12499 ↗
33. Oxidation/corrosion of BN-based coatings as prospective interphases for SiC/SiC composites10.1016/j.jeurceramsoc.2020.07.056 ↗
34. F. Rebillat, X. Martin, E. Garitte, A. Guette, Overview on the Self-Sealing Process in the SiCF/[SI,C,B]M Composites under Wet Atmosphere at High Temperature, Design, Development, and Applications of Engineering Ceramics and Composites (2010) 151-166.10.1002/9780470909836.ch14 ↗
35. Oxidation resistance of hot-pressed SiC–BN composites10.1016/j.ceramint.2006.10.010 ↗
36. Influence of h-BN as additive on microstructure and oxidation mechanism of C/C-SiC composite10.1016/j.jeurceramsoc.2019.06.032 ↗
37. High-temperature flexural properties of SiBC modified C/SiC composites10.1016/j.ceramint.2013.11.072 ↗
38. X.g. Luan, Y. Zou, X. Hai, H. Bai, Q. Zhang, R. Riedel, L. Cheng, Degradation mechanisms of a self-healing SiC(f)/BN(i)/[SiC-B4C](m) composite at high temperature under different oxidizing atmospheres, Journal of the European Ceramic Society 38(11) (2018) 3804-3813.10.1016/j.jeurceramsoc.2018.05.001 ↗
39. Study on interfacial debonding stress and damage mechanisms of C/SiC composites using acoustic emission10.1016/j.ceramint.2020.10.013 ↗
40. Identification of damage mechanisms of carbon fiber reinforced silicon carbide composites under static loading using acoustic emission monitoring10.1016/j.ceramint.2019.04.082 ↗
41. Acoustic emission and electrical resistance in SiC-based laminate ceramic composites tested under tensile loading10.1016/j.jeurceramsoc.2017.05.003 ↗