journal article·2021-06

Blister formation in He-H co-implanted InP: A comprehensive atomistic study

N. Daghbouj, Jiajie Lin, H.S. Sen, M. Callisti, Bingsheng Li, M. Karlik, T. Polcar, Zhenghao Shen, Min Zhou, Tiangui You, Xin Ou

Publisher page

Abstract

Abstract The blistering efficiency in He-H-ions co-implanted and annealed InP has been found to peak and vanish in a narrow range of ion fluence ratio (ΦH/ΦHe = 1.5–3.5) with a fixed He fluence of 2 × 1016 He+/cm2. The blisters are formed at low fluence (ΦH/ΦHe = 1.5), peaked in the middle (ΦH/ΦHe = 2.5), and disappeared at the high fluence ratio (ΦH/ΦHe = 3.5). To get a fundamental understanding of blister formation in nanoscale, the defect profiles were studied by various experimental techniques combined with FEM and ab-initio simulations. Cross-section TEM images showed that at a low fluence ratio, He and H are stored in microcracks and bubbles whereas, at a high fluence ratio, the ions are trapped only inside bubbles. These atomic processes that occur during and after co-implantation and annealing are presented together with detailed scenarios in an attempt to explain our results. Based on DFT simulations, the de-trapping of He atoms from the small clusters is energetically cheaper compared to the migration of He from the large clusters formed at high fluence. Moreover, at a high fluence ratio, the presence of large clusters inhibits the He diffusion to the small clusters (precursor of blisters) by capturing migrating He atoms.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (81)

Show source-provided references
1. Wafer-scale heterogeneous integration InP on trenched Si with a bubble-free interface10.1063/5.0004427 ↗
2. Calculated spin-orbit splitting of all diamond-like and zinc-blende semiconductors: Effects of p1∕2 local orbitals and chemical trends10.1103/PhysRevB.70.035212 ↗
3. Optical properties of BP, BAs and BSb compounds under hydrostatic pressure10.1016/j.physb.2005.06.018 ↗
4. Simulation of optical function for phosphide crystals following the DFT band structure calculations
5. High-transconductance InAs/AlSb heterojunction field-effect transistors with delta-doped AlSb upper barriers10.1109/55.144998 ↗
6. Molecular-dynamics prediction of the thermal conductivity of thin InP nanowires: similarities to Si10.1103/PhysRevB.80.155408 ↗
7. Transfer of InP epilayers by wafer bonding10.1016/j.jcrysgro.2004.04.053 ↗
8. Szentpali, Evaluation of InP-to-silicon heterobonding10.1016/S0921-5107(00)00626-7 ↗
9. Indium phosphide on silicon heteroepitaxy: lattice deformation and strain relaxation10.1063/1.346386 ↗
10. Silicon on insulator material technology10.1049/el:19950805 ↗
11. The influence of ion-implantation damage on hydrogen-induced ion-cut10.1016/S0168-583X(00)00540-1 ↗
12. M. Ionescu, A. Deslandes, R. Holmes, M. C. Guenette, I. Karatchevtseva, and G. R. Lumpkin, Effect of annealing upon retention of He and H in irradiated SiC, Mater. Sci. Forum 879, 810–814 ISSN: 1662 (2016).10.4028/www.scientific.net/MSF.879.810 ↗
13. Fabrication of thin body InAs-on-insulator structures by Smart Cut method with H+ implantation at room temperature10.7567/1347-4065/aafa68 ↗
14. Silicon exfoliation by hydrogen implantation: actual nature of precursor defects10.1016/j.nimb.2017.04.033 ↗
15. Impact of the transient formation of molecular hydrogen on the microcrack nucleation and evolution in H-implanted Si (001)10.1063/1.2829807 ↗
16. Damage microstructure evolution of helium ion irradiated SiC under fusion relevant temperatures10.1016/j.jeurceramsoc.2018.04.060 ↗
17. In situ Observation of microstructure Evolution in 4H–SiC under 3.5 keV He Irradiation10.1016/j.jnucmat.2016.01.017 ↗
18. Kinetic aspects of the growth of hydrogen induced platelets in SiC10.1063/1.373556 ↗
19. Wafer-scale 4H-silicon carbide-on-insulator (4H–SiCOI) platform for nonlinear integrated optical devices10.1016/j.optmat.2020.109990 ↗
20. Freestanding ultrathin single crystalline SiC substrate by MeV H ion-slicing10.1063/1.5025889 ↗
21. Study of surface exfoliation on 6H-SiC induced by H2+ implantation10.1016/j.physb.2016.12.027 ↗
22. Vegard’s-law-like dependence of the activation energy of blistering on the x composition in hydrogenated a-SixGe1-x10.1016/j.jallcom.2018.05.269 ↗
23. H. Shi, K. Huang, F. Mu, T. You, Q. Ren, J. Lin, W. Xu, T. Jin, H. Huang, A. Yi, S. Zhang, Z. Li, M. Zhou, J. Wang, K. Xu, and X. Ou, Realization of wafer-scale single-crystalline GaN film on CMOS-compatible Si(100) substrate by ion cutting technique, Semicond. Sci. Technol. (2020) in press.10.1088/1361-6641/abb073 ↗
24. Investigation of hydrogen implantation induced blistering in GaN
25. Investigation on thermodynamics of ion-slicing of GaN and heterogeneously integrating high-quality GaN films on CMOS compatible Si(100) substrates10.1038/s41598-017-15094-1 ↗
26. Lattice modification in KTiOPO4 by hydrogen and helium sequentially implantation in submicrometer depth10.1063/1.4949529 ↗
27. Effects of hydrogen implantation temperature on InP surface blistering10.1063/1.2926682 ↗
28. A. Fontcuberta i Morral, J. M. Zahler, M. J. Griggs, Harry A. Atwater, and Y. J. Chabal, Spectroscopic studies of the mechanism for hydrogen-induced exfoliation of InP, Phys. Rev. B 72, 085219 (2005).10.1103/PhysRevB.72.085219 ↗
29. the Phenomenology of ion implantation-induced blistering and thin-layer splitting in compound semiconductors10.1007/s11664-010-1334-x ↗
30. Temperature dependence of hydrogen-induced exfoliation of InP10.1063/1.1773367 ↗
31. Investigation of helium implantation induced blistering in InP10.1016/j.jlumin.2006.08.073 ↗
32. Low temperature InP layer transfer onto Si by helium implantation and direct wafer bonding10.1088/0268-1242/21/9/016 ↗
33. Efficient production of silicon-on-insulator films by co-implantation of He+ with H+10.1063/1.120945 ↗
34. On the microstructure of Si coimplanted with H+ and He+ ions at moderate energies10.1063/1.122875 ↗
35. Reboh · J. Appl. Phys. · 2010 · 108 · 02350210.1063/1.3459884 ↗
36. The mechanisms of surface exfoliation in H and He implanted Si crystals10.1016/j.scriptamat.2011.09.012 ↗
37. N. Daghbouj, Ph.D. thesis, University Toulouse III-Paul Sabatier, (2016).
38. The effect of order and dose of H and He sequential implantation on defect formation and evolution in silicon10.1063/1.2432380 ↗
39. N. Daghbouj, N. Cherkashin, F.-X. Darras, V. Paillard, M. Fnaiech, and A. Claverie, Effect of the order of He+ and H+ ion co-implantation on damage generation and thermal evolution of complexes, platelets, and blisters in silicon, J. Appl. Phys. 119, 135308 (2016).10.1063/1.4945032 ↗
40. Impact of He and H relative depth distributions on the result of sequential He+ and H+ ion implantation and annealing in silicon10.1063/1.5012505 ↗
41. Microstructural evolution of helium-implanted 6H-SiC subjected to different irradiation conditions and annealing temperatures: a multiple characterization study10.1016/j.actamat.2019.09.027 ↗
42. The structural evolution of light-ion implanted 6H-SiC single crystal: comparison of the effect of helium and hydrogen10.1016/j.actamat.2020.02.046 ↗
43. Localized exfoliation versus delamination in H and He coimplanted (001) Si10.1063/1.3116738 ↗
44. Study of hydrogen implantation-induced blistering in GaSb for potential layer transfer applications10.1088/1361-6463/aa7522 ↗
45. Diffusion and impurity segregation in hydrogen-implanted silicon carbide10.1063/1.4882996 ↗
46. 6H-SiC blistering efficiency as a function of the hydrogen implantation fluence10.1016/j.apsusc.2018.10.005 ↗
47. Temperature dependence of blistering in hydrogen implanted Si and Ge10.1016/j.nimb.2012.10.037 ↗
48. Kinetic evolution of blistering in hydrogen-implanted silicon10.1063/1.4813858 ↗
49. F. I. Allen, P. Hosemann, and M. Balooch, Key mechanistic features of swelling and blistering of helium-ion-irradiated tungsten, Scr Mater. 178, 256 (2020).10.1016/j.scriptamat.2019.11.039 ↗
50. Lattice swelling and modulus change in a helium-implanted tungsten alloy: X-ray micro-diffraction, surface acoustic wave measurements, and multiscale modelling10.1016/j.actamat.2015.01.055 ↗
51. EBSD characterization of hydrogen induced blisters and internal cracks in TRIP-assisted steel10.1016/j.matchar.2019.110029 ↗
52. Helium-ion microscopy, helium-ion irradiation and nanoindentation of Eurofer 97 and ODS Eurofer10.1016/j.jnucmat.2017.07.054 ↗
53. Cracks and blisters formed close to a silicon wafer surface by He-H co-implantation at low energy10.1063/1.4938108 ↗
54. Efficient ion-slicing of InP thin film for Si based hetero-integration10.1088/1361-6528/aae281 ↗
55. J. F. Ziegler and J. P. Biersack, “SRIM computer code,” see http:// www.srim.org (2008).
56. Threshold energy for atomic displacement in InP10.1103/PhysRevB.34.2470 ↗
57. Modelling of point defect complex formation and its application to H+ ion implanted silicon10.1016/j.actamat.2015.07.078 ↗
58. The amorphization of 3C-SiC irradiated at moderately elevated temperatures as revealed by X-ray diffraction10.1016/j.actamat.2017.08.030 ↗
59. S. A. Stepanov, 2007, see http://sergey.gmca.aps.anl.gov/gid_sl.html.
60. A method to determine the pressure and densities of gas stored in blisters: application to H and He sequential ion implantation in silicon10.1016/j.mee.2018.01.006 ↗
61. Inhomogeneous electron gas10.1103/PhysRev.136.B864 ↗
62. Self-consistent equations including exchange and correlation effects10.1103/PhysRev.140.A1133 ↗
63. Ab initio molecular dynamics for liquid metals10.1103/PhysRevB.47.558 ↗
64. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set10.1016/0927-0256(96)00008-0 ↗
65. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
66. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
67. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
68. Vacancy-interface-helium interaction in Zr-Nb multi-layer system: A first-principles study10.1016/j.jnucmat.2019.02.030 ↗
69. N. Daghbouj, M. Callisti, H.S. Sen a, M. Karlik, J. Cech, M. Vronka, V. Havránek, J. Capek, P. Minárik, P. Bábor, T. Polcar, Interphase boundary layer-dominated strain mechanisms in Cu+ implanted Zr-Nb nanoscale multilayers, Acta Mater. 202, 317–330 (2021).10.1016/j.actamat.2020.10.072 ↗
70. S. Reboh, F. Schaurich, A. Declemy, J. F. Barbot, M. F. Beaufort, N. Cherkashin, and P. F. P. Fichtner, On the microstructure of Si coimplanted with H+ and He+ ions at moderate energies, J. Appl. Phys. 108, 023502 (2010).10.1063/1.3459884 ↗
71. F. P. Luce, S. Reboh, E. Vilain, F. Madeira, J. P. Barnes, N. Rochat, T. Salvetat, A. Tauzin, F. Milesi, F. Mazen, and C. Deguet, Influence of Implantation Temperature on the Formation of Hydrogen-Related Defects in InP, proc of IIT n° 6939972, (2014).10.1109/IIT.2014.6939972 ↗
72. Synergistic effects of high energy helium irradiation and damage introduction at high temperature on hydrogen isotope retention in plasma facing materials10.1016/j.jnucmat.2020.152122 ↗
73. Variation of the polarizability of noble gases with density10.1063/1.433839 ↗
74. Brillouin measurements of solid n-H2 and n-D2 to 200 kbar at room temperature10.1103/PhysRevLett.47.128 ↗
75. A lower bound on implant density to induce wafer splitting in forming compliant substrate structures10.1063/1.119219 ↗
76. Thermodynamic model of helium and hydrogen co-implanted silicon surface layer splitting10.1016/j.nimb.2009.12.009 ↗
77. Nanomechanical characterization of cavity growth and rupture in hydrogen implanted single-crystal BaTiO310.1063/1.1885183 ↗
78. Mechanics of tungsten blistering II: Analytical treatment and fracture mechanical assessment10.1016/j.jnucmat.2015.07.007 ↗
79. Heterogeneous Integration of Compound Semiconductors10.1146/annurev-matsci-070909-104448 ↗
80. Evaluation of the surface bonding energy of an InP membrane bonded oxide-free to Si using instrumented nanoindentation10.1063/1.4817675 ↗
81. Hardness and fracture toughness of semiconducting materials studied by indentation and erosion techniques10.1016/0025-5416(88)90489-2 ↗