Effects of copper-plasma deposition on weathering properties of wood surfaces

P. Gascón-Garrido, N. Mainusch, H. Militz, W. Viöl, C. Mai

Publisher page

Abstract

Abstract Thin layers of copper micro-particles were deposited on the surfaces of Scots pine ( Pinus sylvestris L.) micro-veneers using atmospheric pressure plasma to improve the resistance of the surfaces to weathering. Three different loadings of copper were established. Micro-veneers were exposed to artificial weathering in a QUV weathering tester for 0, 24, 48, 96 and 144 h following the standard EN 927-6 [1] . Mass losses after each exposure showed significant differences between copper coated and untreated micro-veneers. Tensile strength was assessed at zero span (z-strength) and finite span (f-strength) under dry conditions (20 °C, 65% RH). During 48 h, micro-veneers lost their z-strength progressively. In contrast, copper coating at highest loading imparts a photo-protective effect to wood micro-veneers during 144 h exhibiting z-strength retention of 95%. F-strength losses were similar in all copper treated and untreated micro-veneers up to 96 h. However, after 144 h, copper coated micro-veneers at highest loading showed significantly greater strength retention of 56%, while untreated micro-veneers exhibited only 38%. Infrared spectroscopy suggested that copper coating does not stabilize lignin. Inductively Coupled Plasma revealed that micro-veneers coated with the highest loading exhibited the lowest percentage of copper loss. Blue stain resistance of copper coated Scots pine following the guidelines of EN 152 [2] was performed. Additional test with different position of the coated surface was also assessed. Copper coating reduced fungal growth when coated surface is exposed in contact with vermiculite. Spores of Aureobasidium pullulans were not able to germinate on the copper coated surface positioned uppermost.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Wood Treatment and Properties · Plant Pathogens and Fungal Diseases · Plant Surface Properties and Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (79)

Show source-provided references
1. EN 927-6 · 2006
2. EN 152 · 2012
3. Weathering of wood
4. Depth profiling of photo-induced degradation in wood by FT-IR microspectroscopy10.1007/BF00766722 ↗
5. Measuring penetration of light into wood by detection of photo-induced free radicals
6. Chemistry of weathering protection
7. Photochemical degradation of acetylated, methylated, phenylhydrazine-modified, and ACC-treated wood10.1002/app.1984.070290111 ↗
8. Light absorbing properties of pulp and pulp components
9. Weathering and photochemistry of wood
10. Reduction of weathering degradation of wood through plasma-polymer coating10.1515/HF.1999.104 ↗
11. Eaton · 1993
12. Growth of Aureobasidium pullulans on lignin breakdown products at weathered wood surfaces10.1016/S0269-915X(97)80095-X ↗
13. Studies on the colouring matter of blue-stain fungi. Part 2. Electron microscopic observations of the hyphae walls10.1515/hfsg.1989.43.6.371 ↗
14. Zabell · 1992
15. Schmidt · 2006
16. Banov · 1973
17. Feist · 1983
18. Bowne · 1962
19. Rabek · 1990
20. Review of the weathering and photostability of modified wood10.1080/17480270903249391 ↗
21. Black · 1974
22. Photodegradation and photoprotection of wood surfaces
23. Application of ESCA to evaluate wood and cellulose surfaces modified by aqueous chromium trioxide treatment10.1016/0166-6622(84)80167-5 ↗
24. Liu · 1994
25. Wood surface protection with some titanium, zirconium and manganese compounds10.1016/S0141-3910(03)00193-9 ↗
26. Effect of accelerated weathering on surface chemistry of modified wood10.1016/j.apsusc.2006.12.005 ↗
27. Weathering of copper-amine treated wood10.1016/j.apsusc.2009.08.071 ↗
28. Do the unique properties of nanometals affect leachability or efficacy against fungi and termites?10.1016/j.ibiod.2009.01.007 ↗
29. Toxicity and carcirogenicity of Cr(VI) in animal models and humans10.3109/10408449709078442 ↗
30. Evaluation of biocidal efficacy of copper alloy coatings in comparison with solid metal surfaces: generation of organic copper phosphate nanoflowers10.1111/jam.12094 ↗
31. Kartal · 2013
32. Yasuda · 1985
33. Introduction to plasmas
34. Plasma treatment of wood
35. Plasma treatment of wood
36. Wood surface modification in dielectric barrier discharges at atmospheric pressure10.1016/S0257-8972(03)00372-4 ↗
37. Modification of wood using a glow-discharge plasma derived from water
38. Pinus pinaster surface treatment realized in spatial and temporal afterglow DBD conditions10.1051/epjap:2008021 ↗
39. Plasma treatment of heat treated beech wood—investigation on surface free energy10.1515/HF.2008.074 ↗
40. Surface energy modification by radiofrequency inductive and capacitive plasmas at low pressures on sugar maple: an exploratory study
41. Investigation of pure and plasma-treated spruce with surface analytical techniques
42. Plasma activation of wood surface by diffuse coplanar surface barrier discharge10.1007/s11090-007-9117-8 ↗
43. Sanding vs. plasma treatment of aged wood: a comparison with respect to surface energy10.1016/j.ijadhadh.2007.11.001 ↗
44. Electron spectroscopy on plasma treated lignin and cellulose10.1515/hf.2010.048 ↗
45. Wood modification by atmospheric pressure plasma treatment
46. Wood veneer modification by atmospheric pressure plasma treatment for improved absorption characteristics
47. Improved absorption characteristics of thermally modified beech veneer produced by plasma treatment10.1007/s00107-011-0581-8 ↗
48. Increasing the water uptake of wood veneres through plasma treatment at atmospheric pressure10.1007/s00107-014-0815-7 ↗
49. Investigation of wood and timber surface modification by dielectric barrier discharge at atmospheric pressure10.1002/ppap.200731209 ↗
50. Modification of sugar maple (Acer saccharum) and black spruce (Picea mariana) wood surfaces in a dielectric barrier discharge (DBD) at atmospheric pressure10.1163/016942410X501007 ↗
51. Plasma modification of wood surfaces to improve the performance of clear coatings
52. Effects of plasma modification on adhesion properties of wood10.1016/j.ijadhadh.2011.10.003 ↗
53. Surface modification of wood by plasma polimerisation10.1108/03699420210412575 ↗
54. Hydrophobic wood surfaces generated by non-equilibrium, atmospheric pressure (NEAPP) plasma-enhanced coating10.1080/15421400801917486 ↗
55. Wood coated with plasma-polymer for water repellence10.1007/s00226-007-0160-7 ↗
56. Effect of plasma treatment on the wood flour for wood flour/PP composites10.1177/0892705708091604 ↗
57. Deposition of hydrophobic functional groups on wood surfaces using atmospheric-pressure dielectric barrier discharge in helium-hexamethyldisiloxane gas mixtures10.1002/ppap.201100222 ↗
58. Plasma treatment for enhanced adhesion of coatings to wood
59. Degradation of wood surfaces by water. Changes in mechanical properties of thin wood strips10.1007/BF02608208 ↗
60. Effect of treatments with 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU) on the tensile properties of wood10.1515/HF.2007.008 ↗
61. Effect of lignin and hemicelluloses on the tensile strength of micro-veneers determined at finite span and zero span10.1515/hf.2011.173 ↗
62. Investigations into the photodegradation of wood using microtensile testing. Part 4: Tensile properties and fractography of weathered wood10.1007/s00107-002-0282-4 ↗
63. Investigations into the photodegradation of wood using microtensile testing. Part 1: The application of microtensile testing to measurement of photodegradation rates10.1007/s001070050103 ↗
64. Weathering and photoprotection of wood
65. Microtensile testing of wood – overview of practical aspects of methodology10.5552/drind.2014.1320 ↗
66. A note on assessing the deterioration of thin wood veneers during weathering
67. Rapid loss of lignin at wood surfaces during natural weathering
68. A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds Part 1. Loss in zero-span tensile strength and weight of thin wood veneers10.1515/hfsg.1989.43.5.289 ↗
69. FTIR spectra of milled wood lignins and lignin polymer models (DHP's) with enhanced resolution obtained by deconvolution10.1080/02773818808070698 ↗
70. Preventing light induced degradation of wood by acetylation: a study on lignin and lignin model compounds
71. Weathering of wood modified with the N-methylol compound 110.1016/j.polymdegradstab.2004.08.017 ↗
72. Infrared spectra of Eucalyptus regnans F. Muell and Pinus radiata D. Don10.1515/hfsg.1964.18.4.108 ↗
73. Degradation of surfaces during natural weathering. Effects on lignin and cellulose and on the adhesion of acrylic latex primers10.1007/BF00244437 ↗
74. Comparisons of the photostability of esterified wood10.1016/S0141-3910(00)00171-3 ↗
75. Studies of the degradation and protection of wood surfaces10.1007/BF00194471 ↗
76. Determination of phenolic hydroxyl group content of milled wood lignins (MWL's) from different botanical origins using selective aminolysis, FTIR 1H-NMR, and UV spectroscopy10.1515/hfsg.1992.46.5.425 ↗
77. Schmidt · 1994
78. A tannin/copper preservation treatment for wood10.1515/hfsg.1998.52.2.133 ↗
79. The effect of copper on the growth of wood-rotting fungi and a blue stain fungus10.1007/s11274-007-9434-3 ↗