Ultraviolet laser-induced damage of freestanding silica nanoparticle films
Source abstract
Abstract
Abstract Silica nanoparticle antireflection films are essential for the development of high-power laser systems because of their high laser damage threshold in ultraviolet (e.g., 351 nm or 355 nm). However, most laser damage reports focus on the films standing on substrates, and the intrinsic laser damage behaviors of the silica nanoparticle films are poorly understood due to the influence of the substrates. Here, we investigate the ultraviolet laser damage behaviors of the freestanding silica nanoparticle films. We find that silica nanoparitcle films demonstrate higher laser damage threshold than the fused silica substrates under the irradiation of 355-nm laser. For the films on the fused silica substrates, the laser damage is caused by the substrates. In the case of freestanding films, laser-damage resistance is strongly dependent on the film thickness and the amount of organic groups in the films. The laser damage threshold increases from 103 to 159 J/cm2 @ 355 nm with decreasing the film thickness from 322 to 31 nm. In addition, removal of organic groups from the films results in higher laser damage threshold. Our findings provide insight into the laser damage behavior of the silica nanoparticle films and foreshow a possible way to improve the laser-damage resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Laser-induced spectroscopy and plasma · Surface Roughness and Optical Measurements
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Advanced mitigation process (AMP) for improving laser damage threshold of fused silica optics10.1038/srep31111 ↗
2. Laser-induced damage initiation and growth of optical materials
3. Comparative studies on the laser-induced damage of TiO2 films with different additives and thickness10.1016/j.ijleo.2015.09.097 ↗
4. Identification of the formation phases of filamentary damage induced by nanosecond laser pulses in bulk fused silica10.1063/1.4930942 ↗
5. Origin of the damage ring pattern in fused silica induced by multiple longitudinal modes laser pulses10.1063/1.4861748 ↗
6. Oxygen plasma etching of fused silica substrates for high power laser optics10.1016/j.apsusc.2018.05.105 ↗
7. Influence of vacuum on nanosecond laser-induced surface damage morphology in fused silica at 1064nm10.1016/j.apsusc.2015.11.199 ↗
8. Insight into the organic-inorganic hybrid and microstructure tailor mechanism of sol-gel ORMOSIL antireflective coatings10.1021/acs.jpcc.7b10294 ↗
9. Timing of polyethylene glycol addition for the control of SiO2 sol structure and sol–gel coating properties10.1007/s11998-016-9864-7 ↗
10. Synthesis of ultrasmall silica nanoparticles for application as deep-ultraviolet antireflection coatings10.1016/j.apsusc.2017.05.124 ↗
11. Laser-induced damage on ordered and amorphous sol-gel silica coatings10.1364/OME.4.002478 ↗
12. Role of coating defects in laser-induced damage to dielectric thin films10.1063/1.1654764 ↗
13. Effect of boundary continuity on nanosecond laser damage of nodular defects in high-reflection coatings10.1364/OL.42.000478 ↗
14. Optical properties and laser damage threshold of HfO2-SiO2 mixed composite thin films10.1364/AO.53.000850 ↗
15. Investigation of laser-induced damage by various initiators on the subsurface of fused silica10.1364/OE.20.022095 ↗
16. Model laser damage precursors for high quality optical materials10.1364/OE.22.003393 ↗
17. National Ignition Facility laser performance status10.1364/AO.46.003276 ↗
18. Sol–gel-processed hybrid silica-PDMS layers for the optics of high-power laser flux systems10.1007/s10853-016-9825-7 ↗
19. Superhydrophobic antireflective silica films: fractal surfaces and laser-induced damage thresholds10.1364/AO.44.000527 ↗
20. Hydro-oleophobic silica antireflective films with high laser-damage threshold10.1016/j.optlastec.2010.07.001 ↗
21. Ultraviolet laser-induced damage on fused silica substrate and its sol-gel coating10.1364/OL.37.002364 ↗
22. Increased laser-damage resistance of sol-gel silica coating by structure modification10.1021/jp307390u ↗
23. Durable solgel antireflective films with high laser-induced damage thresholds for inertial confinement fusion10.1364/JOSAB.22.000905 ↗
24. Sol–gel broadband anti-reflective single-layer silica films with high laser damage threshold10.1016/S0040-6090(03)00828-9 ↗
25. High laser damage threshold porous silica antireflective coating10.1364/AO.25.001481 ↗
26. Effect of polyvinyl butyral on the microstructure and laser damage threshold of antireflective silica films10.1016/j.tsf.2010.11.023 ↗
27. HF-based etching processes for improving laser damage resistance of fused silica optical surfaces10.1111/j.1551-2916.2010.04112.x ↗
28. Reaction ion etching process for improving laser damage resistance of fused silica optical surface10.1364/OE.24.000199 ↗
29. Understanding the effect of wet etching on damage resistance of surface scratches10.1038/s41598-018-19716-0 ↗
30. Laser induced damage characteristics of fused silica optics treated by wet chemical processes10.1016/j.apsusc.2015.09.065 ↗
31. Extracting the distribution of laser damage precursors on fused silica surfaces for 351 nm, 3 ns laser pulses at high fluences (20–150 J/cm2)10.1364/OE.20.011561 ↗
32. A new dip coating method to obtain large-surface coatings with a minimum of solution10.1002/adma.201502518 ↗
33. Femtosecond laser-induced periodic surface structures on titanium nitride coatings for tribological applications10.1016/j.apsusc.2016.10.132 ↗
34. Correlations between the oxygen deficiency and the laser damage resistance of different oxide films10.1016/j.apsusc.2013.10.121 ↗
35. Laser-induced damage of Ta2O5 films obtained from TaCl5 precursor and annealed at different temperatures10.1016/j.apsusc.2015.03.121 ↗
36. Improving the laser damage resistance of oxide thin films and multilayers via tailoring ion beam sputtering parameters10.1016/j.apsusc.2014.09.048 ↗
37. Low temperature processing of multilayer dielectrics mirrors by sol–gel method10.1016/j.matlet.2015.09.020 ↗
38. Sol-gel processing of zirconia coating for HR mirrors with high laser damage threshold10.1023/A:1008761010781 ↗
39. Comparison of different high and low index materials in the manufacture of high laser damage threshold mirrors at the 351 nm wavelength10.1023/A:1008617727647 ↗
40. Impact of storage induced outgassing organic contamination on laser induced damage of silica optics at 351 nm10.1364/OE.17.018703 ↗
41. Improvement of the bulk laser damage threshold of potassium dihydrogen phosphate crystals by reducing the organic impurities in growth solution10.1063/1.99429 ↗
42. Mitigation of organic laser damage precursors from chemical processing of fused silica10.1364/OE.22.029568 ↗
43. Sol-gel based hydrophobic antireflective coatings on organic substrates: a detailed investigation of ammonia vapor treatment (AVT)10.1021/cm403787v ↗
44. A superamphiphobic coating with an ammonia-triggered transition to superhydrophilic and superoleophobic for oil-water separation10.1002/ange.201411283 ↗
45. Properties of sol–gel derived scratch-resistant nano-porous silica films by a mixed atmosphere treatment10.1016/S0022-3093(00)00257-X ↗