Electro-spark deposition in vacuum using graphite electrode at different electrode polarities: Peculiarities of microstructure, electrochemical and tribological properties
Source abstract
Abstract
Abstract Titanium and its alloys are widely used in offshore and costal infrastructure, but need protection against wear and corrosion in saline environments. Compared to other surface engineering methods, electro-spark deposition (ESD) does not have the drawbacks of small thickness and poor adhesion of protective coatings. However, ESD in air or inert atmosphere using a graphite electrode does not provide sufficient continuity of a protective layer due to a low efficiency of carbon transfer. To enhance carbon transfer, Ti was subjected to ESD in vacuum using a graphite electrode. The main difference between vacuum and air deposition is that, in addition to spark discharges, arc evaporation occurs. It was shown that the carbon content, microstructure, and phase composition of modified Ti layer can be well controlled by changing electrode polarity and pulse energy. At cathodic polarity, arc discharge occurs on graphite electrode, which leads to increased carbon evaporation and a higher carbon content in the coating. Resulting coatings protect Ti from wear and corrosion in 3.5 wt.% NaCl solution due to formation of TiC layer. Coatings with top graphite layer show the lowest values of friction coefficient and corrosion current density, as well as fast corrosion potential recovery during tribocorrosion tests.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Coatings · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Microstructure, phase and tribocorrosion behavior of 60NiTi alloy10.1016/j.apsusc.2019.143838 ↗
2. Titanium alloys for marine application10.1016/S0921-5093(98)01180-0 ↗
3. Titanium Alloys for Aerospace Applications10.1002/adem.200310095 ↗
4. Leyens · 2003
5. Microbiologically influenced corrosion of titanium caused by aerobic marine bacterium Pseudomonas aeruginosa10.1016/j.jmst.2018.08.001 ↗
6. Microbiologically Influenced Corrosion in
7. Corrosion of Titanium: Part 1: Aggressive Environments and Main Forms of Degradation
8. Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
9. A Review on Biomedical Titanium Alloys: Recent Progress and Prospect10.1002/adem.201801215 ↗
10. Microstructure and wear resistance of a Ni-WC composite coating on titanium grade 2 obtained by electroplating and electron beam remelting10.1016/j.matchar.2020.110674 ↗
11. Chapter 4 - Automobile applications of titanium
12. Applications of Titanium Sheets in Modern Building Construction
13. Chapter 7 - Sporting goods: Components for bicycles
14. A study of the microstructure and hardness of two titanium alloys: Commercially pure and Ti–6Al–4V10.1016/j.jallcom.2009.06.172 ↗
15. Mechanical properties of biomedical titanium alloys10.1016/S0921-5093(97)00806-X ↗
16. Anomalous relationship between hardness and wear properties of a superelastic nickel–titanium alloy10.1063/1.1646218 ↗
17. Morphology, microstructure, and hardness of titanium (Ti-6Al-4V) blocks deposited by wire-feed additive layer manufacturing (ALM)10.1016/j.msea.2011.10.095 ↗
18. Reduction of friction coefficient of ultrafine-grained CP titanium10.1016/j.msea.2003.12.026 ↗
19. Tribological properties of titanium alloys10.1016/0043-1648(91)90249-T ↗
20. Surface modification of titanium, titanium alloys, and related materials for biomedical applications10.1016/j.mser.2004.11.001 ↗
21. Review of the biocompatibility of micro-arc oxidation coated titanium alloys10.1016/j.matdes.2015.07.086 ↗
22. Surface modification of titanium alloy implants10.1016/0142-9612(94)90113-9 ↗
23. Surface modification of titanium alloys for combined improvements in corrosion and wear resistance10.1016/S0257-8972(98)00580-5 ↗
24. Surface Modification of Titanium and Titanium Alloys: Technologies, Developments, and Future Interests10.1002/adem.201901258 ↗
25. Surface Modification of Titanium by Producing Ti/TiN Surface Composite Layers via FSP, Acta10.1007/s40195-017-0529-z ↗
26. Effect of surface mechanical attrition treatment of titanium using alumina balls: surface roughness, contact angle and apatite forming ability10.1007/s11706-013-0208-6 ↗
27. 12 - Laser surface modification of titanium alloys
28. Improving the tribocorrosion resistance of Ti6Al4V surface by laser surface cladding with TiNiZrO2 composite coating10.1016/j.apsusc.2015.03.152 ↗
29. A comparison of corrosion, tribocorrosion and electrochemical impedance properties of pure Ti and Ti6Al4V alloy treated by micro-arc oxidation process10.1016/j.apsusc.2014.11.030 ↗
30. Resistance of PVD Coatings to Erosive and Wear Processes: A Review10.3390/coatings10100921 ↗
31. Improving the wear and corrosion resistance of Ti–6Al–4V alloy by deposition of TiSiN nanocomposite coating with pulsed-DC PACVD10.1016/j.wear.2017.07.009 ↗
32. Conditions for formation of MAX phase Cr2AlC in electrospark coatings deposited onto titanium alloy10.1016/j.surfcoat.2016.04.058 ↗
33. Microstructure and tribological properties of Zr-based amorphous-nanocrystalline coatings deposited on the surface of titanium alloys by Electrospark Deposition10.1016/j.apsusc.2015.08.233 ↗
34. Interface behavior study of WC92–Co8 coating produced by electrospark deposition10.1016/j.apsusc.2004.05.299 ↗
35. Two-layer nanocomposite WC/a-C coatings produced by a combination of pulsed arc evaporation and electro-spark deposition in vacuum10.1016/j.matdes.2019.107645 ↗
36. Tribological and mechanical properties of nanocrystalline-TiC/a-C nanocomposite thin films10.1116/1.3294717 ↗
37. Advanced TiC/a-C: H nanocomposite coatings deposited by magnetron sputtering10.1016/j.jeurceramsoc.2005.06.023 ↗
38. Tribological properties of nc-TiC/a-C: H coatings prepared by magnetron sputtering at low and high ion bombardment of the growing film10.1016/j.surfcoat.2013.10.026 ↗
39. Deposition and some properties of nanocrystalline, nanocomposite and amorphous carbon-based coatings for tribological applications10.1016/j.jmatprotec.2004.09.044 ↗
40. Compositional, structural and mechanical characteristics of nc-TiC/a-C: H nanocomposite films10.1016/j.apsusc.2008.06.020 ↗
41. Nanocomposite TiC/a–C: H hard coatings deposited by reactive PVD10.1016/S0257-8972(00)00888-4 ↗
42. On the control of deposition process for enhanced mechanical properties of nc-TiC/a-C: H coatings with DC magnetron sputtering at low or high ion flux10.1016/j.surfcoat.2013.11.001 ↗
43. Tribocorrosion behaviors of nc-TiC/a-C: H nanocomposite coatings: In-situ electrochemical response10.1016/j.tsf.2021.138719 ↗
44. X-ray diffraction patterns of graphite and turbostratic carbon10.1016/j.carbon.2007.03.038 ↗
45. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
46. Graphitization in a high-pressure, low-temperature metamorphic gradient: a Raman microspectroscopy and HRTEM study10.1007/s00410-001-0324-7 ↗
47. Understanding the Application of Raman Spectroscopy to the Detection of Traces of Life10.1089/ast.2009.0344 ↗
48. A multi wavelength Raman scattering study of defective graphitic carbon materials: The first order Raman spectra revisited10.1016/j.carbon.2016.06.017 ↗
49. Structure and properties of in situ-generated two-dimensional turbostratic graphite nodules10.1016/j.carbon.2017.09.036 ↗
50. Microstructure and properties of low friction TiC□C nanocomposite coatings deposited by magnetron sputtering10.1016/S0257-8972(01)01493-1 ↗
51. Carbon 1s X-ray Photoemission Line Shape Analysis of Highly Oriented Pyrolytic Graphite: The Influence of Structural Damage on Peak Asymmetry10.1021/la052922r ↗
52. Gogotsi · 2006 · 800
53. Structure of Carbon Materials Explored by Local Transmission Electron Microscopy and Global Powder Diffraction Probes
54. A concise model for evaluating water electrolysis10.1016/j.ijhydene.2010.12.029 ↗
55. Low-voltage DC/AC electrolysis of water using porous graphite electrodes10.1016/j.electacta.2010.04.022 ↗
56. Performance properties of electro-spark deposited carbide-ceramic coatings modified by laser beam10.1016/j.phpro.2010.08.163 ↗
57. Interfacial energy as the driving force for diffusion bonding of ceramics10.1016/j.actamat.2020.01.015 ↗