journal article·2015-11

Pre-ablation treatment of carbon/carbon composites to improve the thermal shock resistance for SiC coating under oxyacetylene torch

Jia-Ping Zhang, Qian-Gang Fu, Jun-Ling Qu, He-Jun Li

Publisher page

Abstract

Abstract C/C composites were pre-ablated for different time (0 s, 15 s, 30 s and 45 s) under oxyacetylene torch. The mass ablation rate of the C/C composites was 0.39 mg cm −2 s −1 . An interlocking transition layer of SiC was formed on the pre-ablated C/C composites by pack cementation. Thermal shock test of the SiC coated C/C composites was performed under oxyacetylene torch from 1873 K to room temperature. Compared with the coated C/C composites pre-ablated for 0 s, 15 s and 45 s, after 10 thermal cycles, no coating/substrate gaps or penetrating cracks were found in the SiC coated C/C composites with the C/C substrate pre-ablated for 30 s. The good shock performance was attributed to the interlocking structure of transition layer, which could efficiently alleviate the mismatch of thermal expansion coefficient between C/C substrate and SiC coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Oxidation microstructure studies of reinforced carbon/carbon10.1016/j.carbon.2005.11.013 ↗
2. Carbon–carbon composites10.1146/annurev.ms.24.080194.000315 ↗
3. Laser ablation behaviors of SiC–ZrC coated carbon/carbon composites10.1016/j.surfcoat.2011.03.039 ↗
4. Oxidation kinetics of the AlPO4 ceramic coatings by pulse arc discharge deposition on SiC–C/C composites10.1016/j.vacuum.2014.11.010 ↗
5. Erosion resistance of Mo–Si–Cr coating-modified C/C composites in a wind tunnel at 1873K10.1016/j.jallcom.2014.10.189 ↗
6. Sealing of cracks in the rhenium coating on C/C composites by alloying with cobalt10.1016/j.surfcoat.2014.10.032 ↗
7. Mo–Si–Al–C multiphase oxidation protective coating for carbon/carbon composites10.1016/j.apsusc.2013.03.050 ↗
8. SiC coating toughened by HfC nanowires to protect C/C composites against oxidation10.1016/j.apsusc.2014.05.042 ↗
9. Microstructure and oxidation resistance of C–AlPO4–mullite coating prepared by hydrothermal electrophoretic deposition for SiC C/C composites10.1016/j.ceramint.2012.07.024 ↗
10. A novel laser technique for oxidation-resistant coating of carbon–carbon composite10.1016/S0008-6223(00)00200-1 ↗
11. Resistance to oxidation of graphite silicided by reactive infiltration10.1016/j.jeurceramsoc.2011.05.005 ↗
12. Microstructure and property of SiC coating for carbon materials10.1016/j.fusengdes.2007.03.001 ↗
13. Microstructure and oxidation of multi-layer MoSi2–CrSi2–Si coatings for SiC coated carbon/carbon composites10.1016/j.corsci.2010.05.020 ↗
14. Oxidation pre-treatment and electrophoretic deposition of SiC nanowires to improve the thermal shock resistance of SiC coating for C/C composites10.1016/j.jallcom.2015.02.075 ↗
15. The degradation behavior of SiC coated PIP–C/SiC composites in thermal cycling environment10.1016/j.compositesb.2015.04.028 ↗
16. Fatigue of ceramic matrix composites10.1016/0956-7151(94)00304-Z ↗
17. Corrosion behavior of pre-oxidized and thermally nitrided stainless steel for polymer electrolyte membrane fuel cell bipolar plates10.1016/j.corsci.2012.01.014 ↗
18. Oxidation pre-treatment to improve the mechanical property and oxidation resistance of Si–Mo–Cr coated C/C composites10.1016/j.corsci.2014.02.008 ↗
19. Microstructure and thermal shock resistance of the peg-nail structured TBCs treated by selective laser modification10.1016/j.apsusc.2014.08.084 ↗
20. Effect of LaB6 on the thermal shock property of MoSi2–SiC coating for carbon/carbon composites10.1016/j.apsusc.2012.09.124 ↗
21. The effect of zirconium carbide on ablation of carbon/carbon composites under an oxyacetylene flame10.1016/j.corsci.2010.09.028 ↗
22. Thermal shock properties of 3D-C/SiC composites prepared via polymer infiltration pyrolysis (PIP)10.1016/j.ceramint.2014.01.122 ↗