Abstract

Abstract The Ni modified layers were prepared on the surface of Ti6Al4V substrate by the plasma surface alloying technique. The surface and cross-section morphology, element concentration and phase composition were investigated by thermal field emission scanning electron microscopy (SEM), and glow discharge optical emission spectroscopy (GDOES), X-ray diffraction (XRD), respectively. The cross-section nano-scale hardness of the Ni modified layer was measured by nanoindenter. The results showed that the Ni modified layers exhibited triple-layer structure and continuous gradient distribution of the concentration. From the surface to the matrix, they were 2 μm Ni deposition layer, 8 μm Ni-rich alloying layer including the phases of Ni 3 Ti, NiTi, Ti 2 Ni, AlNi 3 and 24 μm Ni-poor alloying layer forming the solid solution of nickel. With increasing of the thickness of the Ni modified layer, the microhardness increased first, reached the climax, then gradient decreased. The erosion tests were performed on the surfaces of the untreated and treated Ti6Al4V samples using MSE (Micro-slurry-jet Erosion) method. The experiment results showed that the wear rate of every layer showed different values, and the Ni-rich alloying layer was the lowest. The strengthening mechanism of the Ni modified layer showed micro-cutting wearing.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. The corrosion–wear response of CrTi coatings10.1016/j.wear.2006.12.058 ↗
2. Surface modification of titanium alloy Ti6Al4V by plasma niobium alloying process10.1016/j.surfcoat.2006.07.061 ↗
3. Erosion- and cavitation–corrosion of titanium and its alloys10.1016/S0043-1648(01)00709-8 ↗
4. Composite TiNNi thin films deposited by reactive magnetron sputter ion-plating10.1016/S0257-8972(98)00688-4 ↗
5. NiTiO 2 nanocomposite coating with high resistance to corrosion and wear10.1016/j.surfcoat.2010.04.061 ↗
6. The use of nickel graphite composite coatings for the mitigation of gross slip fretting wear on Ti6Al4V interfaces10.1016/j.wear.2009.03.023 ↗
7. Structure and mechanical properties of pure titanium film deposited onto TiNi shape memory alloy substrate by magnetron DC sputtering10.1016/j.tsf.2003.12.147 ↗
8. Characteristics of TiNi alloy thin films10.1016/S0040-6090(01)01325-6 ↗
9. A new type of wear-resistant material: pseudo-elastic TiNi alloy10.1016/S0043-1648(98)00269-5 ↗
10. Structure and properties of nitrided surface layer produced on NiTi shape memory alloy by low temperature plasma nitriding10.1016/j.apsusc.2014.07.109 ↗
11. Fabrication of NiTi intermetallic compound coating made by laser plasma hybrid spraying mechanically alloy powders10.1016/S0257-8972(01)00994-X ↗
12. Abrasive wear property of laser melting/deposited Ti2Ni/TiNi intermetallic alloy10.1016/S1003-6326(07)60277-5 ↗
13. Nanoscale compositional analysis of NiTi shape memory alloy films deposited by DC magnetron sputtering10.1116/1.4816841 ↗
14. Abrasive wear property of laser melting/deposited Ti2Ni/TiNi intermetallic alloy10.1016/S1003-6326(07)60277-5 ↗
15. Dry sliding wear property of a laser melting/deposited Ti2Ni/TiNi intermetallic alloy10.1016/j.intermet.2007.09.008 ↗
16. Evaluation of wear resistance of thin hard coatings by a new solid particle impact test10.1016/S0043-1648(01)00743-8 ↗
17. Evaluation of erosive wear resistance of TiN coatings by a slurry jet impact test10.1016/j.wear.2005.09.030 ↗
18. Cavitation erosion behavior of laser gas nitrided Ti and Ti6Al4V alloy10.1016/S0921-5093(03)00062-5 ↗
19. Cavitation erosion–corrosion characteristics of laser surface modified NiTi shape memory alloy10.1016/S0257-8972(02)00399-7 ↗
20. Effect of gas nitriding treatment on cavitation erosion behavior of commercially pure Ti and Ti–6Al–4V alloy10.1016/j.surfcoat.2013.01.023 ↗
21. Effect of microstructure on the erosion behavior of carbon steel10.1016/j.wear.2014.12.004 ↗
22. Surface modification by gas nitriding for improving cavitation erosion resistance of CP-Ti10.1016/j.apsusc.2014.01.152 ↗
23. Double glow plasma surface alloying and plasma nitriding10.1016/j.surfcoat.2006.07.187 ↗
24. Microstructure and tribological behaviors of Ti6Al4V alloy treated by plasma Ni alloying10.1016/j.apsusc.2011.07.040 ↗
25. Effect of TiNi in dry sliding wear of laser melt deposited Ti2Ni/TiNi alloys10.1016/j.matchar.2008.05.007 ↗
26. Influence of annealing on structural, morphological, compositional and surface properties of magnetron sputtered nickel–titanium thin films10.1016/j.apsusc.2013.05.159 ↗
27. Funakubo · 1987 · 275