Abstract The formation of nanodimensional structures on the surface of Tin (Sn) has been explored as a function of the laser fluence and pulse duration. The targets were exposed by employing femtosecond pulses of a Ti: Sapphire laser (wavelength of 800 nm, pulse length of 25 fs and pulse repetition rate of 1 kHz) in ethanol. In order to investigate the effect of fluence, the targets were exposed to 1000 succeeding pulses for four various fluences ranging from 4.7 to 11.8 J cm−2 with the pulse duration of 25 fs. To probe the effect of pulse duration, targets were exposed for various pulse durations ranging from 25 fs to 100 fs at a constant fluence of 11.8 J cm−2 (i.e. maximum). Nano sized structures including globules, droplets, craters and grooves were observed by SEM analysis. The dependence of structure formation on the laser fluence and pulse duration has been explored both for central as well as peripheral ablated areas. For increasing fluences, the more energy deposition is responsible for the growth of distinct features. For increasing fluence, the size distribution of nanostructures reduces and their number density increases after fragmentation. As the pulse width increases, the size distribution of structures increases significantly due to enhanced thermal effects. The development of nanostructures has been correlated with structural analysis carried out by micro-Raman spectroscopy. The formation of various bands e.g. SnO, SnO2, C2H5 Sn, Sn–CO complexes after laser irradiation of Sn in a liquid-confined environment (ethanol) has been observed. For higher fluences more energy deposition takes place which enhances the chemical reactivity and is responsible for an appearance of additional and strong bands. However, with increasing pulse width more thermal effects are responsible for bond breaking and disappearance of those peaks which are identified for the shortest pulse duration. It is found first time that both the pulse duration as well as laser fluence are promising parameters to be explored for the modification of the Sn surface. The optimum growth of smallest structures is possible only for the highest fluence and the shortest pulse duration within the utilized range of parameters where the maximum chemical reactivity takes place.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Laser-Ablation Synthesis of Nanoparticles · Laser-induced spectroscopy and plasma · Laser Material Processing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Refining femtosecond laser induced periodical surface structures with liquid assist10.1016/j.apsusc.2012.09.101 ↗
2. Femtosecond laser induced nanostructure formation: self-organization control parameters10.1007/s00339-008-4671-3 ↗
3. Nanotexturing of gold films by femtosecond laser-induced melt dynamics10.1007/s00339-005-3212-6 ↗
4. Fundamentals and prospects of ultra-short laser-radiation for material processing, surface analysis and medical applications10.1117/12.478655 ↗
5. Rapid bulk analysis using femtosecond laser ablation inductively coupled plasma time-of-flight mass spectrometry10.1039/c2ja10368k ↗
6. Surface topography (nano-sized hillocks) and particle emission of metals, dielectrics and semiconductors during ultra-short-laser ablation: towards a coherent understanding of relevant processes10.1016/j.apsusc.2009.05.090 ↗
7. Identification of ultra-fast electronic and thermal processes during femtosecond laser ablation of Si10.1007/s00339-012-7067-3 ↗
8. Laser-assisted nanostructuring of Tungsten in liquid environment10.1016/j.apsusc.2012.02.135 ↗
9. Laser control of the properties of nanostructures on Ta and Ni under their ablation in liquids
10. Nanosecond pulsed laser ablation of brass in a dry and liquid-confined environment10.1007/s00339-012-7175-0 ↗
11. Generation of surface nanostructures on nickel by liquid-phase laser ablation and their surface-enhanced Raman scattering activity10.1070/QE2010v040n04ABEH014259 ↗
12. Effect of dry and wet ambient environment on the pulsed laser ablation of titanium10.1016/j.apsusc.2012.12.049 ↗
13. Generation of nanostructures on metals by laser ablation in liquids10.1070/QE2010v040n11ABEH014444 ↗
14. Laser ablation in liquids: applications in the synthesis of nanocrystals10.1016/j.pmatsci.2006.10.016 ↗
15. Laser ablation in a liquid-confined environment using a nanosecond laser pulse10.1063/1.2905314 ↗
16. Laser ablative approach for the synthesis of cadmium-hydroxide nanocomposite10.1007/s11051-009-9696-9 ↗
17. Nanoparticles produced by laser ablation of solids in liquid environment10.1007/s00339-004-2660-8 ↗
18. Synthesis of ultrafine SnO2-x nanocrystals by pulsed laser-induced reactive quenching in liquid medium10.1021/jp0347466 ↗
19. The growth of nanoscale periodic and dot-like structures on the surface of stainless steel with femtosecond laser pulses in the dry and wet ambient environment10.1007/s00339-013-7675-6 ↗
20. Laser ablation in water: a route to synthesize nanoparticles of titanium monoxide10.1016/j.cplett.2010.07.023 ↗
21. Formation of conical microstructures upon laser evaporation of solids10.1007/s003390100530 ↗
22. Self-influence of a femtosecond laser beam upon ablation of Ag in liquids10.1007/s00339-003-2357-4 ↗
23. Socrates · 2001
24. Micro-Raman investigation of tin dioxide nanostructured material based on annealing effect10.1002/jrs.2919 ↗
25. Parker · 1983