Evaluation of atomic layer deposited alumina as a protective layer for domestic silver articles: Anti-corrosion test in artificial sweat
Source abstract
Abstract
Abstract This study evaluated the effectiveness of alumina fabricated by atomic layer deposition (ALD) as a protective coating for silver articles against the corrosion caused by body contact. An artificial sweat solution was used to simulate body contact. ALD alumina layers of varying thicknesses ranging from 20 to 80 nm were deposited on sputtered silver samples. The stability of the protective layer was evaluated by immersing the coated samples in the artificial sweat solution at 25 and 35 °C for 24 h. We confirmed that a sufficiently thick layer of ALD alumina is effective in protecting the shape and light reflectance of the underlying silver, whereas the uncoated bare silver is severely degraded by the artificial sweat solution. Inductively coupled plasma mass spectrometry and X-ray photoelectron spectroscopy were used for in-depth analyses of the chemical stability of the ALD-coated silver samples after immersion in the sweat solution.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Corrosion mechanisms for silver exposed to the atmosphere10.1149/1.2221162 ↗
2. Atmospheric corrosion of silver, copper, and nickel — Environmental test10.1149/1.2131352 ↗
3. Analysis of Ag corrosion products10.1149/2.055308jes ↗
4. Protection of silver surfaces against tarnishing by means of alumina/titania-nanolayers10.1016/j.surfcoat.2011.03.101 ↗
5. Protecting silver cultural heritage objects with atomic layer deposited corrosion barriers10.1186/s40494-015-0066-x ↗
6. Corrosion protection of silver coated reflectors by atomic layer deposited Al2O310.1016/j.solener.2013.11.038 ↗
7. Atomic layer deposition of yttria-stabilized zirconia for solid oxide fuel cells10.1021/cm070913t ↗
8. Atomic layer deposition of thin-film ceramic electrolytes for high-performance fuel cells10.1039/c3ta11399j ↗
9. Vibration atomic layer deposition for conformal nanoparticle coating10.1116/1.4845735 ↗
10. Chemical protection of polycarbonate surfaces by atomic layer deposition of alumina with oxygen plasma pretreatment10.1002/admi.201600340 ↗
11. Nanoporous silver cathode surface treated by atomic layer deposition of CeOx for low-temperature solid oxide fuel cells10.1088/0957-4484/27/18/185403 ↗
12. Low-temperature Al2O3 atomic layer deposition10.1021/cm0304546 ↗
13. Resistive switching characteristics of polycrystalline SrTiO3 films10.1063/1.4883646 ↗
14. Thin film encapsulation for flexible AM-OLED: a review10.1088/0268-1242/26/3/034001 ↗
15. Process–property relation in high-k ALD SrTiO3 and BaTiO3: a review10.1039/C6TC05158H ↗
16. Tarnish protection of silver jewels by plasma polymer coatings10.1016/S0257-8972(03)00713-8 ↗
17. Maximum noble-metal efficiency in catalytic materials: atomically dispersed surface platinum10.1002/anie.201402342 ↗
18. Ca test of Al2O3 gas diffusion barriers grown by atomic layer deposition on polymers10.1063/1.2221912 ↗
19. Low-temperature atomic layer deposition of Al2O3 thin coatings for corrosion protection of steel: Surface and electrochemical analysis10.1016/j.corsci.2011.02.036 ↗
20. Al2O3 and TiO2 atomic layer deposition on copper for water corrosion resistance10.1021/am2009579 ↗
21. Al2O3/TiO2 nanolaminate thin film encapsulation for organic thin film transistors via plasma-enhanced atomic layer deposition10.1021/am500458d ↗
22. Corrosion protection of steel with oxide nanolaminates grown by atomic layer deposition10.1149/2.061111jes ↗
23. Electrochemical and time-of-flight secondary ion mass spectrometry analysis of ultra-thin metal oxide (Al2O3 and Ta2O5) coatings deposited by atomic layer deposition on stainless steel10.1016/j.electacta.2011.02.074 ↗
24. Chemical stability of titania and alumina thin films formed by atomic layer deposition10.1021/acsami.5b03278 ↗
25. Silver or silver nanoparticles: a hazardous threat to the environment and human health?10.32725/jab.2008.015 ↗
26. Oral toxicity of silver ions, silver nanoparticles and colloidal silver – a review10.1016/j.yrtph.2013.11.002 ↗
27. Atomic layer deposition of alumina onto carbon fibers10.1111/j.1551-2916.2010.04340.x ↗
28. Control of thickness and morphology of thin alumina films deposited via pulsed chemical vapor deposition (pulsed CVD) through variation of purge times10.1016/j.surfcoat.2011.03.009 ↗