Al-Ti-W alloys deposited by magnetron sputtering: Effective barrier to prevent steel hydrogen embrittlement
Source abstract
Abstract
Abstract Thin film represents a promising alternative for the protection of metallic structures against hydrogen embrittlement and corrosion degradation. Al-Ti-W coatings were deposited by magnetron sputtering technique using three pure metallic targets. Tungsten was incorporated in Al-Ti amorphous coating with different contents ranging from 0 to 17 at% by keeping a constant Ti/Al ratio at an average of 0.8. The deposition rate was calculated in order to obtain 4 µm as an uniform film thickness. XRD, DSC and TEM analyses were performed to confirm the amorphous state of the coatings and to determine the glass transition temperature (Tg) and crystallization temperature peak (Tp). These temperatures were increased respectively from 423 °C and 595 °C to 490 °C and 665 °C with the increase of W concentration up to 17 at%. Corrosion resistance in a saline solution decreased with the increase of W content.The incorporation of W element induced an increase of the thin film hardness (H) and Young’s modulus (Er) from 9 GPa to 9.35 GPa and from 117 GPa to 131,79 GPa, respectively. The surface roughness varied with the incorporation of W that strongly influenced the coatings’ corrosion behavior. Chemical and electrochemical hydrogen charging techniques were performed to expose coated steels to hydrogen sources. W addition in the binary Al-Ti coatings strongly enhanced their resistance to hydrogen absorption. The estimated total hydrogen content trapped in the coated steel during a cathodic polarization decreased with the incorporation of W.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. Bp Statistical Review of World Energy 2020, 68 (2020).
2. Hydrogen at Scale (H 2 @Scale): Key to a Clean, Economic, and Sustainable Energy System, The10.1149/2.F04181if ↗
3. Hydrogen Supply Chains for Mobility—Environmental and Economic Assessment10.3390/su10061699 ↗
4. Pollution 2.Pdf.
5. Assessing the Public Health Impacts of Urban Air Pollution in 25 European Cities: Results of the Aphekom Project10.1016/j.scitotenv.2013.01.077 ↗
6. Development of High Pressure Gaseous Hydrogen Storage Technologies10.1016/j.ijhydene.2011.02.125 ↗
7. Development of European Hydrogen Infrastructure Scenarios—CO2 Reduction Potential and Infrastructure Investment10.1016/j.enpol.2005.12.019 ↗
8. Hydrogen Embrittlement Phenomena and Mechanisms10.1515/corrrev-2012-0502 ↗
9. 2002
10. ABSORPTION AND DIFFUSION OF HYDROGEN IN STEELS
11. Hydrogen Adsorption on Nanosized Platinum and Dynamics of Spillover onto Alumina and Titania10.1021/acs.jpcc.7b03733 ↗
12. Influence of Sandblasting and Hydrogen on Tensile and Fatigue Properties of Pipeline API 5L X52 Steel10.1016/j.ijhydene.2010.11.081 ↗
13. Hydrogen Embrittlement Understood10.1007/s11663-015-0325-y ↗
14. Sofronis · Viable Mechanisms of Hydrogen Embrittlement—A Review, in AIP Conference Proceedings · 2006 · Vol. 837 · 64
15. Hydrogen Embrittlement in Different Materials: A Review10.1016/j.ijhydene.2018.09.201 ↗
16. Gangloff · Hydrogen Assisted Cracking of High Strength Alloys · 2003 · 195
17. Review of Environmentally Assisted Cracking10.1007/s11661-010-0472-3 ↗
18. R. P. Gangloff, Critical Issues in Hydrogen Assisted Cracking of Structural Alloys, 1, 25 (n.d.).
19. Filiform Corrosion of Aluminium Sheet. I. Corrosion Behaviour of Painted Material10.1016/S0010-938X(98)00026-2 ↗
20. Evaluation of the Surface Treatment Effect on the Anticorrosive Performance of Paint Systems on Steel10.1016/S0300-9440(03)00112-7 ↗
21. Graphene Coating as a Protective Barrier against Hydrogen Embrittlement10.1016/j.ijhydene.2014.05.132 ↗
22. Niobium Coating Applied by HVOF as Protection against Hydrogen Embrittlement of API 5CT P110 Steel10.1016/j.surfcoat.2017.05.017 ↗
23. The Effects of Sacrificial Coatings on Hydrogen Embrittlement and Re-Embrittlement of Ultra High Strength Steels10.1016/j.corsci.2007.11.023 ↗
24. Effects of Tungsten on the Hydrogen Embrittlement Behaviour of Microalloyed Steels10.1016/j.corsci.2014.01.042 ↗
25. S. Yamaura, Y. Shimpo, H. Okouchi, M. Nishida, O. Kajita, and A. Inoue, The Effect of Additional Elements on Hydrogen Permeation Properties of Melt-Spun Ni-Nb-Zr Amorphous Alloys*, 4 (n.d.).
26. Mechanism for Adsorption, Dissociation and Diffusion of Hydrogen in Hydrogen Permeation Barrier of α-Al2O3: A Density Functional Theory Study10.1016/j.ijhydene.2012.10.108 ↗
27. Preparation Technique and Alloying Effect of Aluminide Coatings as Tritium Permeation Barriers: A Review10.1016/j.ijhydene.2015.01.052 ↗
28. Deuterium Permeation through Eurofer and α-Alumina Coated Eurofer10.1016/j.jnucmat.2004.03.008 ↗
29. D. Stover, H. P. Buchkremer, and R. Hecker, HYDROGEN AND DEUTERIUM PERMEATION THROUGH METALLIC AND SURFACE-OXIDIZED CHROMIUM, 10 (n.d.).
30. Erbium Oxide as a New Promising Tritium Permeation Barrier10.1016/j.jnucmat.2007.03.183 ↗
31. Preparation and Properties of Erbium Oxide Films Deposited by Radio Frequency Magnetron Sputtering10.1016/j.apsusc.2014.04.086 ↗
32. Tritium-Permeation-Barrier Properties of Erbium Oxide (TPB) Coating on CLAM Steel10.1016/j.fusengdes.2018.12.022 ↗
33. R. Checchetto, L. M. Gratton, A. Miotello, and C. Tosello, Deuterium Permeation through Sit 2 Thin Film Deposited on Stainless Steel Substrate, 6 (1997).10.1016/S0022-3093(97)00173-7 ↗
34. Performances of AlN Coatings as Hydrogen Isotopes Permeation Barriers10.1016/j.fusengdes.2015.11.043 ↗
35. Hydrogen Permeation Barriers: Basic Requirements
36. Microstructural Influence on Hydrogen Permeation and Trapping in Steels10.1016/j.matdes.2019.107605 ↗
37. Zhang et al. - 2013 - Energetics and Diffusion of Hydrogen in Hydrogen p.Pdf.
38. Thin Film Metallic Glasses: Unique Properties and Potential Applications10.1016/j.tsf.2012.03.092 ↗
39. Development of Amorphous Ni-P Coating over API X70 Steel for Hydrogen Barrier Application10.1016/j.surfcoat.2020.126356 ↗
40. Hydrogen Permeation through Silicon Nitride Films10.1016/j.jallcom.2012.05.110 ↗
41. Effects of Test Conditions on Corrosion Reactions and Hydrogen Absorption in Hydrogen Embrittlement Tests Using an Ammonium Thiocyanate Solution10.2355/isijinternational.ISIJINT-2015-288 ↗
42. Transgranular Stress Corrosion Cracking of High-Pressure Pipelines in Contact with Solutions of Near Neutral PH10.5006/1.3294348 ↗
43. Characteristic Studies on the Zr-Based Metallic Glass Thin Film Fabricated by Magnetron Sputtering Process10.1016/j.surfcoat.2008.06.099 ↗
44. Study of the Characteristics and Corrosion Behavior for the Zr-Based Metallic Glass Thin Film Fabricated by Pulse Magnetron Sputtering Process10.1016/j.tsf.2009.03.049 ↗
45. Obeydavi · Microstructure, Mechanical Properties and Corrosion Performance of Fe44Cr15Mo14Co7C10B5Si5 Thin Film Metallic Glass Deposited by DC Magnetron Sputtering · 2020 · 17
46. A. Inoue, STABILIZATION OF METALLIC SUPERCOOLED LIQUID AND BULK AMORPHOUS ALLOYS p, 28 (n.d.).
47. Classification of Bulk Metallic Glasses by Atomic Size Difference
48. Billard · Pulvérisation cathodique magnétron · 2005 · 23
49. Mechanically Reinforced and Corrosion-Resistant Sputtered Amorphous Aluminium Alloy Coatings10.1016/S0257-8972(97)00231-4 ↗
50. X-Ray Diffraction Study of Amorphous Alloys Al–Ni–Ce–Sc with Using Ehrenfest’s Formula10.1016/j.jnoncrysol.2006.05.031 ↗
51. Microstructure Analysis of Element W in Improving the Ni–P Deposit Thermal Stability10.1016/j.jmrt.2020.03.073 ↗
52. Investigation of Thermal Stability, Phase Formation, Electrical, and Microstructural Properties of Sputter-Deposited Titanium Aluminide Thin Films10.1016/j.tsf.2004.01.048 ↗
53. Microstructure Evolution during Annealing of an Amorphous TiAl Sheet10.1016/S0921-5093(02)00189-2 ↗
54. Alloy design of gamma titanium aluminides based on phase diagrams10.1016/S0966-9795(98)00048-X ↗
55. On the Amorphous Nature of Sputtered Thin Film Alloys10.1016/j.actamat.2016.02.035 ↗
56. Review Article: Stress in Thin Films and Coatings: Current Status
57. Effects of Tungsten Contents on the Microstructure, Mechanical and Anticorrosion Properties of Zr–W–Ti Thin Film Metallic Glasses10.1016/j.tsf.2015.01.063 ↗
58. Preparation and Structure of AlW Thin Films10.1016/S0040-6090(97)00508-7 ↗
59. Biocompatibility and Mechanical Property Evaluation of Zr-Ti-Fe Based Ternary Thin Film Metallic Glasses10.1016/j.surfcoat.2016.11.039 ↗
60. Formation of Manganese-Rich Layers during Anodizing of Al–Mn Alloys10.1016/S0010-938X(99)00025-6 ↗
61. The Composition and Morphology of Anodic Films on Al-Mo Alloys10.1149/1.1837499 ↗
62. A Corrosion Study on W-Cu Alloys in Sodium Chloride Solution at Different PH10.1016/j.jmst.2020.03.031 ↗
63. Effects of Compositional and Structural Features on Corrosion Behavior of Nickel-Tungsten Alloys10.1007/s10008-008-0712-2 ↗
64. Electrochemical and Surface Investigation of Zirconium Based Metallic Glass Zr59Ti3Cu20Al10Ni8 Alloy in Nitric Acid and Sodium Chloride Media10.1016/j.jallcom.2010.05.002 ↗
65. Influence of Metallurgical Parameters on the Electrochemical Behavior of Electrodeposited Ni and Ni–W Nanocrystalline Alloys10.1016/j.apsusc.2016.02.101 ↗
66. Electrochemical Behavior of Ni W Alloys Obtained by Magnetron Sputtering10.1016/j.surfcoat.2018.07.071 ↗
67. The Hydrogen Evolution Reaction in Alkaline Solution: From Theory, Single Crystal Models, to Practical Electrocatalysts10.1002/anie.201710556 ↗
68. The Influence of Microstructure on Hydrogen Transport in Carbon Steels10.1016/0010-938X(96)00109-6 ↗
69. Studies on Hydrogen Permeability of 2.25% Cr–1% Mo Ferritic Steel: Correlation with Microstructure10.1016/S0022-3115(00)00706-6 ↗