journal article·2022-03Open access

Titanium anodization in deep eutectic solvents: The effect of anodizing time on the morphology and structure of anodic layers

Juliusz Winiarski, Włodzimierz Tylus, Mirosława Pawlyta, Bogdan Szczygieł

Abstract

Deep eutectic solvents (DES) are successfully used as green solvents for electrochemical polishing of titanium. The tests performed showed that they can also be used for the production of nanometric TiO2 layers on Grade 2 titanium with thickness and crystallinity controlled by the anodizing time. Anodic polarization at 60 °C in choline dihydrogencitrate salt : oxalic acid DES allows to obtain amorphous TiO2 layer with a thickness of 5–11 nm in just a few seconds. Extending this time to 30 s causes, apart from increasing layer thickness, a distinct development of its surface. In the layer formed during the 20 min of polarization, nanosized crystalline domains begin to dominate, and the thickness of the TiO2 layer increases to approx. 30 nm. The process accompanying titanium anodizing is the incorporation of small amounts of “organic” carbon, most likely DES residues, into the structure of TiO2 layers.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic and Structural Properties of Oxides · Corrosion Behavior and Inhibition · Ionic liquids properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Thermal oxidation behaviour of bulk titanium with nanocrystalline surface layer10.1016/j.corsci.2012.03.005 ↗
2. Effect of anodic oxidation parameters on the titanium oxides formation10.1016/j.corsci.2006.04.002 ↗
3. Time dependence of growth and crystallization of anodic titanium oxide films in potentiostatic mode10.1016/j.corsci.2013.06.004 ↗
4. Debunking the formation mechanism of nanopores in four kinds of electrolytes without fluoride ion10.1016/j.elecom.2021.107093 ↗
5. Deep eutectic solvents (DESs) and their applications10.1021/cr300162p ↗
6. Deep eutectic solvents: syntheses, properties and applications10.1039/c2cs35178a ↗
7. Utilization of deep eutectic solvents in dispersive liquid-liquid micro-extraction10.1016/j.trac.2019.115651 ↗
8. Titanium anodizing in a choline dihydrogencitrate salt-oxalic acid deep eutectic solvent: a step towards green chemistry in surface finishing of titanium and its alloys10.1039/D1RA01655E ↗
9. Self-organization of TiO2 nanobamboos by anodization with deep eutectic solvent10.1016/j.electacta.2014.11.084 ↗
10. M.C. Biesinger, B.P. Payne, A.P. Grosvenor, L.W.M. Lau, A.R. Gerson, R.St.C. Smart, Resolving Surface Chemical States in XPS Analysis of First Row Transition Metals, Oxides and Hydroxides: Cr, Mn, Fe, Co and Ni, Appl. Surf. Sci. 257 (2011) 2717–2730. https://doi.org/10.1016/j.apsusc.2010.10.051.10.1016/j.apsusc.2010.10.051 ↗
11. Structural and thermal parameters for rutile and anatase10.1107/S010876819100335X ↗