Oxidation and recrystallization of platinum group metals (Pt, Pd, Rh) in oxygen. Surface and subsurface reconstruction of polycrystalline platinum during annealing in the O2 atmosphere over the temperature range of 600–1400 K
Source abstract
Abstract
Abstract Scanning electron microscopy, energy-dispersive and X-ray photoelectron spectroscopies, as well as X-ray diffraction analysis were used to study the morphology, microstructure and chemical composition of surface and subsurface layers of Pt(poly) after treatment in O2 at T = 600–1400 K. It was found that the Pt(poly) microstructure is determined by the reaction of O2 with the surface carbon and platinum recrystallization. At T = 600–1000 K a part of the surface graphite-like film is removed and the surface microstructure remains virtually unchanged. The fcc lattice parameter of platinum (a), the size of the coherent scattering region (D), and microdistortion of the metal lattice (e) virtually do not change and are equal to 3.920 A, 100 nm and 0.05%, respectively. At T > 1000 K, the а value remains virtually constant and sizes of D, grains and microfacets substantially increase to ca. 500–600 nm, 40 and 1 μm, whereas the e value decreases to ca. 0.014%. At T = 600–1400 K, dissolution of oxygen in the platinum lattice and formation of bulk PtO2 oxide are not observed; however, oxygen is able to accumulate at grain boundaries and other defects in the amount of 5–10 at.%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Materials Characterization Techniques · Catalytic Processes in Materials Science · Electron and X-Ray Spectroscopy Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Matthey
2. Matthey
3. Matthey
4. Ignition-extinction of ethane-air mixtures over noble metals10.1023/A:1019010316753 ↗
5. Ignition in alkane oxidation on noble metal catalysts10.1016/S0920-5861(98)00302-2 ↗
6. Satterfield · 1980
7. Lloyd · 2011 · 120
8. Elementary steps in the catalytic oxidation of carbon monoxide on platinum metals10.1016/S0360-0564(08)60133-9 ↗
9. On the kinetics of oxygen adsorption on Pt(lll) surface10.1016/0039-6028(73)90053-8 ↗
10. The adsorption of oxygen on a stepped platinum single crystal surface10.1016/0039-6028(78)90190-5 ↗
11. Characterization of oxidized platinum surfaces by X-ray photoelectron spectroscopy10.1016/0039-6028(84)90778-7 ↗
12. Study of multilayer surface oxidation of platinum by electrical resistance technique10.1016/0039-6028(78)90106-1 ↗
13. Reactions of oxygen with the Platinum metals10.1595/003214065X925156 ↗
14. Platinum recovery in ammonia oxidation plants10.1595/003214069X13128 ↗
15. Morphology and etching processes on macroscopic metal catalysts10.1016/0079-6816(79)90001-7 ↗
16. Catalytic etching of platinum in NH3 oxidation10.1016/0021-9517(74)90165-1 ↗
17. Etching of platinum–rhodium alloys in oxygen-containing atmospheres10.1016/j.jallcom.2005.04.164 ↗
18. Chemical vapor transport of platinum and rhodium with oxygen as transport agent10.1016/j.jcrysgro.2005.02.024 ↗
19. Kraehnert · 2005
20. Savitsky · 1989
21. Kofstad · 1966
22. Gottstein · 2004
23. Novikov · 1975
24. Goldstein · 2003
25. Feldman · 1986
26. Catalytic corrosion of platinoid gauzes in the oxidation of ammonia with air. Surface reconstruction of platinoid gauzes at 1133 K in air, in ammonia, and in the NH3 + O2 reaction medium10.1134/S0023158418010093 ↗
27. Moulder · 1995
28. Carbon in platinum and palladium10.1595/003214070X1411420 ↗
29. Microfaceting and thermodynamic stability of the surface under chemisorption conditions10.1007/s10975-005-0075-y ↗
30. X-ray line broadening from filed Aluminium and Wolfram10.1016/0001-6160(53)90006-6 ↗
31. Kazenas · 1976
32. Thermodynamics of the gaseous oxides of the platinum-group metals