Nanosecond laser-induced surface damage and material failure mechanism of single crystal CaF2 (111) at 355 nm
Source abstract
Abstract
Abstract Surface damage and material failure mechanism of CaF2 single crystal by 355 nm/6.8 ns laser pulses are systematically studied in this work. Surface damage characteristics, such as damage threshold, damage growth threshold, damage growth laws and damage growth coefficient of CaF2 crystal are carefully studied. Surface material cracking and local material vitrification (from CaF2 crystal to defective CaF2-x materials) are revealed. Material decomposition, oxidation and formation of Ca0, Ca2+and (F−-F−) centers in surface layer are illustrated. Laser-driven thermal accumulation and thermal-stress gradient in CaF2 crystal are calculated and discussed based on the theory of Fourier heat conduction and thermal-elastic constitutive equations. Theory analysis suggests that the material failure process in CaF2 crystal is mainly driven by significant thermal stress gradient. Thermal gradient induce the material decomposition and local vitrification in CaF2 crystal. Combined results on surface damage and material failure behavior are beneficial to understand nanosecond laser-driven modifications and damage in fluoride crystals at ultraviolet wavelength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Materials for high-energy laser windows: oxyfluoride glass vs. fusion-cast CaF210.1117/12.603242 ↗
2. Evaluation of high-quality CaF2 single crystals for ultraviolet laser applications10.1117/12.584849 ↗
3. Improvements in CaF2 material properties for next-generation microlithography applications10.1117/12.534578 ↗
4. Laser grade CaF2 with controllable properties: growing conditions and structural imperfection10.1088/0022-3727/40/24/014 ↗
5. Properties of large CaF2 crystals grown by CZ method for lens materials10.1117/12.556614 ↗
6. Exterior surface damage of calcium fluoride outcoupling mirrors for DUV lasers10.1364/OE.17.008253 ↗
7. The role of defects in laser surface damage thresholds of fluoride crystals10.1007/BF00616299 ↗
8. Laser damage of CaF2 (111) surfaces at 248 nm10.1016/0169-4332(95)00440-8 ↗
9. Spectroscopic studies of pulsed-laser-induced damage sites in heated CaF2 crystals10.1117/12.344449 ↗
10. Accelerated damage to blank and antireflectance-coated CaF2 surfaces under 157-nm laser irradiation10.1117/12.485470 ↗
11. Improved laser damage threshold performance of calcium fluoride optical surfaces via Accelerated Neutral Atom Beam (ANAB) processing
12. Laser-induced damage of F-SiO2 protected fluoride-based AR coatings on subsurface-damage-free CaF2 at 193 nm10.1117/12.2243783 ↗
13. Long-term damage test of CaF2 optical window under irradiation of 4ω Nd:YAG laser10.1143/JJAP.43.644 ↗
14. The formation of metallic nanoparticles in single crystal CaF2 under 157 nm excimer laser irradiation10.1063/1.2177931 ↗
15. Investigation in the degradation of CaF2 outcouplers in excimer lasers operating at 193nm
16. Nano-second UV laser damage and ablation from fluoride crystals polished by different techniques10.1007/s003390051520 ↗
17. Laser-induced front side etching of CaF2 crystals with KrF excimer laser10.1016/j.apsusc.2012.11.067 ↗
18. Sem-analysis of fracture features formed in excimer-laser induced surface damage of CaF210.1080/10420159508218812 ↗
19. Study of haze in 193 nm high dose irradiated CaF2 crystals10.1117/12.836409 ↗
20. 248 nm high fluence irradiation of CaF2 crystals10.1117/12.752813 ↗
21. Laser-damage processes in cleaved and polished CaF2 at 248 nm10.1117/12.240356 ↗
22. Laser damage of cleaved and polished CaF2 at 248 nm10.1016/0168-583X(96)00061-4 ↗
23. Surface quality and laser-damage behavior of chemo-mechanically polished CaF2 single crystals characterized by scanning electron microscopy10.1023/A:1004695217861 ↗
24. Laser-stimulated desorption and damage at polished CaF2 surfaces irradiated with 532 nm laser light10.1016/0168-583X(94)96299-5 ↗
25. Comparison of volumetric and surface heating sources in the modeling of laser melting of ceramic materials
26. A universal theoretical model for thermal integration in materials during repetitive pulsed laser-based processing10.1016/j.ijleo.2018.05.061 ↗
27. Weber · 2003 · Vol. IV
28. Summary abstract: laser etching and evaporation of CaF2 studied by mass spectrometry10.1116/1.583667 ↗
29. Local devitrification on an oxyfluoride glass doped with Ho3+ ions under Argon laser irradiation10.1016/j.optmat.2008.10.015 ↗
30. Formation of metallic colloids in CaF2 by intense ultraviolet light10.1063/1.3673301 ↗
31. Dynamics of the plume containing nanometric-sized particles ejected into the atmospheric air following laser-induced breakdown on the exit surface of a CaF2 optical window10.1063/1.4862815 ↗
32. Handbook of X-ray photoelectron
33. Characterization of Ca aggregates on CaF2 (111)-surfaces by atomic force, XPS, and fluorescence microscopy10.1016/0168-583X(94)96298-7 ↗