journal article·2021-12

Wetting and joining of surface-oxidized SiC ceramic with calcium lithium aluminosilicate glass filler

Jian Fang, Liangbo Sun, Songsong Guo, Tipeng Shan, Yue Wen, Chunfeng Liu, Jie Zhang

Publisher page

Abstract

Abstract A novel strategy was developed to join SiC ceramics via a two-step method (i.e., SiC surface was modified by pre-oxidation treatment before bonding) using CaO-Li2O-Al2O3-SiO2 (CLAS) glass as the joining material. The wetting behavior, joint microstructure, bonding strength, fracture characteristics, and joining mechanism were investigated. Due to the formation of the SiO2 layer on the SiC surface by the pre-oxidation, the wettability of CLAS glass solder on the SiC matrix was significantly improved and the interfacial bonding was also enhanced. The microstructure of the joint revealed that the nanoscale eutectic structure composed of wollastonite and spodumene and the rod-shaped anorthite with micron-size were the main products in the joint seam. Besides, the content and size of anorthite in the joints increased with the increase of the joining temperature. Compared with one-step joining, the two-step method can obtain more reliable SiC/SiC joints due to the strong interfacial bonding. As a result, the optimal shear strength of 127 MPa was achieved at a joining temperature of 1240 °C, which was 119% higher than that obtained by the one-step joining method.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Microwave Dielectric Ceramics Synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. The effect of oxide, carbide, nitride and boride additives on properties of pressureless sintered SiC: A review10.1016/j.jeurceramsoc.2019.02.042 ↗
2. Microstructural design of sliding wear sliding wear-resistant liquid-phase-sintered SiC: an overview10.1016/j.jeurceramsoc.2007.02.190 ↗
3. Fabrication of SiC ceramic architectures using stereolithography combined with precursor infiltration and pyrolysis10.1016/j.ceramint.2019.04.100 ↗
4. Wetting of polycrystalline SiC by molten Al and Al-Si alloys10.1016/j.apsusc.2014.08.055 ↗
5. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
6. Recent progress in the development of SiC composites for nuclear fusion applications10.1016/j.jnucmat.2018.06.017 ↗
7. A structural model for multi-layered ceramic cylinders and its application to silicon carbide cladding of light water reactor fuel10.1016/j.jnucmat.2014.12.013 ↗
8. Study on Compatibility Between Silicon Carbide and Solid Breeding Materials Under Neutron Irradiation10.13182/FST11-A12367 ↗
9. Non-destructive evaluation of the strain distribution in selected-area He+ ion irradiated 4H-SiC10.1016/j.apsusc.2019.144051 ↗
10. Coupled effects of electronic and nuclear energy deposition on damage accumulation in ion-irradiated SiC10.1016/j.actamat.2020.08.014 ↗
11. Corrosion behavior of ion-irradiated SiC in FLiNaK molten salt10.1016/j.corsci.2019.108229 ↗
12. Measurement of swelling-induced residual stress in ion implanted SiC, and its effect on micromechanical properties10.1016/j.actamat.2020.06.030 ↗
13. Seamless joining of silicon carbide ceramics through an sacrificial interlayer of Dy3Si2C210.1016/j.jeurceramsoc.2019.09.002 ↗
14. Joining of β-SiC by spark plasma sintering10.1016/j.jeurceramsoc.2013.12.023 ↗
15. Joining technology—A challenge for the use of SiC components in HTRs10.1016/j.nucengdes.2015.12.022 ↗
16. Radiation-tolerant joining technologies for silicon carbide ceramics and composites10.1016/j.jnucmat.2013.10.002 ↗
17. Progress in development of SiC-based joints resistant to neutron irradiation10.1016/j.jeurceramsoc.2019.10.055 ↗
18. Microstructures of diffusion bonded SiC ceramics using Ti and Mo interlayers10.1016/j.jnucmat.2013.07.008 ↗
19. Microstructures of laser bonded SiC ceramics with Zr interlayers10.1016/j.jnucmat.2014.08.014 ↗
20. Nano-infiltration and transient eutectic (NITE) phase joining SiC ceramics at 1500 °C10.1016/j.ceramint.2019.08.193 ↗
21. Effects of neutron irradiation on mechanical properties of silicon carbide composites fabricated by nano-infiltration and transient eutectic-phase process10.1016/j.jnucmat.2013.10.005 ↗
22. A dual-phase microstructural approach to damage and fracture of Ti3SiC2/SiC joints10.1016/j.jnucmat.2017.11.054 ↗
23. Pressureless joining of silicon carbide using Ti3SiC2 MAX phase at 1500 °C10.1016/j.ceramint.2020.02.155 ↗
24. Joining of SiC monoliths using a thin MAX phase tape and the elimination of joining layer by solid-state diffusion10.1016/j.jeurceramsoc.2018.04.006 ↗
25. High temperature properties of the monolithic CVD β-SiC materials joined with a pre-sintered MAX phase Ti3SiC2 interlayer via solid-state diffusion bonding10.1016/j.jeurceramsoc.2016.11.006 ↗
26. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology10.1016/j.jnucmat.2015.08.004 ↗
27. Microwave assisted combustion synthesis in the system Ti–Si–C for the joining of SiC: Experimental and numerical simulation results10.1016/j.jeurceramsoc.2013.03.005 ↗
28. A heat-resistant preceramic polymer with broad working temperature range for silicon carbide joining10.1016/j.jeurceramsoc.2017.08.033 ↗
29. Joining of SiCf/SiC using polycarbosilane and polysilazane preceramic mixtures10.1016/j.ceramint.2018.03.061 ↗
30. Radiation stable, hybrid, chemical vapor infiltration/preceramic polymer joining of silicon carbide components10.1016/j.jnucmat.2017.02.012 ↗
31. Joining of SiC ceramics via a novel liquid preceramic polymer (V-PMS)10.1016/j.ceramint.2015.02.008 ↗
32. Effects of neutron irradiation on glass ceramics as pressure-less joining materials for SiC based components for nuclear applications10.1016/j.jnucmat.2012.05.035 ↗
33. He-irradiation effects on glass-ceramics for joining of SiC-based materials10.1016/j.jnucmat.2016.01.024 ↗
34. Microstructure and properties of SiCf/SiC joint brazed by Y-Al-Si-O glass10.1016/j.ceramint.2018.02.092 ↗
35. Ytterbium disilicate-based glass-ceramic as joining material for ceramic matrix composites10.1016/j.jeurceramsoc.2020.10.022 ↗
36. Y2O3–Al2O3–SiO2-based glass-ceramic fillers for the laser-supported joining of SiC10.1016/j.jeurceramsoc.2014.01.019 ↗
37. CaO-Al2O3 glass-ceramic as a joining material for SiC based components: A microstructural study of the effect of Si-ion irradiation10.1016/j.jnucmat.2018.01.033 ↗
38. Joining of SiC ceramics using CaO-Al2O3-SiO2 (CAS) glass ceramics10.1016/j.jeurceramsoc.2019.09.030 ↗
39. Microstructure and mechanical properties of SiCf/SiC joints brazed using CaO-MgO-Al2O3-SiO2 glass10.1016/j.ceramint.2019.01.218 ↗
40. Study of Li2O addition on crystallization behavior and thermal expansion properties of CaO-Al2O3–SiO2 (CAS) glass-ceramic and its application for joining SiC ceramic10.1016/j.jeurceramsoc.2020.10.061 ↗
41. High temperature oxidation behaviors of bulk SiC with low partial pressures of air and water vapor in argon
42. Oxidation Transitions for SiC Part I. Active-to-Passive Transitions10.1111/jace.12108 ↗
43. Joining pre-oxidized dense Si3N4 to porous Si3N4 with β-spodumene based glass-ceramic interlayer10.1016/j.apsusc.2019.03.124 ↗
44. Joining of SiC-based materials for nuclear energy applications10.1016/j.jnucmat.2010.12.160 ↗
45. Microstructure and mechanical properties of low-activation glass-ceramic joining and coating for SiC/SiC composites10.1016/S0022-3115(00)00096-9 ↗
46. Interface structure and radiation damage resistance in Cu-Nb multilayer nanocomposites10.1103/PhysRevLett.100.136102 ↗