Abstract
Abstract The structure and tribological properties of commercially pure titanium (cp-Ti) samples after non-vacuum electron beam surface alloying with carbon were studied. Two types of powders were used to introduce carbon in surface layer of cp-Ti: titanium carbide (TiC) and mixture of pure titanium and graphite (“Ti + C”). Single layer and multilayer coatings were studied. Application of electron beam for alloying provided cladding rate of 4.5 m 2 /h. The thickness of the clad coatings was 1.6–2.0 mm. The main phases received after “Ti + C” powder cladding were α-titanium, TiC, and retained graphite. In the samples obtained by cladding of TiC, graphite was not observed. A factor determining the microhardness and tribological properties of the cladded layer was the volume fraction of TiC. Maximum coating microhardness of 8 GPa was obtained by cladding of single layer of TiC powder or two layers of the “Ti + C” mixture. Two types of tests were carried out to evaluate the wear resistance of the samples. In friction tests against loose abrasive particles, the wear rate of the best samples was 9.3 times lower than that of cp-Ti. In wear tests using fixed abrasive particles, the relative wear resistance of the best samples was 2.3 times higher than that of cp-Ti.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Pulsed Power Technology Applications · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Surface carburizing of Ti–6Al–4V alloy by laser melting10.1016/j.optlaseng.2009.11.001 ↗
2. (Ti,Al)/(Ti,Al)N coatings produced by laser surface alloying10.1016/S0167-577X(01)00451-7 ↗
3. Laser surface nitriding of titanium and a titanium alloy10.1016/0924-0136(95)02110-8 ↗
4. Effects of nitrogen gas flow rates on the microstructure and properties of laser-nitrided IMI318 titanium alloy (Ti–4V–6Al)10.1016/S0924-0136(97)00408-1 ↗
5. Enhancing the microstructure and properties of titanium alloys through nitriding and other surface engineering methods10.1016/j.surfcoat.2004.07.115 ↗
6. Surface nitriding of Ti–6Al–4V alloy with a high power CO2 laser10.1016/j.optlastec.2007.07.005 ↗
7. Improvement of the hardness and wear resistance of (TiC, TiN)/Ti–6Al–4V surface-alloyed materials fabricated by high-energy electron-beam irradiation10.1007/s11661-001-0174-y ↗
8. Microstructural modification and property improvement of boride/Ti–6Al–4V surface-alloyed materials fabricated by high-energy electron-beam irradiation10.1007/s11661-001-0039-4 ↗
9. Improvement of high-temperature hardness of (TiC, TiB)/Ti–6Al–4V surface composites fabricated by high-energy electron-beam irradiation10.1016/j.surfcoat.2003.10.017 ↗
10. Correlation of microstructure with hardness and fracture properties of (TiC,SiC)/Ti–6Al–4V surface composites fabricated by high-energy electron-beam irradiation10.1016/S0257-8972(03)00811-9 ↗
11. Cladding of tantalum and niobium on titanium by electron beam, injected in atmosphere
12. Atmospheric electron-beam cladding of carbon containing powder mixtures onto technically pure titanium VT1-0
13. Surface modification of TA2 pure titanium by low energy high current pulsed electron beam treatments10.1016/j.apsusc.2011.03.005 ↗
14. Microstructure and property modifications in a near α Ti alloy induced by pulsed electron beam surface treatment10.1016/j.surfcoat.2011.07.017 ↗
15. Microstructure and defect of titanium alloy electron beam deep penetration welded joint10.1016/S1003-6326(11)61510-0 ↗
16. B. Courant, H.J. J., S. Benayoun, Surface treatment of titanium by laser irradiation to improve resistance to dry-sliding friction, Wear 236 (1999) 39–46.10.1016/S0043-1648(99)00254-9 ↗
17. Surface modification of TC4 Ti alloy by laser cladding with TiC+Ti powders10.1016/S1003-6326(09)60441-6 ↗
18. Structure and properties of steel under non-vacuum electron-beam welding deposition of titani-um, tantalum, molybdenum and graphite powders
19. Laser cladding of Ti–6Al–4V alloy with TiC and TiC+NiCrBSi powders10.1016/S0257-8972(00)01082-3 ↗
20. Microstructure and tribological properties of in situ synthesized TiC, TiN, and SiC reinforced Ti3Al intermetallic matrix composite coatings on pure Ti by laser cladding10.1016/j.apsusc.2008.07.180 ↗
21. Laser fabrication of Ti6Al4V/TiC composites using simultaneous powder and wire feed10.1016/j.msea.2006.09.093 ↗
22. Microstructure and wear properties of TiCN/Ti coatings on titanium alloy by laser cladding10.1016/j.optlaseng.2009.08.003 ↗
23. Temperature dependence of morphology of TiC reinforcement in in situ Ti-6Al/TiC composites10.1023/A:1010981029110 ↗
24. In situ formation of titanium carbide using titanium and carbon-nanotube powders by laser cladding10.1016/j.apsusc.2011.11.058 ↗
25. Structure of surface layers produced by non-vacuum electron beam boriding10.1016/j.apsusc.2013.07.121 ↗
26. Surface hardening of steels with carbon by non-vacuum electron-beam processing10.1016/j.surfcoat.2014.01.038 ↗
27. Standard Test Method for Measuring Abrasion Using the Dry Sand/Rubber Wheel Apparatus, in, ASTM International, 2010.