journal article·2015-10

Characteristics of laser textured silicon surface and effect of mud adhesion on hydrophobicity

B.S. Yilbas, H. Ali, M. Khaled, N. Al-Aqeeli, N. Abu-Dheir, K.K. Varanasi

Publisher page

Abstract

Abstract Laser gas assisted texturing of silicon wafer surface is carried out. Morphological and metallurgical changes in the treated layer are examined using the analytical tools. Microhardness and fracture toughness of the laser treated surface are measured using the indentation technique while residual stress formed is determined from the X-ray diffraction data. The hydrophobicity of the textured surfaces are assessed incorporating the contact angle data and compared with those of as received workpiece surfaces. Environmental dust accumulation and mud formation, due to air humidity, at the laser treated and as received workpiece surfaces are simulated and the effect of the mud residues on the properties of the laser treated surface are studied. The adhesion work due to the presence of the mud on the laser treated surface is also measured. It is found that laser textured surface composes of micro/nano poles and fibers, which in turn improves the surface hydrophobicity significantly. In addition, formation of nitride species contributes to microhardness increase and enhancement of surface hydrophobicity due to their low surface energy. The mud residues do not influence the fracture toughness and microhardness of the laser textured surface; however, they reduced the surface hydrophobicity significantly.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Modification and Superhydrophobicity · Adhesion, Friction, and Surface Interactions · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Silicon substrate as a novel cell culture device for myoblast cells10.1186/1423-0127-21-47 ↗
2. Electric current dependence of a self-cooling device consisting of silicon wafers connected to a power MOSFET10.1007/s11664-013-2856-9 ↗
3. Electronic devices on various substrates: fabrication of releasable single-crystal silicon–metal oxide field-effect devices and their deterministic assembly on foreign substrates10.1002/adfm.201190063 ↗
4. Efficient black silicon solar cell with a density-graded nanoporous surface: optical properties, performance limitations, and design rules10.1063/1.3231438 ↗
5. N-type black silicon solar cells10.1016/j.egypro.2013.07.358 ↗
6. Self-cleaning surfaces—virtual realities10.1038/nmat856 ↗
7. Study on surface tension and adhesion for flip chip packaging
8. Reaction-bonded silicon nitride: its formation and properties10.1007/BF00561287 ↗
9. Laser treatment of silicon at nitrogen ambient: thermal stress analysis10.1179/174329409X409495 ↗
10. Laser treatment of zirconia surface for improved surface hydrophobicity10.1016/j.jallcom.2014.11.069 ↗
11. Falling dust characteristics in Riyadh City, Saudi Arabia during winter months
12. Progressive evolution of silicon surface microstructures via femtosecond laser irradiation in ambient air10.1016/j.apsusc.2014.06.105 ↗
13. Direct modification of silicon surface by nanosecond laser interference lithography10.1016/j.apsusc.2013.05.042 ↗
14. Ellipsometric analysis of silicon surfaces textured by ns and sub-ps KrF laser pulses10.1016/j.tsf.2013.10.102 ↗
15. Fabrication of luminescent a-Si:SiO2 structures by direct irradiation of high power laser on silicon surface10.1016/j.apsusc.2014.03.168 ↗
16. Comparison of structures and hydrophobicity of femtosecond and nanosecond laser-etched surfaces on silicon10.1016/j.apsusc.2012.08.092 ↗
17. Sub-wavelength surface structures on silicon irradiated by femtosecond laser pulses at 1300 and 2100nm wavelengths10.1016/j.apsusc.2006.11.004 ↗
18. Femtosecond laser-induced formation of surface structures on silicon and glassy carbon surfaces10.1016/j.phpro.2011.03.101 ↗
19. Influence of irradiation dose on laser-induced surface nanostructures on silicon10.1016/j.apsusc.2012.10.140 ↗
20. Pulsed TEA CO2 laser surface modifications of silicon10.1016/S0169-4332(02)01156-X ↗
21. Modification of wetting properties of laser-textured surfaces by depositing triboelectrically charged Teflon particles10.1007/s00396-012-2757-0 ↗
22. Residual stress in plasma electrolytic oxidation coatings on Al alloy produced by pulsed unipolar current10.1016/j.surfcoat.2005.08.092 ↗
23. Activated reactive evaporation deposited silicon nitride as a masking material for MEMS fabrication10.1088/0960-1317/15/10/023 ↗
24. Determination of surface stress of high temperature ceramic material
25. Fracture toughness and crack morphologies in eroded WC–Co–Cr thermally sprayed coatings10.1016/S0167-577X(98)00092-5 ↗
26. Surface treatment of plasma sprayed ceramic coatings by a laser beam10.1016/0257-8972(88)90089-8 ↗
27. Quasi-static solid particle damage in brittle solids—I. Observations analysis and implications10.1016/0001-6160(76)90042-0 ↗
28. Indentation fracture toughness of brittle materials for palmqvist cracks10.1007/978-1-4613-3488-0_7 ↗
29. High-strength silicon nitride ceramics obtained by grain-boundary crystallization10.1007/BF02403951 ↗
30. Self-interstitials and thermal donor formation in silicon: new measurements and a model for the defects10.1088/0022-3719/16/19/002 ↗
31. The influence of gas jet velocity in laser heating-a moving workpiece case10.1243/0954406001523524 ↗
32. Neumann · 1979 · vol. II
33. Enhanced condensation on lubricant-impregnated nanotextured surfaces10.1021/nn303867y ↗
34. Recent progress in preparation of superhydrophobic surfaces: a review
35. Wettability of porous surfaces10.1039/tf9444000546 ↗
36. Resistance of solid surfaces to wetting by water10.1021/ie50320a024 ↗
37. Self-cleaning efficiency of artificial superhydrophobic surfaces10.1021/la803860d ↗
38. Self-cleaning efficiency of artificial superhydrophobic surfaces10.1021/la803860d ↗
39. Surface energy of fusion bonded silicon nitride to silicon
40. Low hydrogen content stoichiometric silicon-nitride films deposited by plasma-enhanced chemical vapor-deposition10.1063/1.349544 ↗
41. Local atomic-structure in thin-films of silicon-nitride and silicon diimide produced by remote plasma-enhanced chemical-vapor deposition10.1103/PhysRevB.33.7069 ↗
42. Development of PMMA-precoating metal prostheses via injection molding: residual stresses10.1002/jbm.1041 ↗
43. Adhesion and cohesion10.1155/2012/951324 ↗