Effect of welding thermal cycles on the oxidation resistance of 9 wt.% Cr heat resistant steels in 550 °C lead-bismuth eutectic
Source abstract
Abstract
Abstract The oxidation resistance for the heat affected zone (HAZ) and base metal of 9 wt.% Cr heat resistant steel in 550 °C lead-bismuth eutectic has been investigated. The oxide film presents a three-layer structure. The outer layer is Fe3O4 while the inner layer is mainly FeCr2O4. The oxide film thickness becomes thinner and thinner in turns of the coarse grained HAZ, fine grained HAZ, inter-critical HAZ and base metal. The oxygen diffusion is the rate determining step during the oxidation process. The Cr-enriched M23C6 plays a significant role on the oxidation rate at the initial stage of oxidation. Increasing the carbon content is a useful method to improve the oxidation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
2. Assessment of the influence of surface finishing and weld joints on the corrosion/oxidation behaviour of stainless steels in lead bismuth eutectic10.1016/j.jnucmat.2010.12.230 ↗
3. HCM12A Cr-rich oxide layer investigation using 3D atom probe10.1016/j.jnucmat.2013.09.011 ↗
4. Elevated temperature ferritic and martensitic steels and their application to future nuclear reactors10.1179/174328005X41140 ↗
5. Physical—chemical principles of lead—bismuth coolant technology
6. High temperature oxidation of Fe-9Cr-1Mo steel in liquid metal10.4028/www.scientific.net/MSF.595-598.519 ↗
7. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
8. Oxidation mechanism of steels in liquid–lead alloys10.1007/s11085-005-4392-3 ↗
9. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb–Bi eutectic alloy (Part III)10.1016/j.corsci.2008.06.049 ↗
10. Oxidation mechanism of an Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy at 470°C (Part II)10.1016/j.corsci.2008.06.051 ↗
11. Modeling of oxidation of structural materials in LBE systems10.1016/j.jnucmat.2007.07.022 ↗
12. Heat and mass transfer calculations in heavy liquid metal loops under forced convection flow conditions10.1016/j.jnucmat.2005.05.013 ↗
13. Corrosion scales on various steels after exposure to liquid lead–bismuth eutectic10.1016/j.jnucmat.2013.09.034 ↗
14. Corrosion behaviour of steels in lead–bismuth at 823K,10.1016/j.jnucmat.2004.07.013 ↗
15. Nano-indentation measurement of oxide layers formed in LBE on F/M steels10.1016/j.jnucmat.2008.02.073 ↗
16. A model for mild steel oxidation in CO210.1007/BF00610578 ↗
17. Corrosion of carbon steels in high temperature acid chloride solutions10.1016/0010-938X(91)90105-X ↗
18. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
19. Fracture toughness of low activation ferritic steel (JLF-1) weld joint at room temperature10.1016/S0022-3115(98)00172-X ↗
20. Production and preliminary characterization of ferritic–martensitic steel T91 cladding tubes for LBE or Pb cooled nuclear systems10.1016/j.jnucmat.2011.04.053 ↗
21. Long-term corrosion behavior of martensitic steel welds in static molten Pb–17Li alloy at 550°C10.1016/j.corsci.2015.04.001 ↗
22. Microstructure of heat resistant chromium steel weld metals10.1016/0169-4332(94)00491-9 ↗
23. Thermal cycling, microstructure and mechanical properties of 9Cr2WVTa steel welds10.1016/j.jmatprotec.2015.03.017 ↗
24. An overview of the welding technologies of CLAM steels for fusion application10.1016/j.fusengdes.2012.06.009 ↗
25. Compatibility of CLAM steel weldments with static LiPb alloy at 550°C10.1016/j.fusengdes.2012.04.012 ↗
26. Stress corrosion of 1. 4914 steel in Pb-17Li and liquid metal embrittlement (LME) susceptibility of its welded structure
27. Compatibility of ferritic–martensitic steel T91 welds with liquid lead–bismuth eutectic: comparison between TIG and EB welds10.1016/j.jnucmat.2009.10.054 ↗
28. Compatibility of martensitic/austenitic steel welds with liquid lead bismuth eutectic environment10.1016/j.jnucmat.2008.12.043 ↗
29. Mechanical properties of a 316L/T91 weld joint tested in lead–bismuth liquid10.1016/j.matdes.2009.01.038 ↗
30. Bischoff · 2016
31. Liquid metal embrittlement susceptibility of welded MANET II (DIN 1.4914) in liquid Pb-17Li10.1016/0022-3115(95)00185-9 ↗
32. Microstructural evolution and mechanical properties of heat affected zones for 9Cr2WVTa steels with different carbon contents10.1016/j.matdes.2014.08.018 ↗
33. Effect of vanadium on microstructure and mechanical properties of TIG weld joint of China low activation martensitic steel10.1007/s10894-015-9904-9 ↗
34. Effect of silicon contents on the microstructures and mechanical properties of heat affected zones for 9Cr2WVTa steels10.1016/j.jnucmat.2015.11.055 ↗
35. On the mechanism of sulphide scale formation on iron10.1016/S0010-938X(65)80018-X ↗
36. Effects of dilute substitutional solutes on interstitial carbon in α-Fe: interactions and associated carbon diffusion from first-principles calculations10.1103/PhysRevB.90.024103 ↗
37. Thermal stability and the structure of vacancy–solute clusters in iron alloys10.1016/j.actamat.2014.11.026 ↗
38. Effects of pre-formed nanostructured surface layer on oxidation behaviour of 9Cr2WVTa steel in air and liquid Pb–Bi eutectic alloy10.1016/j.corsci.2015.10.021 ↗
39. Oxidation behavior of ferritic/martensitic steels in stagnant liquid LBE saturated by oxygen at 600°C
40. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
41. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
42. Microstructural investigation of the oxidation of an Fe-3 pct Cr alloy10.1007/BF02648380 ↗
43. Microstructure and elevated-temperature erosion-oxidation behaviour of aluminized 9Cr-1Mo Steel10.1016/j.apsusc.2012.07.096 ↗
44. Microstructure and stress distribution on TIG welded joint of CLAM steel10.1007/s10894-015-9910-y ↗
45. Lim · 2006
46. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
47. Cation diffusion in cr2 O 310.1149/1.2427973 ↗
48. Self-diffusion of iron in iron oxides and the Wagner theory of oxidation
49. Determination of oxygen diffusion rates in magnetite from natural isotopic variations10.1130/0091-7613(1991)019<0653:DOODRI>2.3.CO;2 ↗
50. Liquid metal embrittlement (LME) susceptibility of the 8–9% Cr martensitic steels F82H-mod., OPTIFER IVb and their simulated welded structures in liquid Pb–17Li10.1016/S0022-3115(00)00097-0 ↗
51. Corrosion analysis of CLAM steel in flowing liquid LiPb at 480°C10.1016/j.fusengdes.2010.06.021 ↗
52. Effect of alloy grain size and silicon content on the oxidation of austenitic Fe-Cr-Ni-Mn-Si alloys in pure O210.1007/BF00662967 ↗