Abstract

A degenerated wide bandgap semiconductor is a rare system. In general, implant levels lie deeper in the band-gap and carrier freeze-out usually takes place at room temperature. Nevertheless, we have observed that heavily doped n-type degenerated 3C-SiC films are achieved by nitrogen implantation level of ∼6x1020cm-3 at 20K. According to temperature dependent Hall measurements, nitrogen activation rates decrease with the doping level from almost 100% (1.5x1019cm-3, donor level 15meV) to ∼12% for 6x1020cm-3. Free donors are found to saturate in 3C-SiC at ∼7x1019cm-3. The implanted film electrical performances are characterized as a function of the dopant doses and post implantation annealing (PIA) conditions by fabricating Van der Pauw structures. A deposited SiO2 layer was used as the surface capping layer during the PIA process to study its effect on the resultant film properties. From the device design point of view, the lowest sheet resistivity (∼1.4mΩ.cm) has been observed for medium doped (4x1019cm-3) sample with PIA 1375 °C 2 h without a SiO2 cap.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. (Invited) high quality 3C-SiC for MOS applications10.1149/1.3631504 ↗
2. Reliable method for eliminating stacking fault on 3C-SiC (001)10.4028/www.scientific.net/MSF.717-720.173 ↗
3. Bow free 4″ diameter 3C-SiC epilayers formed upon wafer-bonded Si/SiC substrates10.1149/2.007206ssl ↗
4. Development of 3C-SiC MOSFETs
5. Nickel Ohmic contacts to N-implanted (0001) 4H-SiC10.1007/s11664-010-1128-1 ↗
6. Jones · 1993
7. Surface roughening in ion implanted 4H-silicon carbide10.1007/s11664-999-0016-z ↗
8. Electronic behaviors of high-dose phosphorus-ion implanted 4H–SiC (0001)10.1063/1.1756213 ↗
9. Protection of selectively implanted and patterned silicon carbide surfaces with graphite capping layer during post-implantation annealing10.1088/0268-1242/20/3/003 ↗
10. A comparison of the AlN annealing cap for 4H SiC annealed in a nitrogen versus an argon atmosphere
11. Annealing ion implanted SiC with an AlN cap10.1016/S0921-5107(98)00518-2 ↗
12. Using a PLD BN/AlN composite as an annealing cap for ion implanted SiC
13. Structural and transport properties in alloyed Ti/Al Ohmic contacts formed on p-type Al-implanted 4H-SiC annealed at high temperature10.1088/0022-3727/44/25/255302 ↗
14. Structural and chemical comparison of graphite and BN/AlN caps used for annealing ion implanted SiC10.1007/s11664-008-0405-8 ↗
15. Effect of graphite cap for implant activation on inversion channel mobility in 4H-SiC MOSFETs
16. Study of SiO2 encapsulation for aluminum and phosphorus implant activation in 4H-SiC10.1016/j.matlet.2010.08.048 ↗
17. Structural and electrical characterizations of n-type implanted layers and ohmic contacts on 3C-SiC10.1016/j.nimb.2011.06.004 ↗
18. Ti–Ni ohmic contacts on 3C–SiC doped by nitrogen or phosphorus implantation10.1016/j.mseb.2010.03.084 ↗
19. Electrical characterization of nitrogen implanted 3C-SiC by SSRM and CTLM measurements
20. Regrowth of 3C-SiC on CMP treated 3C-SiC/Si epitaxial layers10.4028/www.scientific.net/MSF.483-485.197 ↗
21. Surface melt patterns on silicon10.1107/S0365110X58001080 ↗
22. Improved performance of 4H-SiC PiN diodes using a novel combined high temperature oxidation and annealing process10.1109/TSM.2014.2336701 ↗
23. Contact phenomena and interactions in the system SiC-SiO2-R x O y in condensed matter10.1007/BF00361533 ↗
24. Electrical properties of N ion implanted layer in 3C-SiC (100) grown on self-standing 3C-SiC substrate10.4028/www.scientific.net/MSF.556-557.579 ↗
25. Schroder · 2006
26. Growth of high-mobility 3C-SiC epilayers by chemical vapor deposition10.1143/JJAP.27.L434 ↗
27. Dose influence on physical and electrical properties of nitrogen implantation in 3C-SiC on Si10.4028/www.scientific.net/MSF.711.154 ↗
28. Temperature dependence of electrical properties of nitrogen-doped 3C-SiC10.1143/JJAP.26.L533 ↗
29. High-temperature electrical properties of 3C-SiC epitaxial layers grown by chemical vapor deposition”10.1063/1.94973 ↗
30. High temperature high-dose implantation of aluminum in 4H-SiC10.1063/1.1764934 ↗
31. Hopping conduction in heavily doped bulk n-type SiC10.1007/s11664-997-0135-3 ↗
32. Modelling the metal–semiconductor band structure in implanted ohmic contacts to GaN and SiC10.1088/0965-0393/21/3/035004 ↗
33. Compensation in epitaxial cubic SiC films10.1063/1.97048 ↗
34. The location and shape of the conduction band minima in cubic silicon carbide10.1016/0022-2313(77)90030-8 ↗
35. Electron cyclotron resonance in cubic SiC10.1016/0038-1098(85)91107-X ↗