Abstract

Abstract Plasma processing has been widely reported as an effective tool in relieving or removing surface/subsurface damage induced by previous mechanical machining process. However, the surface morphology evolution during removing the damage using plasma processing is rarely reported. In this research, this procedure is studied based on experiments and robust numerical models developed on the basis of Level Set Method (LSM). Even if some unique properties of plasma etching are observed, such as particle redistribution, the dominant role of isotropic etching of plasma processing is verified based on experiments and 2D LSM simulations. With 2D LSM models, the damage removal process under various damage characteristics is explored in detail. Corresponding peak-to-valley roughness evolution is investigated as well. Study on morphology evolution is also conducted through the comparison between experiments and 3D LSM computations. The modeling results and experiments show good agreement with each other. The trends of simulated roughness evolution agree with the experiments as well. It is revealed that the plasma processing may end up with a planar surface depending on the damage characteristics. The planarization procedure can be divided into four parts: crack opening and pit formation; pit coalescing and shallow pits subsumed by deep ones; morphology duplicate etching; and finally a planar and damage free surface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Metal and Thin Film Mechanics · Advanced Machining and Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Surface/subsurface damage and the fracture strength of ground ceramics10.1016/0924-0136(95)02090-X ↗
2. Combining wet etching and real-time damage event imaging to reveal the most dangerous laser damage initiator in fused silica10.1364/OL.38.002632 ↗
3. Fracture-induced subbandgap absorption as a precursor to optical damage on fused silica surfaces10.1364/OL.35.002702 ↗
4. Surface roughening of ground fused silica processed by atmospheric inductively coupled plasma10.1016/j.apsusc.2015.03.001 ↗
5. Ultra-precision surface finishing by ion beam and plasma jet techniques—status and outlook10.1016/j.nima.2009.11.013 ↗
6. Ultra-Precision surface machining with reactive plasma jets10.1002/ctpp.201310058 ↗
7. Plasma jet machining a novel technology for precision machining of optical elements10.1002/vipr.201000423 ↗
8. Reactive atom plasma (RAP) figuring machine for meter class optical surfaces10.1007/s11740-013-0467-1 ↗
9. Shape correction of optical surfaces using plasma chemical vaporization machining with a hemispherical tip electrode10.1364/AO.51.000401 ↗
10. Rapid, noncontact optical figuring of aspheric surfaces with plasma assisted chemical etching (PACE)10.1117/12.22788 ↗
11. The morphology and chemistry evolution of fused silica surface after Ar/CF4 atmospheric pressure plasma processing10.1016/j.apsusc.2013.09.100 ↗
12. Basis of macroscopic and microscopic surface shaping and smoothing by plasma assisted chemical etching10.1116/1.587512 ↗
13. The dissolution of Na2O-MgOCaO-SiO2 glass in aqueous HF solutions10.1007/BF01132419 ↗
14. Wet chemical etching of silicate glasses in hydrofluoric acid based solutions10.1007/BF01352182 ↗
15. The effect of HF/NH4F etching on the morphology of surface fractures on fused silica10.1016/j.jnoncrysol.2009.01.037 ↗
16. Modeling wet chemical etching of surface flaws on fused silica10.1117/12.836912 ↗
17. Fronts propagating with curvature-dependent speed: algorithms based on Hamilton-Jacobi formulations10.1016/0021-9991(88)90002-2 ↗
18. Sethian · 1999
19. Osher · 2003
20. Chu
21. The flexible, extensible and efficient toolbox of level set methods10.1007/s10915-007-9174-4 ↗
22. Roughening in plasma etch fronts of Si(100)10.1103/PhysRevLett.82.4882 ↗
23. Microtrench formation in polysilicon plasma etching over thin gate oxide10.1149/1.2220831 ↗