A comparative analysis of Inconel 718 made by additive manufacturing and suction casting: Microstructure evolution in homogenization
Source abstract
Abstract
Homogenization is one of the critical stages in the post-heat treatment of additive manufacturing (AM) component to achieve uniform microstructure. During homogenization, grain coarsening could be an issue to reserve strength, which requires careful design of both time and temperature. Therefore, a proper design of homogenization becomes particularly important for AM design, for which work hardening is usually no longer an option. In this work, we discovered an intriguing phenomenon during homogenization of suction-cast and AM Inconel 718 superalloys. Through both short and long-term isothermal heat treatments at 1180°C, we observed an abnormal grain growth in the suction-cast alloy but continuous recrystallization in the alloy made by laser powder bed fusion (LPBF). The grain size of AM samples keeps as small as 130 μm and is even slightly reduced after homogenization for 12 hours. The homogeneity of Nb in the AM alloys is identified as the critical factor for NbC formation, which further influences the recrystallization kinetics at 1180°C. Multi-type dislocation behaviors are studied to elucidate the grain refinement observed in homogenized alloys after LPBF. This work provides a new pathway on microstructure engineering of AM alloys for improved mechanical performance superior to traditionally manufactured ones.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (97)
Show source-provided references
1. Physical aspects of process control in selective laser sintering of metals10.1002/adem.200310099 ↗
2. Binding mechanisms in selective laser sintering and selective laser melting10.1108/13552540510573365 ↗
3. Flexible manufacturing of metallic products by selective laser melting of powder10.1016/j.ijmachtools.2006.01.024 ↗
4. Single track formation in selective laser melting of metal powders10.1016/j.jmatprotec.2010.05.010 ↗
5. Laser additive manufacturing of ceramic components: materials, processes, and mechanisms
6. Linking process, structure, property, and performance for metal-based additive manufacturing: computational approaches with experimental support10.1007/s00466-015-1240-4 ↗
7. The microstructure and mechanical properties of deposited-IN718 by selective laser melting10.1016/j.jallcom.2011.10.107 ↗
8. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting10.1016/j.actamat.2011.12.032 ↗
9. On conventional versus direct ageing of Alloy 71810.1016/j.actamat.2018.06.034 ↗
10. Numerical modeling of heat-transfer and the influence of process parameters on tailoring the grain morphology of IN718 in electron beam additive manufacturing10.1016/j.actamat.2016.03.063 ↗
11. Multiscale modeling of the mechanical behavior of IN718 superalloy based on micropillar compression and computational homogenization10.1016/j.actamat.2015.07.006 ↗
12. Texture control during laser deposition of nickel-based superalloy10.1016/j.scriptamat.2012.06.014 ↗
13. Morphology of γ’ and γ" precipitates and thermal stability of Inconel 718 type alloys10.1007/BF02649604 ↗
14. Some aspects of the precipitation of metastable intermetallic phases in INCONEL 71810.1007/BF02647549 ↗
15. Aging effects on the microstructure and creep behavior of Inconel 718 superalloy10.1016/j.msea.2008.04.097 ↗
16. Keiser · 1976
17. Selective laser melting additive manufacturing of Inconel 718 superalloy parts: densification, microstructure and properties10.1016/j.jallcom.2013.09.171 ↗
18. Mechanical and microstructural investigation of nickel-based superalloy IN718 manufactured by selective laser melting (SLM)10.1002/adem.201500158 ↗
19. Effect of energy input on microstructural evolution of direct laser fabricated IN718 alloy10.1016/j.matchar.2015.06.027 ↗
20. Effect of different heat treatments on the microstructure and mechanical properties in selective laser melted INCONEL 718 alloy10.1080/10426914.2016.1257805 ↗
21. Grain structure control of additively manufactured metallic materials10.3390/ma10111260 ↗
22. Characterization of nano-scale oxides in austenitic stainless steel processed by powder bed fusion10.1016/j.scriptamat.2018.06.011 ↗
23. Effect of heat treatment on microstructure evolution of Inconel 718 alloy fabricated by selective laser melting10.1016/j.jallcom.2018.06.112 ↗
24. Solidification structures of Inconel 718 with microalloying elements10.7449/1994/Superalloys_1994_81_88 ↗
25. Laves phase in alloy 718 fusion zone—microscopic and calorimetric studies10.1016/j.matchar.2014.11.035 ↗
26. Investigations of MX and γ’/γ" precipitates in the nickel-based superalloy 718 produced by electron beam melting10.1016/j.msea.2007.07.012 ↗
27. Microstructure and mechanical properties of Inconel 718 electron beam welds10.1179/174328405X62260 ↗
28. Effect of heat treatment variations on the mechanical properties of Inconel 718 selective laser melted specimens
29. Comparison of microstructures and mechanical properties of Inconel 718 alloy processed by selective laser melting and casting10.1016/j.msea.2018.03.073 ↗
30. Improvement in stress rupture properties of inconel 718 gas tungsten arc welds using current pulsing10.1007/s10853-005-0590-2 ↗
31. Vacuum heat treatment of iron parts produced by selective laser melting: microstructure, residual stress and tensile behavior10.1016/j.matdes.2013.08.085 ↗
32. Effect of homogenization heat treatment on the microstructure and heat-affected zone microfissuring in welded cast alloy 71810.1007/BF02648966 ↗
33. The formation and control of Laves phase in superalloy 718 welds10.1023/A:1018541915113 ↗
34. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
35. Effect of annealing on the microstructure and magnetic properties of soft magnetic Fe-Si produced via laser additive manufacturing10.1016/j.scriptamat.2017.08.042 ↗
36. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting10.1016/j.msea.2015.05.035 ↗
37. Comparison of microstructures and mechanical properties of Inconel 718 alloy processed by selective laser melting and casting10.1016/j.msea.2018.03.073 ↗
38. Microstructure and mechanical properties of selective laser melted Inconel 718 compared to forging and casting10.1016/j.matlet.2015.10.136 ↗
39. Microstructure and anisotropic mechanical properties of EBM manufactured Inconel 718 and effects of post heat treatments10.1016/j.msea.2017.03.085 ↗
40. Microstructure and hardness studies of Inconel 718 manufactured by selective laser melting before and after solution heat treatment10.1016/j.msea.2017.02.062 ↗
41. Impact of heat treatment on mechanical behaviour of Inconel 718 processed with tailored microstructure by selective laser melting10.1016/j.matdes.2017.05.065 ↗
42. High Temp Metals, https://www.hightempmetals.com/techdata/hitempInconel718data.php (accessed November 3, 2019).
43. Special Metals, https://www.specialmetals.com/assets/smc/documents/inconel_alloy_718.pdf (accessed November 3, 2019).
44. ASTM International · 2018 · 1
45. Microstructure and yield strength of SLM-fabricated CM247LC Ni-Superalloy10.1016/j.actamat.2017.02.007 ↗
46. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
47. Columnar to equiaxed transition in Al-Mg(-Sc)-Zr alloys produced by selective laser melting10.1016/j.scriptamat.2017.10.021 ↗
48. Characterization of SLM-fabricated Inconel 718 after solid solution and precipitation hardening heat treatments10.1007/s10853-018-2851-x ↗
49. Mitigation of anisotropic fatigue in nickel alloy 718 manufactured via selective laser melting10.1016/j.matdes.2019.108095 ↗
50. Improved plasticity of Inconel 718 superalloy fabricated by selective laser melting through a novel heat treatment process10.1016/j.matdes.2019.107915 ↗
51. Heat treatment of Inconel 718 produced by selective laser melting: microstructure and mechanical properties10.1016/j.msea.2019.02.046 ↗
52. Microstructure and properties of vacuum cast Sc-containing Be–Al alloys
53. Microstructure and metastable phase in rapidly solidified TiAl alloy prepared by vacuum suction casting10.1002/crat.201900054 ↗
54. Microstructure evolution and mechanical properties’ improvement of NiAl-Cr(Mo)-Hf eutectic alloy during suction casting and subsequent HIP treatment10.1016/j.intermet.2009.05.003 ↗
55. Microstructure and mechanical properties of Hf and Ho doped NiAl-Cr(Mo) near eutectic alloy prepared by suction casting10.1016/j.matchar.2009.06.005 ↗
56. Nickel-based superalloy microstructure obtained by pulsed laser powder bed fusion10.1016/j.matchar.2017.07.024 ↗
57. Grain growth behaviour during near-γ’ solvus thermal exposures in a polycrystalline nickel-base superalloy10.1016/j.actamat.2013.02.028 ↗
58. Formation mechanism of abnormally large grains in a polycrystalline nickel-based superalloy during heat treatment processing10.1016/j.actamat.2019.02.012 ↗
59. Cybermaterials: materials by design and accelerated insertion of materials10.1038/npjcompumats.2015.9 ↗
60. Effect of standard heat treatment on the microstructure and mechanical properties of selective laser melting manufactured Inconel 718 superalloy10.1016/j.msea.2015.06.021 ↗
61. Influences of hot-isostatic-pressing temperature on microstructure, tensile properties and tensile fracture mode of Inconel 718 powder compact10.1016/j.msea.2014.01.095 ↗
62. Strengthening mechanisms in Inconel 718 superalloy10.1179/030634583790421032 ↗
63. Shearing of γ" precipitates and formation of planar slip bands in Inconel 718 during cyclic deformation10.1016/j.scriptamat.2004.11.023 ↗
64. Surface integrity and structural stability of broached Inconel 718 at high temperatures10.1007/s11661-016-3515-6 ↗
65. Effects of processing routes on room temperature tensile strength and elongation for Inconel 71810.1016/j.matdes.2017.01.069 ↗
66. TEM study of high-temperature precipitation of delta phase in inconel 718 alloy10.1155/2011/940634 ↗
67. The quantitative effect of rapid cooling upon the constitution of binary alloys
68. Bemerkungen zur schichtkristallbildung
69. Differential thermal analysis (DTA) study of the homogenization process in alloy 71810.7449/1991/Superalloys_1991_147_160 ↗
70. An inherent strain based multiscale modeling framework for simulating part-scale residual deformation for direct metal laser sintering
71. Rationalization of microstructure heterogeneity in INCONEL 718 builds made by the direct laser additive manufacturing process10.1007/s11661-014-2370-6 ↗
72. On the theory of normal and abnormal grain growth10.1016/0001-6160(65)90200-2 ↗
73. The control of the grain size by particles
74. Ultra-large single crystals by abnormal grain growth10.1038/s41467-017-00383-0 ↗
75. Electron beam melting of Inconel 718: effects of processing and post-processing10.1080/02670836.2018.1424379 ↗
76. The role of annealing twins during recrystallization of Cu10.1016/j.actamat.2007.03.021 ↗
77. Effect of grain boundaries on texture formation during dynamic recrystallization of magnesium alloys10.1016/j.actamat.2017.01.063 ↗
78. Mean field modelling of dynamic and post-dynamic recrystallization during hot deformation of Inconel 718 in the absence of δ phase particles10.1016/j.msea.2015.12.102 ↗
79. A new grain orientation spread approach to analyze the dynamic recrystallization behavior of a cast-homogenized Mg-Zn-Zr alloy using electron backscattered diffraction10.1016/j.msea.2017.10.062 ↗
80. Twin recrystallization mechanisms in magnesium-rare earth alloys10.1016/j.actamat.2015.05.044 ↗
81. Evolution of recrystallization texture in a 0.78 wt.% Cr extra-low-carbon steel after warm and cold rolling10.1016/j.actamat.2011.04.027 ↗
82. Localized recrystallization during creep in nickel-based superalloys GTD444 and René N510.1016/j.actamat.2014.03.052 ↗
83. Nucleation and preferential growth mechanism of recrystallization texture in high purity binary magnesium-rare earth alloys10.1016/j.actamat.2017.07.038 ↗
84. Quantification of the recrystallized fraction in a nickel-base-alloy from EBSD-data10.1017/S1431927603026229 ↗
85. Understanding a microstructure using GOS (grain orientation spread) and its application to recrystallization study of hot deformed Al-Cu-Mg alloys10.4028/www.scientific.net/MSF.558-559.153 ↗
86. A study of the heterogeneity of plastic deformation in IF steel by EBSD10.1016/j.msea.2012.03.068 ↗
87. Growth of MC particles on stacking faults and dislocations10.1016/0026-0800(87)90063-2 ↗
88. Abnormal grain growth induced by cyclic heat treatment10.1126/science.1238017 ↗
89. Microstructure and fracture behavior of TiC particles reinforced Inconel 625 composites prepared by laser additive manufacturing10.1016/j.jallcom.2017.10.280 ↗
90. Dislocation sources
91. Deformation behavior of γ" strengthened Inconel 71810.1016/0001-6160(88)90139-3 ↗
92. Low cycle fatigue behavior of Inconel 718 at 298 K and 823 K10.1007/BF02667395 ↗
93. Direct observation of individual dislocation interaction processes with grain boundaries10.1126/sciadv.1501926 ↗
94. Mathematical simulation of grain boundary liquation in HAZ during welding-study on weldability of cast Alloy 718 rReport 5)
95. Diffusion of chromium in Inconel-60010.1016/0022-3115(77)90026-5 ↗
96. Grain boundary self-diffusion of 51Cr and 59Fe in austenitic NiFeCr alloys10.1016/0921-5093(91)90830-G ↗
97. Grain boundary diffusion