Synchrotron X-ray imaging of directed energy deposition additive manufacturing of titanium alloy Ti-6242
Source abstract
Abstract
Abstract Directed Energy Deposition Additive Manufacturing (DED-AM) is transformative for the production of larger, geometrically complex metallic components. However, the mechanical properties of titanium alloy DED-AM components do not always reach their full potential due to microstructural features including porosity and regions of lack of fusion. Using in situ and operando synchrotron X-ray imaging we gain insights into key laser-matter interaction and microstructural feature formation mechanisms during DED-AM of Ti-6242. Analysis of the process conditions reveals that laser power is dominant for build efficiency while higher traverse speed can effectively reduce lack of fusion regions. We also elucidate the mechanisms underlying several physical phenomena occurring during the deposition of titanium alloys, including the formation of a saddle-shaped melt pool and pore pushing. The findings of this work clarify the transient kinetics behind the DED-AM of titanium alloys and can be used as a guide for optimising industrial additive manufacturing processes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
2. Application of directed energy deposition-based additive manufacturing in repair10.3390/app9163316 ↗
3. The role of laser additive manufacturing methods of metals in repair, refurbishment and remanufacturing - enabling circular economy10.1016/j.phpro.2016.08.077 ↗
4. Design framework for multifunctional additive manufacturing: coupled optimization strategy for structures with embedded functional systems
5. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
6. Fatigue behavior of porous Ti-6Al-4V made by laser-engineered net shaping10.3390/ma11020284 ↗
7. Grain structure control of additively manufactured metallic materials10.3390/ma10111260 ↗
8. Microstructure modelling of laser metal powder directed energy deposition of alloy 718
9. Effect of processing conditions on the microstructure, porosity, and mechanical properties of Ti-6Al-4V repair fabricated by directed energy deposition10.1016/j.jmatprotec.2018.08.041 ↗
10. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
11. Fatigue behaviour of additively-manufactured metallic parts10.1016/j.prostr.2017.11.053 ↗
12. Effect of manufacturing parameters on the microstructure and mechanical properties of metal laser sintering parts of precipitate hardenable metals10.1007/s00170-018-2586-5 ↗
13. Material processing of hydroxyapatite and titanium alloy (HA/Ti) composite as implant materials using powder metallurgy: a review10.1016/j.matdes.2013.09.045 ↗
14. Hierarchical tailoring of strut architecture to control permeability of additive manufactured titanium implants10.1016/j.msec.2013.05.050 ↗
15. Additive manufactured porous titanium structures: Through-process quantification of pore and strut networks10.1016/j.jmatprotec.2014.05.006 ↗
16. Mechanical properties and microstructure of laser welded Ti–6Al–2Sn–4Zr–2Mo (Ti6242) titanium alloy10.1016/j.msea.2016.02.068 ↗
17. Real-time monitoring of laser powder bed fusion process using high-speed X-ray imaging and diffraction10.1038/s41598-017-03761-2 ↗
18. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
19. An instrument for in situ time-resolved X-ray imaging and diffraction of laser powder bed fusion additive manufacturing processes10.1063/1.5017236 ↗
20. Ultrafast dynamics of laser-metal interactions in additive manufacturing alloys captured by in situ X-ray imaging
21. Development of synchrotron X-ray micro-tomography under extreme conditions of pressure and temperature10.1107/S1600577516016623 ↗
22. In situ synchrotron investigation of grain growth behavior of nano-grained UO210.1016/j.scriptamat.2016.12.025 ↗
23. R. Cunningham, C. Zhao, N. Parab, C. Kantzos, Keyhole threshold and morphology in laser melting revealed by ultrahigh-speed x-ray imaging, 852, 2019, pp. 849–852.10.1126/science.aav4687 ↗
24. In-situ high-speed X-ray imaging of piezo-driven directed energy deposition additive manufacturing10.1038/s41598-018-36678-5 ↗
25. In situ rheological measurements at extreme pressure and temperature using synchrotron X-ray diffraction and radiography10.1107/S0909049509034426 ↗
26. I12: the joint engineering, environment and processing (JEEP) beamline at diamond light source10.1107/S1600577515003513 ↗
27. Melt pool morphology in directed energy deposition additive manufacturing process10.1088/1757-899X/861/1/012012 ↗
28. Capturing Marangoni flow via synchrotron imaging of selective laser melting10.1088/1757-899X/861/1/012010 ↗
29. Y. Chen, S.J. Clark, L. Sinclair, C.L.A. Leung, S. Marussi, T. Connolley, O. V. Magdysyuk, R.C. Atwood, G.J. Baxter, M.A. Jones, D.G. McCartney, I. Todd, P.D. Lee, In situ and Operando X-ray Imaging of Directed Energy Deposition Additive Manufacturing, ArXiv, 2020, 1–31. http://arxiv.org/abs/2006.09087.
30. In situ X-ray quantification of melt pool behaviour during directed energy deposition additive manufacturing of stainless steel10.1016/j.matlet.2020.129205 ↗
31. Fiji: an open-source platform for biological-image analysis10.1038/nmeth.2019 ↗
32. Effect of metal vaporization behavior on keyhole-mode surface morphology of selective laser melted composites using different protective atmospheres10.1016/j.apsusc.2015.07.044 ↗
33. Working distance passive stability in laser directed energy deposition additive manufacturing10.1016/j.matdes.2018.11.021 ↗
34. Laser direct metal deposition: theory and applications in manufacturing and maintenance10.1533/9781845699819.6.461 ↗
35. Phase-contrast imaging using polychromatic hard X-rays10.1038/384335a0 ↗
36. Partitioning of laser energy during directed energy deposition
37. Surface oxides and sintering of metals10.1179/pom.1981.24.4.177 ↗
38. Influence of a pulsed laser regime on surface finish induced by the direct metal deposition process on a Ti64 alloy10.1016/j.jmatprotec.2013.10.004 ↗
39. Influence of various process conditions on surface finishes induced by the direct metal deposition laser technique on a Ti-6Al-4V alloy10.1016/j.jmatprotec.2012.11.015 ↗
40. K.H. Richter, S. Orban, S. Nowotny, Laser cladding of the titanium alloy TI6242 to restore damaged blades, ICALEO 2004 - 23rd Int. Congr. Appl. Laser Electro-Optics, Congr. Proc., 2004. doi: 10.2351/1.5060222.10.2351/1.5060222 ↗
41. XCT analysis of the influence of melt strategies on defect population in Ti-6Al-4V components manufactured by selective electron beam melting10.1016/j.matchar.2015.02.008 ↗
42. J.E. Ramirez, B. Han, S. Liu, Effect of Welding Variables and Solidification Substructure on Weld Metal Porosity, 25, 1994, pp. 2285–2294.10.1007/BF02652328 ↗
43. In situ radiographic and ex situ tomographic analysis of pore interactions during multilayer builds in laser powder bed fusion
44. The influence of porosity on fatigue crack initiation in additively manufactured titanium components10.1038/s41598-017-06504-5 ↗
45. The effect of laser power and traverse speed on microstructure, porosity and build height in laser-deposited Ti-6Al-4V10.1016/S1359-6462(00)00408-5 ↗
46. Thermal process maps for controlling microstructure in laser-based solid freeform fabrication
47. Mechanistic models for additive manufacturing of metallic components10.1016/j.pmatsci.2020.100703 ↗
48. Interaction of porosity with a planar solid/liquid interface10.1007/s11661-004-0260-z ↗
49. Redistribution of particles during solidification10.2355/isijinternational.35.693 ↗
50. Fusion zone microstructure andporosity in electron beam welds of anα+βtitanium alloy10.1007/s11661-999-1011-y ↗
51. The role of hydrogen in titanium alloy weldments