Effect of hot isostatic pressing of laser powder bed fused Inconel 625 with purposely induced defects on the residual porosity and fatigue crack propagation behavior
Source abstract
Abstract
Abstract Inconel 625 specimens with different levels of purposely induced defects (up to ~3% of specimen volume) were manufactured by laser powder bed fusion. They were subjected to a stress relief annealing followed by hot isostatic pressing. After each step of post-processing, the residual porosity and the pore size distribution were measured using the computed tomography technique. Tensile and fatigue crack growth testing were then carried out to evaluate the impact of residual defects on the mechanical resistance and damage tolerance of the manufactured specimens. Hot isostatic pressing was effective in reducing the processing-induced defect count and size, but near-the-surface defects were still observed. Large clusters of residual defects were also observed for specimens manufactured with ~3% porosity. The elongation at break, and, to a lesser extent, the tensile strength were impacted by an as-manufactured porosity as small as 0.25%. Fatigue crack growth testing showed that HIP increases the threshold stress intensity factor for long fatigue crack propagation from ~7 to ~9 MPa*m1/2 and that irrespective of the level of as-manufactured porosity. An as-manufactured porosity smaller that 1% did not impact the fatigue crack growth rate of hot isostatic pressed specimens significantly, whereas occasional crack retardation was observed for specimens with an as-manufactured porosity of ~3%.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (89)
Show source-provided references
1. The status, challenges, and future of additive manufacturing in engineering10.1016/j.cad.2015.04.001 ↗
2. The impact of additive manufacturing in the aircraft spare parts supply chain: supply chain operation reference (scor) model based analysis10.1080/09537287.2013.808835 ↗
3. Jones, R., et al. Damage Tolerant Assessment of Additively Manufactured Replacement Parts. in Proceedings of the 13th International Conference on the Mechanical Behaviour of Materials (ICM13), Melbourne, Australia. 2019.
4. Saraçyakupoğlu · Qualif. Addit. Manuf. Parts Aviat. Ind. · 2019
5. Additively manufactured Ti-6Al-4V replacement parts for military aircraft10.1016/j.ijfatigue.2019.02.041 ↗
6. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
7. Additive manufacturing in the context of structural integrity10.1016/j.ijfatigue.2016.07.005 ↗
8. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
9. Overview of materials qualification needs for metal additive manufacturing10.1007/s11837-015-1810-0 ↗
10. Detecting void-induced scatter of fatigue life of selective laser melting-fabricated inconel 718 using miniature specimens10.1088/2053-1591/aafdcd ↗
11. The influence of porosity on fatigue crack initiation in additively manufactured titanium components10.1038/s41598-017-06504-5 ↗
12. Modeling and simulation of thermal field and solidification in laser powder bed fusion of nickel alloy IN62510.1016/j.optlastec.2018.08.016 ↗
13. Melt pool temperature and cooling rates in laser powder bed fusion
14. Comparative Assessment of Physics-Based Computational Models on the NIST Benchmark Study of Molten Pool Dimensions and Microstructure for Selective Laser Melting of Inconel 62510.1007/s40192-021-00201-y ↗
15. Energy input effect on morphology and microstructure of selective laser melting single track from metallic powder10.1016/j.jmatprotec.2012.11.014 ↗
16. A critical review of powder-based additive manufacturing of ferrous alloys: process parameters, microstructure and mechanical properties10.1016/j.matdes.2018.02.018 ↗
17. Influence of scan strategy and process parameters on microstructure and its optimization in additively manufactured nickel alloy 625 via laser powder bed fusion10.1007/s00170-016-9429-z ↗
18. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
19. Progress towards metal additive manufacturing standardization to support qualification and certification10.1007/s11837-017-2265-2 ↗
20. Defects in additive manufactured metals and their effect on fatigue performance: a state-of-the-art review10.1016/j.pmatsci.2020.100724 ↗
21. Influence of SLM process parameters on the surface finish, porosity rate and fatigue behavior of as-built Inconel 625 parts10.1016/j.jmatprotec.2017.12.043 ↗
22. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting10.1016/j.matdes.2016.05.070 ↗
23. Application of X-ray CT method for discontinuity and porosity detection in 316L stainless steel parts produced with SLM technology10.1016/j.acme.2014.02.003 ↗
24. Effect of laser-plume interaction on part quality in multi-scanner laser powder bed fusion
25. Spatter formation in selective laser melting process using multi-laser technology10.1016/j.matdes.2017.06.040 ↗
26. Productivity optimization of laser powder bed fusion by hot isostatic pressing
27. Hot isostatic pressing of IN718 components manufactured by selective laser melting
28. Lamikiz, A., Additive Manufacturing of the Superalloy Turbine Blades by Selective Laser Melting: Surface Quality, Microstructure and Porosity. New Technologies, Development and Application III: p. 267.
29. Long fatigue crack propagation behavior of Inconel 625 processed by laser powder bed fusion: Influence of build orientation and post-processing conditions10.1016/j.ijfatigue.2018.07.008 ↗
30. Build location effect on the single-track pore characteristics formed with the laser powder bed fusion process
31. Defect characteristics and analysis of their variability in metal L-PBF additive manufacturing10.1016/j.matdes.2019.108091 ↗
32. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
33. Additive manufactured AlSi10Mg samples using selective laser melting (SLM): microstructure, high cycle fatigue, and fracture behavior10.1016/j.matdes.2011.07.067 ↗
34. An analysis of defects influence on axial fatigue strength of maraging steel specimens produced by additive manufacturing10.1016/j.ijfatigue.2018.08.034 ↗
35. The influence of porosity on fatigue crack initiation in additively manufactured titanium components10.1038/s41598-017-06504-5 ↗
36. Competing crack initiation behaviors of a laser additively manufactured nickel-based superalloy in high and very high cycle fatigue regimes10.1016/j.ijfatigue.2020.105580 ↗
37. The effect of defects and notches in quasi-static and fatigue loading of Inconel 718 specimens produced by selective laser melting10.1016/j.ijfatigue.2020.105637 ↗
38. Fundamental aspects of hot isostatic pressing: an overview10.1007/s11661-000-0078-2 ↗
39. Producing metal parts with selective laser sintering/hot isostatic pressing.10.1007/s11837-998-0299-1 ↗
40. Hot isostatic pressing (HIP) technology and its applications to metals and ceramics10.1023/B:JMSC.0000044878.11441.90 ↗
41. Post‐processing of selective laser sintered metal parts10.1108/13552549510086853 ↗
42. Laser powder bed fabrication of nickel-base superalloys: influence of parameters; characterisation, quantification and mitigation of cracking
43. Fatigue strength estimation methodology of additively manufactured metallic bulk material
44. Effects of defects, surface roughness and HIP on fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.prostr.2017.11.055 ↗
45. Effects of defects on mechanical properties in metal additive manufacturing: a review focusing on X-ray tomography insights10.1016/j.matdes.2019.108385 ↗
46. Long fatigue crack propagation behavior of Inconel 625 processed by laser powder bed fusion: Influence of build orientation and post-processing conditions10.1016/j.ijfatigue.2018.07.008 ↗
47. Surface pick-up of argon during hot isostatic pressing of material built by laser powder bed fusion
48. Hot isostatic pressing in metal additive manufacturing: X-ray tomography reveals details of pore closure
49. Effect of heat treatments on pore morphology and microstructure of laser additive manufactured parts
50. Comparison of microstructure and mechanical properties of 316 L austenitic steel processed by selective laser melting with hot-isostatic pressed and cast material10.1016/j.msea.2016.10.012 ↗
51. The effects of hot isostatic pressing (HIP) and solubilization heat treatment on the density, mechanical properties, and microstructure of austenitic stainless steel parts produced by selective laser melting (SLM)10.1007/s00170-020-05072-9 ↗
52. Solubility of argon in laser additive manufactured α-titanium under hot isostatic pressing condition10.1016/j.commatsci.2017.01.040 ↗
53. Influence of trapped gas on pore healing under hot isostatic pressing in nickel-base superalloys10.3390/cryst10121147 ↗
54. Porosity regrowth during heat treatment of hot isostatically pressed additively manufactured titanium components10.1016/j.scriptamat.2016.05.002 ↗
55. Stress-defect-life interactions of fatigued additively manufactured alloy 71810.1016/j.ijfatigue.2020.106033 ↗
56. Overview on microstructure- and defect-sensitive fatigue modeling of additively manufactured materials.10.1007/s11837-018-2987-9 ↗
57. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes10.1016/j.ijfatigue.2016.06.020 ↗
58. Further studies into crack growth in additively manufactured materials10.3390/ma13102223 ↗
59. Fatigue life prediction of additively manufactured material: Effects of surface roughness, defect size, and shape10.1111/ffe.12799 ↗
60. Defence · MIL-STD-1530D Stand. Pract. -Aircr. Struct. Integr. Program (ASIP). · 2016
61. Jones, R., et al. Damage Tolerant Assessment of Additively Manufactured Replacement Parts.
62. Long fatigue crack propagation behavior of laser powder bed-fused inconel 625 with intentionally-seeded porosity10.1016/j.ijfatigue.2019.06.008 ↗
63. ASTM · 2014
64. Optimization of laser powder bed fusion processing using a combination of melt pool modeling and design of experiment approaches: density control
65. The average grain size and grain aspect ratio in metal laser powder bed fusion: Modeling and experiment
66. Standard Test Methods for Tension Testing of Metallic Materials. 2016, ASTM International.
67. Standard Test Method for Measurement of Fatigue Crack Growth Rates. 2015, ASTM International.
68. Chandler · 1996
69. Formation of the Ni 3 Nb δ-phase in stress-relieved Inconel 625 produced via laser powder-bed fusion additive manufacturing10.1007/s11661-017-4304-6 ↗
70. Carlson, R., CAST 625 HOT ISOSTATIC PRJMlNG HIP PARAMETERS-b4.
71. Comparison of microstructures and properties for a ni-base superalloy (Alloy 625) fabricated by electron beam melting
72. International · 2017
73. Effect of heat treatment and hot isostatic pressing on the microstructure and mechanical properties of Inconel 625 alloy processed by laser powder bed fusion10.1016/j.msea.2017.02.038 ↗
74. Effects of hot isostatic pressing on the elastic modulus and tensile properties of 316L parts made by powder bed laser fusion10.1016/j.msea.2017.03.100 ↗
75. Kluczynski · Eff. Process Parameter Modif. Hot Isostatic Press. Mech. Prop. Sel. Laser-Melted 316L Steel · 2020
76. Characterization of inconel 625 fabricated using powder-bed-based additive manufacturing technologies10.1016/j.jmatprotec.2018.08.031 ↗
77. Hyer, H., et al., Microstructural Development in As Built and Heat Treated IN625 Component Additively Manufactured by Laser Powder Bed Fusion. Journal of Phase Equilibria and Diffusion: p. 1–14.10.1007/s11669-020-00855-9 ↗
78. Effects of grain size and precipitate size on the fatigue crack growth behavior of alloy 718 at 427C10.1007/BF02646657 ↗
79. Laser powder bed fusion with intentionally-seeded porosity for prototyping of powder metallurgy parts
80. Influence of heat treatments on microstructure evolution and mechanical properties of Inconel 625 processed by laser powder bed fusion10.1016/j.msea.2018.05.044 ↗
81. Grain size effects in a Ni-based turbine disc alloy in the time and cycle dependent crack growth regimes10.1016/j.ijfatigue.2013.07.014 ↗
82. Plasticity and fracture behavior of Inconel 625 manufactured by laser powder bed fusion: comparison between as-built and stress relieved conditions10.1016/j.msea.2021.140808 ↗
83. The role of texturing and microstructure evolution on the tensile behavior of heat-treated Inconel 625 produced via laser powder bed fusion10.1016/j.msea.2019.138500 ↗
84. Role of misorientation in fatigue crack growth behavior for NG-TIG welded joint of Ni-based alloy10.1016/j.msea.2017.10.090 ↗
85. About the fatigue crack propagation threshold of metals as a design criterion – A review10.1016/j.engfracmech.2015.12.002 ↗
86. Damage tolerant design of additively manufactured metallic components subjected to cyclic loading: state of the art and challenges10.1016/j.pmatsci.2021.100786 ↗
87. Defect-dominated fatigue behavior in type 630 stainless steel fabricated by selective laser melting10.1016/j.msea.2016.04.042 ↗
88. Small fatigue crack growth behavior of Ti-6Al-4V produced via selective laser melting: in situ characterization of a 3D crack tip interactions with defects10.1016/j.ijfatigue.2020.105638 ↗
89. Stress intensity factor equations for branched crack growth10.1016/j.engfracmech.2005.05.004 ↗