Targeted rework strategies for powder bed additive manufacture
Source abstract
Abstract
A major factor limiting the adoption of powder-bed-fusion additive manufacturing for production of parts is the control of build process defects and the effect these have upon the certification of parts for structural applications. In response to this, new methods for detecting defects and to monitor process performance are being developed. However, effective utilisation of such methods to rework parts in process has yet to be demonstrated.This study investigates the use of spatially resolved acoustic spectroscopy (SRAS) scan data to inform repair strategies within a commercial selective laser melting machine. New methodologies which allow for rework of the most common defects observed in selective laser melting (SLM) manufacturing are proposed and demonstrated. Three rework methodologies are applied to targeted surface breaking pores: a hatch pattern, a spiral pattern and a single shot exposure. The work presented shows that it is possible to correct surface breaking pores using targeted re-melting, reducing the depth of defects whilst minimising changes in local texture. For the hatch rework and spiral rework, a reduction in defect depth of 50% and 31% were observed, respectively, however, no improvement was seen after the single shot exposures. This work is part of a programme to develop a method by which defects can be detected and the part reworked in-process during SLM to enable defect specification targets to be met. Although further work in developing build-characterise-rework strategies for integrated and targeted defect correction is needed, the feasibility of the underlying method of identifying and selectively reworking to reduce a defect has now been demonstrated for the first time.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Making sense of 3-D printing: creating a map of additive manufacturing products and services
2. The manufacturing of hard tools from metallic powders by selective laser melting10.1016/S0924-0136(01)00522-2 ↗
3. Study of the wear behaviour of conventional and rapid tooling mould materials
4. Additive manufacturing of tissues and organs10.1016/j.progpolymsci.2011.11.007 ↗
5. Wohlers report 2016: additive manufacturing and 3D printing state of the industry
6. Electron beam additive manufacturing of titanium components: properties and performance10.1115/1.4025773 ↗
7. Promising characteristics of gradient porosity Ti-6Al-4 V alloy prepared by SLM process10.1016/j.jmbbm.2017.01.043 ↗
8. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
9. Review of in-situ process monitoring and in-situ metrology for metal additive manufacturing10.1016/j.matdes.2016.01.099 ↗
10. XCT analysis of the influence of melt strategies on defect population in Ti–6Al–4V components manufactured by Selective Electron Beam Melting10.1016/j.matchar.2015.02.008 ↗
11. Reducing lack of fusion during selective laser melting of CoCrMo alloy: effect of laser power on geometrical features of tracks10.1016/j.matdes.2016.09.086 ↗
12. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
13. Direct selective laser sintering of iron-graphite powder mixture10.1016/S0924-0136(03)00150-X ↗
14. Denudation of metal powder layers in laser powder bed fusion processes10.1016/j.actamat.2016.05.017 ↗
15. Assessing the capability of in-situ nondestructive analysis during layer based additive manufacture
16. Van Elsen · 2007
17. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones10.1016/j.actamat.2016.02.014 ↗
18. The effectiveness of hot isostatic pressing for closing porosity in titanium parts manufactured by selective electron beam melting10.1007/s11661-016-3429-3 ↗
19. Microstructural architecture, microstructures, and mechanical properties for a nickel-base superalloy fabricated by electron beam melting10.1007/s11661-011-0748-2 ↗
20. Possibility of introducing laser surfacing into maintenance service of die-casting dies10.1016/j.surfcoat.2003.10.101 ↗
21. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
22. The investigation of the influence of laser re-melting on density, surface quality and microstructure of selective laser melting parts10.1108/13552541111156450 ↗
23. Investigation of the effect of process parameters on the formation and characteristics of recast layer in wire-EDM of Inconel 71810.1016/j.msea.2009.01.061 ↗
24. Analysis and correction of defects within parts fabricated using powder bed fusion technology10.1088/2051-672X/3/3/034002 ↗
25. Meso-scale defect evaluation of selective laser melting using spatially resolved acoustic spectroscopy10.1098/rspa.2017.0194 ↗
26. Spatially resolved acoustic spectroscopy for selective laser melting10.1016/j.jmatprotec.2016.05.005 ↗
27. The SKED: speckle knife edge detector
28. Spatially resolved acoustic spectroscopy for rapid imaging of material microstructure and grain orientation10.1088/0957-0233/25/5/055902 ↗
29. Orientation characterisation of aerospace materials by spatially resolved acoustic spectroscopy
30. The machinability of Inconel 71810.1016/S0924-0136(96)02624-6 ↗
31. On the effect of scanning strategies in the selective laser melting process10.1080/17452751003688368 ↗
32. On the role of thermal fluid dynamics into the evolution of porosity during selective laser melting10.1016/j.scriptamat.2015.04.016 ↗
33. Montgomery · 2009
34. Organ printing: computer-aided jet-based 3D tissue engineering10.1016/S0167-7799(03)00033-7 ↗
35. Thin-film optoacoustic transducers for subcellular Brillouin oscillation imaging of individual biological cells10.1364/AO.54.008388 ↗
36. Giffi · 2014 · 1
37. Evaluation of selective laser sintering processes by optical coherence tomography10.1016/j.matdes.2015.09.084 ↗