Abstract
The irradiation with the 10 ns pulsed infrared Nd:YAG laser was applied to transform FePdCu multilayers into chemically ordered L10 phase. The X-ray diffraction methods (Theta/2Theta scan, psi-scan, omega-scan) were used to trace the presence of L10 phase after laser annealing with different number of pulses. The size and shape of crystallites was determined depending on their orientation with respect to film plane. The (111) oriented crystallites of constituent metals were built as coherent domains spreading through multilayers during deposition of films. Laser annealing induced the transformation of multilayers to alloy, and the ordering of (111) oriented crystallites. Simultaneously, the (002) oriented crystallites appeared confirming the transformation to L10 alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical and Alloy Processes · Advanced Materials Characterization Techniques · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Determining the low-coercivity temperature coefficient in FePt (fct)/FePt (fcc) nanocomposite films10.1088/1742-6596/200/7/072106 ↗
2. Laser-induced inter-diffusion in AuAg core–shell nanoparticles10.1021/jp002438r ↗
3. Klotzbach · 2011 · 10
4. Direct laser interference patterning: theory and application10.12693/APhysPolA.115.591 ↗
5. Pulsed laser deposition of multicomponent metal and oxide films10.1016/S0169-4332(98)00416-4 ↗
6. Industrial applications of high power diode lasers in materials processing10.1016/S0169-4332(02)01349-1 ↗
7. Fe–Pd thin films as a model system for self-organized exchange coupled nanomagnets10.1063/1.3457219 ↗
8. Microstructural, magnetic anisotropy, and magnetic domain structure correlations in epitaxial FePd thin films with perpendicular magnetic anisotropy10.1109/TMAG.2009.2039923 ↗
9. AFM, XRD and HRTEM studies of annealed FePd thin films10.12693/APhysPolA.117.423 ↗
10. Crystallographic aspects of L10 magnetic materials10.1016/j.scriptamat.2005.04.039 ↗
11. X-ray absorption fine structure and X-ray diffraction studies of crystallographic grains in nanocrystalline FePd:Cu thin films10.1063/1.3553856 ↗
12. Chemical order and crystallographic texture of FePd:Cu thin alloy films10.1063/1.3699061 ↗
13. Surface studies of solids by total reflection of X-rays10.1103/PhysRev.95.359 ↗
14. Laser annealing for solid-phase thin-film reactions10.1063/1.90737 ↗
15. Time–temperature–transformation measurements of FePt thin films in the millisecond regime using pulse laser processing10.1063/1.3506689 ↗
16. Birkholtz · 2006
17. Structure of PtFe/Fe double-period multilayers investigated by X-ray diffraction, reflectivity, diffuse scattering and TEM10.1016/j.apsusc.2006.05.105 ↗
18. Pearson · 1967
19. The state of the art of the diffraction analysis of crystallite size and lattice strain10.1524/zkri.2008.1213 ↗
20. X-ray diffraction and extended X-ray absorption fine-structure characterization of nonspherical crystallographic grains in iron thin films10.1063/1.1810636 ↗