Hydrofluoric–nitric–sulphuric-acid surface treatment of tungsten for carbon fibre-reinforced composite hybrids in space applications
Source abstract
Abstract
Abstract Hybrid material systems, such as combinations of tungsten foils and carbon fibre-reinforced plastic (CFRP), are replacing metal alloy concepts in spacecraft enclosures. However, a good adhesion between the tungsten oxide scale and the epoxy resin used is required. Here, the effects of a hydrofluoric–nitric–sulphuric-acid (HFNS) treatment on tungsten oxides and subsequent adhesion to CFRP are analysed using atomic force microscopy (AFM), X-ray photoelectron spectroscopy (XPS) and fracture testing. The work shows that HFNS treatment results in decreased oxygen content, over 50% thinner tungsten trioxide (WO 3 ) layer and increased nano-roughness on thin tungsten foils. Fracture testing established a 39% increase in the average critical strain for tungsten–CFRP specimens after HFNS treatment was carried out on tungsten. The effect of the oxide scale modification regarding the critical strain energy release rate was Δ G c ≈ 8.4 J/m 2 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicone and Siloxane Chemistry · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Effects of material and/or structure on shielding of electronic devices10.1109/23.556851 ↗
2. Effect of intercalation in graphite epoxy composites on the shielding of high energy radiation10.1557/JMR.1998.0320 ↗
3. CFRP electronics housing for a satellite
4. Radiation shielding of composite space enclosures
5. Koerselman · 2012
6. The structure of oxide layers on tungsten10.1149/1.2425800 ↗
7. Quasi-aligned single-crystalline W18O49 nanotubes and nanowires10.1002/adma.200305122 ↗
8. XPS studies on surface reduction of tungsten oxide nanowire film by Ar+ bombardment10.1016/j.elspec.2012.01.004 ↗
9. High temperature oxidation protection of tungsten
10. Kinetics of the oxidation of pure tungsten from 500°C to 1300°C10.1149/1.2427787 ↗
11. On the oxidation mechanism of pure tungsten in the temperature range 600–800°C10.1016/j.corsci.2011.12.027 ↗
12. Oxidation of tungsten and tungsten carbide in dry and humid atmospheres10.1016/S0263-4368(96)00027-3 ↗
13. The influence of chemical treatments on tungsten films found in integrated circuits10.1016/S0169-4332(01)00308-7 ↗
14. Adherend surface morphology and its influence on the peel strength of adhesive joints bonded with modified phenolic and epoxy structural adhesives10.1016/0143-7496(94)90017-5 ↗
15. Internal stresses, Young's modulus and practical adhesion of organic coatings applied onto 5754 aluminum alloy10.1016/S0040-6090(99)00449-6 ↗
16. Formation and structure of epoxy network interphases at the contact to native metal surfaces10.1016/j.crci.2005.04.009 ↗
17. Role of the interphase in the environmental failure of adhesive joints10.1016/S1359-6454(00)00240-8 ↗
18. Organo-metallic complex characterization formed when liquid epoxy-diamine mixtures are applied onto metallic substrates10.1016/S0032-3861(01)00034-9 ↗
19. Guttmann · 1961 · 22
20. Anodic oxidation of tungsten in sulphuric acid solution-influence of hydrofluoric acid addition10.1016/j.matchemphys.2008.06.029 ↗
21. Structural assessment of tungsten–epoxy bonding in spacecraft composite enclosures with enhanced radiation protection
22. The effect of PVD layer constitution on surface free energy10.1016/S0040-6090(99)00543-X ↗
23. Adhesion phenomena in bonded joints10.1016/j.ijadhadh.2012.04.007 ↗
24. Reproducible XPS on biopolymers: cellulose studies10.1002/sia.1827 ↗
25. Quantitative surface measurements of metal oxide powders by X-ray photoelectron spectroscopy (XPS)10.1016/0039-6028(78)90330-8 ↗
26. 1990
27. Elastic scattering corrections in (AES) and (XPS), II. estimating attenuation lengths and conditions required for their valid use in overlayer/substrate experiments10.1002/(SICI)1096-9918(199706)25:6<430::AID-SIA254>3.0.CO;2-7 ↗
28. Fracture toughness testing of polymer matrix composites
29. Influence of surface treatments on the durability of stainless steel sheets bonded with epoxy10.1163/156856192X00304 ↗
30. Elemental depth profile analysis of hard coatings of tungsten carbide by auger electron (AES-) microprobe/sputtering10.1007/BF00473349 ↗
31. The multi-surface structure and catalytic properties of partially reduced WO3, WO2 and WC+O2 or W+O2 as characterized by XPS10.1016/0368-2048(95)02451-4 ↗
32. Influence of oxygen on the carbide formation on tungsten10.1016/S0022-3115(00)00429-3 ↗
33. Adhesively-bonded joints and repairs in metallic alloys, polymers and composite materials: adhesives, adhesion theories and surface pretreatment10.1023/B:JMSC.0000007726.58758.e4 ↗
34. Crack propagation under mode II dominance at stainless steel-epoxy interfaces with residual stresses and micro-scale roughness10.1016/j.ijsolstr.2013.06.008 ↗
35. The nature of the surface acidity of anodised titanium: an XPS study using 1,2-diaminoethane10.1016/0169-4332(96)00601-0 ↗
36. Cross-sectional nanoindentation for copper adhesion characterization in blanket and patterned interconnect structures: experiments and three-dimensional FEM modeling10.1007/s10704-007-9072-7 ↗
37. X-ray diffraction and fracture based analysis of residual stresses in stainless steel-epoxy interfaces with electropolishing and acid etching substrate treatments10.1016/j.ijadhadh.2012.07.005 ↗
38. Interface crack between two elastic layers10.1007/BF00018123 ↗
39. The effect of geometry on the fracture of adhesive joints10.1016/0143-7496(94)90015-9 ↗
40. The cracked lap shear specimen revisited – a closed form solution10.1016/0020-7683(95)00124-7 ↗
41. Callister · 2003
42. Powell · 2011