Abstract
Abstract The effects on the surface and mechanical properties of stainless steel AISI316L dogbones created using either traditional manufacturing (TM) or laser powder bed fusion (LPBF) exposed to 0.75 M sulfuric acid solution over 2184 h were studied. General corrosion was not a major form of corrosion, based on surface feature changes, surface roughness, and mass loss for either method. No change to the mechanical properties occurred for the TM samples. Both tensile stress and strain decreased for the LPBF samples. The decrease was caused by hydrogen embrittlement, due to the formation of large brittle particles, as demonstrated by scanning electron microscopy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Callister · 2014
2. Corrosion behavior and passive film chemistry of 216L stainless steel in sulphuric acid10.1007/s10853-008-2976-4 ↗
3. Askeland · 2016
4. McCafferty · 2010
5. Alves · 2006
6. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
7. Densification behavior of gas and water atomized 316L stainless steel powder during selective laser melting10.1016/j.apsusc.2010.02.030 ↗
8. Part and material properties in selective laser melting of metals
9. Heat transfer and fluid flow during keyhole mode laser welding of tantalum, Ti-6Al-4V, 304L stainless steel and vanadium10.1088/0022-3727/40/18/037 ↗
10. Direct laser sintering of metal powders: mechanism, kinetics and microstructural features10.1016/j.msea.2006.04.117 ↗
11. Single track formation in selective laser melting of metal powders10.1016/j.jmatprotec.2010.05.010 ↗
12. Density of additively-manufactured, 316L SS parts using laser powder-bed fusion at powers up to 400 W10.1007/s00170-014-5954-9 ↗
13. Composite Micropowders for Selective Laser Sintering10.1007/s11015-016-0183-0 ↗
14. The study of the laser parameters and environment variables effect on mechanical properties of high compact parts elaborated by selective laser melting 316L powder10.1016/j.msea.2013.06.055 ↗
15. Investigation into the effect of process parameters on microstructural and physical properties of 316L stainless steel parts by selective laser melting10.1007/s00170-014-6297-2 ↗
16. Residual stresses in selective laser sintering and selective laser melting
17. On the stress corrosion crack growth behaviour in high temperature water of 316L stainless steel made by laser powder bed fusion additive manufacturing10.1016/j.corsci.2017.09.017 ↗
18. Microstructure and corrosion resistance of laser additively manufactured 316L stainless steel10.1007/s11837-016-1822-4 ↗
19. Evaluation of corrosion resistance of Al-10Si-Mg alloy obtained by means of Direct Metal Laser Sintering10.1016/j.jmatprotec.2015.12.033 ↗
20. The microstructure, mechanical properties, and corrosion resistance of 316 L stainless steel fabricated using laser engineered net shaping10.1016/j.msea.2016.09.028 ↗
21. Sliding wear characteristics and corrosion behaviour of selective laser melted 316L stainless steel10.1007/s11665-013-0784-8 ↗
22. On the corrosion and metastable pitting characteristics of 316L stainless steel produced by selective laser melting10.1149/2.0551706jes ↗
23. Turton · 1998
24. Erosion-corrosion resistance of various stainless steel grades in high-temperature sulfuric acid solutions10.1016/j.wear.2016.06.007 ↗
25. Succession of sulfur-oxidizing Bacteria in the microbial community on corroding concrete in sewer systems10.1128/AEM.02054-06 ↗
26. Laser polishing of additive manufactured Ti alloys10.1016/j.optlaseng.2017.02.005 ↗
27. Microbial corrosion of silicon nitride ceramics by sulphuric acid producing bacteria Acidithiobacillus ferrooxidans10.1016/j.jeurceramsoc.2010.12.001 ↗
28. potentiodynamic polarization behavior and pitting corrosion analysis of 2101 duplex and 301 austenitic stainless steel in sulfuric acid concentrations10.1007/s11668-017-0291-6 ↗
29. Anodic behaviour of stainless steel S43000 in concentrated solutions of sulphuric acid10.1016/S0010-938X(02)00232-9 ↗
30. An AFM and XPS study of corrosion caused by micro-liquid of dilute sulfuric acid on stainless steel10.1016/j.apsusc.2003.12.019 ↗
31. Corrosion behavior of shape memory stainless steel in acid media10.1016/j.jallcom.2011.02.051 ↗
32. Corrosion behavior and passive film chemistry of 216L stainless steel in sulphuric acid10.1007/s10853-008-2976-4 ↗
33. Influence of laser peening on the hydrogen embrittlement resistance of 316L stainless steel10.1016/j.surfcoat.2017.08.037 ↗
34. Effect of hydrogen on dynamic precipitation of carbide in type 304 stainless steel during creep process10.1016/S1359-6454(96)00400-4 ↗
35. ASTM E8-16a · 2016
36. ASTM A240-15b · 2015
37. TA Chen International, Inc · 2014
38. Kneen · 2016
39. ASTM G129-00 · 2000
40. ASTM F519-13 · 2000
41. A kinetic trapping model for hydrogen-induced cracking10.1016/0001-6160(79)90059-2 ↗
42. Effects of hydrogen on the properties of Iron and steel10.1007/BF02654700 ↗