Abstract The formation of a protective oxide ensures the good corrosion resistance of austenitic steels in high temperature steam. However after long-term interaction even the protective oxide may tend to exfoliate and cause operational problems. With shot peening believed to be an effective method for mitigating steamside oxidation and exfoliation, we compared oxide layers formed on two materials: AISI 316H with a rugged untreated surface and Super304H with a shot-peened surface. In addition to conventional methods (SEM/EDS, Raman spectroscopy), Mott-Schottky analysis was used to characterize the oxide layers in order to determine the quality of the protective oxide. The oxides formed on Super 304H showed unexpected semiconducting behaviour with a significantly lower charge carrier density, thereby supporting the benefits of shot peening. Our findings extend the knowledge applicable to the design of more efficient coal-fired power plants.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. Effect of Temperature, Alloy Composition and Surface Treatment on the Steamside Oxidation/Oxide Exfoliation Behavior of Candidate A-USC Boiler Materials
2. Chapter 5.3. steam oxidation
3. Diffusion of cations in chromia layers grown in iron-base alloys10.1007/BF00665632 ↗
4. R. Point defects and cation tracer diffusion in (CrxFe1-x)3-dO4 spinels10.1016/0167-2738(95)00190-H ↗
5. Morphologies of oxide growth and exfoliation in superheater and reheater tubing of steam boilers10.3184/096034011X12982937656387 ↗
6. Austenitic steels for boiler elements in USC power plants
7. Boiler materials for USC coal power plants ?steamside oxidation10.1361/105994906X108756 ↗
8. Oxide scale growth and presumed exfoliation in a 700°C or higher steam condition: A simulation study for future operations of USC power plants10.1016/j.supflu.2014.06.002 ↗
9. Landolt · 2007
10. In situ electrochemical impedance and noise measurements of corroding stainless steel in high temperature water10.1016/j.electacta.2005.10.013 ↗
11. Illumination effects on the stability of the passive film on iron10.1016/0013-4686(94)00341-W ↗
12. Semiconducting properties of thermally grown oxide films on AISI 304 stainless steel10.1016/S0010-938X(99)00082-7 ↗
13. Hosterman · 2011
14. Semiconductor properties and protective rol of passive film of iron base alloys10.1016/j.corsci.2006.05.020 ↗
15. Impedance investigation of thermally formed oxide films on AISI 304L stainless steel10.1016/j.corsci.2009.11.004 ↗
16. High temperature corrosion ?oxidation of pure metals