Abstract
In the present work surface roughness of copper samples after mechanical surface preparation processes (polishing, grinding, sand-blasting) and after exposure in non-oxidizing (high purity argon) and oxidizing (air) conditions at 700 and 750°C have been evaluated by contact profilometer and by fractal analysis. Quantitative description of surfaces that are hidden from the sight of conventional methods is possible by fractal analysis, e.g. in the present work, the roughness of Cu2O/Cu boundary has been evaluated under oxide layer. It has been pointed out, that in both oxidizing and non-oxidizing conditions initial surface roughness of copper is affected by annealing at high temperature: at 700°C surface roughness of polished and ground samples increased but at 750°C decreased in comparison to surface roughness prior to heat treatment. For sand-blasted samples in both oxidizing and non-oxidizing conditions the lowest values of surface roughness parameters were obtained at 750°C. It is then concluded that two phenomena are responsible for such effect: chemical reaction between copper and oxygen and surface diffusion of copper due to high temperature of annealing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Adhesion, Friction, and Surface Interactions · High-Temperature Coating Behaviors · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. High-performance interconnects: an integration overview10.1109/5.929646 ↗
2. New model for low-temperature oxidation of copper single crystal10.1016/j.apsusc.2013.03.096 ↗
3. Study of the air-formed oxide layer at the copper surface and its impact on the copper corrosion in an aggressive chloride medium10.1016/j.electacta.2017.12.187 ↗
4. Electrochemically deposited p–n homojunction cuprous oxide solar cells10.1016/j.solmat.2008.09.023 ↗
5. Atomistic details of oxide surfaces and surface oxidation: the example of copper and its oxides10.1016/j.surfrep.2015.07.001 ↗
6. Oxidation of polycrystalline copper films – pressure and temperature dependence10.1016/j.tsf.2018.02.007 ↗
7. Kofstad · 1988
8. Young · 2016
9. Modeling defect transport during Cu oxidation10.1016/j.corsci.2015.05.067 ↗
10. Mrowec · 1964
11. Oxidation mechanism of Cu2O and defect structure of CuO at high temperatures10.1515/htmp.2011.046 ↗
12. Oxidation of copper at high temperatures10.1007/BF00603530 ↗
13. Oxidation mechanism of copper at 623-1073 K10.2320/matertrans.43.2173 ↗
14. Mimura · 2006
15. The effect of surface enriched chromium and grain refinement by ball milling on corrosion resistance of 316L stainless steel10.1016/j.materresbull.2017.03.022 ↗
16. Influence of surface roughness on the oxidation behavior of a Ni-4.0Cr-5.7Al single crystal superalloy10.1016/j.apsusc.2018.01.226 ↗
17. Enhancing the oxidation resistance of copper by using sandblasted copper surfaces10.1016/j.apsusc.2015.09.203 ↗
18. The effect of surface preparation on high temperature oxidation of Ni, Cu and Ni-Cu alloy10.1016/j.apsusc.2019.01.122 ↗
19. Evolution of surface waviness in thin films via volume and surface diffusion
20. Surface recrystallization and its effect on oxidation of superalloy C26310.1016/j.corsci.2017.09.020 ↗
21. Laser surface texturing to enhance adhesion bond strength of spray coatings – cold spraying, wire-arc spraying, and atmospheric plasma spraying10.1016/j.surfcoat.2017.05.007 ↗
22. TBC bond coat–top coat interface roughness: influence on fatigue life and modelling aspects10.1016/j.surfcoat.2013.09.051 ↗
23. A diffusion-based oxide layer growth model using real interface roughness in thermal barrier coatings for lifetime assessment10.1016/j.surfcoat.2014.12.043 ↗
24. Roughness and oxidation: application to NiO growth on Ni at 800°C10.1016/S0921-5093(00)00944-8 ↗
25. Atomistic investigation of the effects of temperature and surface roughness on diffusion bonding between Cu and Al10.1016/j.actamat.2006.12.040 ↗
26. Stages in the tribologically-induced oxidation of high-purity copper10.1016/j.scriptamat.2018.05.008 ↗
27. Comparison of fractal and profilometric methods for surface topography characterization10.1016/j.apsusc.2007.11.040 ↗
28. Quantitative interface roughness studies of copper oxide on copper10.1016/0040-6090(88)90101-0 ↗
29. Fractal geometry for industrial data evaluation10.1016/j.camwa.2013.01.015 ↗
30. Fractal dimension used for evaluation of oxidation behaviour of Fe-Al-Cr-Zr-C alloys10.1016/j.corsci.2018.01.017 ↗
31. Roughness parameters10.1016/S0924-0136(02)00060-2 ↗
32. Fractal roughness effects on nanoscale grinding10.1016/j.apsusc.2018.10.144 ↗
33. Scale-sensitive fractal analysis of turned surfaces10.1016/S0007-8506(07)63114-X ↗
34. Pit formation and growth of alloy 600 in Cl− ion-containing thiosulphate solution at temperatures 298–573 K using fractal geometry10.1016/S0010-938X(02)00212-3 ↗
35. Effect of processing parameters on MCrAlY bondcoat roughness and lifetime of APS–TBC systems10.1016/j.surfcoat.2014.06.075 ↗
36. Sfrax 1.0
37. Effect of surface roughness on corrosion behavior of the superalloy IN718 in simulated marine environment10.1016/j.jallcom.2018.01.042 ↗
38. Influence of surface roughness on the corrosion behavior of alloy 690TT in PWR primary water10.1016/j.nucengdes.2014.08.023 ↗
39. The homogeneous nucleation mechanism of Cu 2O on Cu(001)10.1016/S1359-6462(98)00026-8 ↗
40. In situ ultra-high vacuum transmission electron microscopy studies of the transient oxidation stage of Cu and Cu alloy thin films10.1016/j.micron.2012.02.007 ↗
41. In situ UHV-TEM investigation of the kinetics of initial stages of oxidation on the roughened Cu(110) surface10.1016/j.susc.2004.04.046 ↗