journal article·2006-11

ZnO thin films on Si(1 1 1) grown by pulsed laser deposition from metallic Zn target

Jie Zhao, Lizhong Hu, Zhaoyang Wang, Jie Sun, Zhijun Wang

Applied Surface Science· Volume 253· Issue 2
Publisher page

Abstract

ZnO thin films with highly c-axis orientation have been fabricated on p-type Si(1 1 1) substrates at 400 degrees C by pulsed laser deposition (PLD) from a metallic Zn target with oxygen pressures between 0.1 and 0.7 mbar. Experimental results indicate that the films deposited at 0.3 and 0.5 mbar have better crystalline and optical quality and flatter surfaces than the films prepared at other pressures. The full width at half maximum (FWHM) of (0 0 0 2) diffraction peak decreases remarkably from 0.46 to 0.19 degrees with increasing annealing temperature for the film prepared at 0.3 mbar. In photoluminescence (PL) spectra at room temperature, the annealed film at 700 degrees C exhibits a smaller ultraviolet (UV) peak FWHM of 108 meV than the as-grown film (119 meV). However, an enhanced deep-level emission is observed. Possible origins to above results are discussed. (c) 2006 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Ga2O3 and related materials · Copper-based nanomaterials and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Reynolds · Solid State Commun. · 1996 · 99 · 87310.1016/0038-1098(96)00340-7 ↗
2. Bagnall · Appl. Phys. Lett. · 1997 · 70 · 223010.1063/1.118824 ↗
3. Tang · Appl. Phys. Lett. · 1998 · 72 · 327010.1063/1.121620 ↗
4. Ohtomo · Appl. Phys. Lett. · 1999 · 75 · 263510.1063/1.125102 ↗
5. Yang · Thin Solid Films · 1998 · 326 · 6010.1016/S0040-6090(98)00763-9 ↗
6. Ryu · Appl. Surf. Sci. · 1998 · 127–129 · 49610.1016/S0169-4332(97)00681-8 ↗
7. Bethke · Appl. Phys. Lett. · 1988 · 52 · 13810.1063/1.99030 ↗
8. Chen · J. Appl. Phys. · 1998 · 84 · 391210.1063/1.368595 ↗
9. Ghosh · J. Appl. Phys. · 2004 · 96 · 268910.1063/1.1769598 ↗
10. Hu · Mater. Lett. · 1995 · 25 · 510.1016/0167-577X(95)00144-1 ↗
11. Kim · Thin Solid Films · 2004 · 446 · 30710.1016/j.tsf.2003.09.057 ↗
12. Kang · J. Appl. Phys. · 2004 · 95 · 124610.1063/1.1633343 ↗
13. Guo · J. Cryst. Growth · 2001 · 223 · 13510.1016/S0022-0248(00)00952-0 ↗
14. Fouchet · J. Appl. Phys. · 2004 · 96 · 322810.1063/1.1772891 ↗
15. Fujimura · J. Cryst. Growth · 1993 · 130 · 26910.1016/0022-0248(93)90861-P ↗
16. Im · J. Appl. Phys. · 2000 · 87 · 455810.1063/1.373102 ↗
17. Sun · Appl. Phys. Lett. · 2000 · 77 · 232210.1063/1.1316069 ↗
18. Vanheusden · J. Appl. Phys. · 1996 · 79 · 798310.1063/1.362349 ↗
19. Cullity · 1978