journal article·2011-10

(Ti,Al,Si,C)N nanocomposite coatings synthesized by plasma-enhanced magnetron sputtering

Yanfeng Wang, Li Zhengxian, Du Jihong, Hua Yunfeng, Wang Baoyun

Applied Surface Science· Volume 258· Issue 1
Publisher page

Abstract

Materials’ surface service property could be enhanced by transition metal nitride hard coatings due to their high hardness, wear and high temperature oxidation resistance, but the higher friction coefficient (0.4–0.9) of which aroused terrible abrasion. In this work, quinternary (Ti,Al,Si,C)N hard coating 3–4 μm was synthesized at 300 °C using plasma enhanced magnetron sputtering system. It was found that the coating`s columnar crystals structure was restrained obviously with the increase of C content and a non-columnar crystals growth mode was indicated at the C content of 33.5 at.%. Both the XRD and TEM showed that the (Ti,Al,Si,C)N hard coatings had unique nanocomposite structures composed of nanocrystalline and amorphous nc-(Ti,Al)(C,N)/nc-AlN/a-Si3N4/a-Si/a-C. However, the coatings were still super hard with the highest hardness of 41 GPa in spite of the carbon incorporation. That a-C could facilitate the graphitization process during the friction process which could improve the coating`s tribological performance. Therefore, that nanocomposite (Ti,Al,Si,C)N coatings with higher hardness (>36 GPa) and a lower friction coefficient (<0.2) could be synthesized and enhance the tribological performance and surface properties profoundly. Highlights ► The columnar crystals are restrained by C incorporation and a typical non-columnar growth mode is obtained. ► The (Ti,Ai,Si,C)N hard coatings has a super higher hardness (about 41 GPa) than that of Ti–Al–Si–N hard coatings. ► The (Ti,Ai,Si,C)N coatings have a very lower friction coefficient (about 0.18) than that of Ti–Al–Si–N hard coatings (about 0.6) and show a better wear state after friction.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Veprek · Appl. Phys. Lett. · 1995 · 66 · 264010.1063/1.113110 ↗
2. Karvankova · Surf. Coat. Technol. · 2006 · 200 · 297810.1016/j.surfcoat.2005.01.003 ↗
3. Xiao · Appl. Surf. Sci. · 2000 · 156 · 15510.1016/S0169-4332(99)00493-6 ↗
4. Derflinger · Surf. Coat. Technol. · 1999 · 113 · 28610.1016/S0257-8972(99)00004-3 ↗
5. Auner · Thin Solid Films · 1983 · 107 · 19110.1016/0040-6090(83)90021-4 ↗
6. Zhou · Thin Solid Films · 2009 · 517 · 524310.1016/j.tsf.2009.03.115 ↗
7. Li · Acta Mater. · 2006 · 54 · 204110.1016/j.actamat.2005.12.034 ↗
8. Wei · Appl. Surf. Sci. · 2011 · 257 · 788110.1016/j.apsusc.2011.04.066 ↗
9. Shum · Wear · 2004 · 257 · 103010.1016/j.wear.2004.07.014 ↗
10. Park · Thin Solid Films · 2004 · 447 · 44310.1016/S0040-6090(03)01122-2 ↗
11. Ma · Surf. Coat. Technol. · 2005 · 194 · 14310.1016/j.surfcoat.2004.05.007 ↗
12. Riberro · Surf. Coat. Technol. · 2004 · 188–189 · 35110.1016/j.surfcoat.2004.08.020 ↗
13. Shtansky · Surf. Coat. Technol. · 2009 · 203 · 359510.1016/j.surfcoat.2009.05.036 ↗
14. Ma · Acta Mater. · 2007 · 55 · 635010.1016/j.actamat.2007.07.046 ↗
15. Shi · Appl. Surf. Sci. · 2008 · 254 · 734210.1016/j.apsusc.2008.05.338 ↗
16. Manory · Surf. Coat. Technol. · 2002 · 155 · 13610.1016/S0257-8972(02)00131-7 ↗
17. Xu · Surf. Coat. Technol. · 2010 · 204 · 191410.1016/j.surfcoat.2009.09.006 ↗
18. Wang · Appl. Surf. Sci. · 2010 · 257 · 110.1016/j.apsusc.2010.06.050 ↗
19. Chen · Mater. Chem. Phys. · 2000 · 65 · 31010.1016/S0254-0584(00)00255-8 ↗
20. Ma · Chin. Tribol. · 2003 · 23 · 179
21. Liu · Acta Mater. · 2004 · 52 · 72910.1016/j.actamat.2003.10.010 ↗
22. Daniel · Wear · 2003 · 254 · 108410.1016/S0043-1648(03)00340-5 ↗
23. Huang · Appl. Surf. Sci. · 2006 · 253 · 247010.1016/j.apsusc.2006.05.003 ↗