Abstract The impact of the ZrO2/La2O3 film thickness ratio and the post deposition annealing in the temperature range between 400 °C and 600 °C on the electrical properties of ultrathin ZrO2/La2O3 high-k dielectrics grown by atomic layer deposition on (1 0 0) germanium is investigated. As-deposited stacks have a relative dielectric constant of 24 which is increased to a value of 35 after annealing at 500 °C due to the stabilization of tetragonal/cubic ZrO2 phases. This effect depends on the absolute thickness of ZrO2 within the dielectric stack and is limited due to possible interfacial reactions at the oxide/Ge interface. We show that adequate processing leads to very high-k dielectrics with EOT values below 1 nm, leakage current densities in the range of 0.01 A/cm2, and interface trap densities in the range of 2–5 × 1012 eV−1 cm−2.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Ferroelectric and Negative Capacitance Devices · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. International Technology Roadmap for Semiconductors, 2007.
2. Wilk · Journal of Applied Physics · 2001 · 89 · 524310.1063/1.1361065 ↗
3. Sze · 1981
4. Kamata · Materials Today · 2008 · 11 · 3010.1016/S1369-7021(07)70350-4 ↗
5. Zimmerman · 2006
6. Dimoulas · Thin Solid Films · 2007 · 515 · 633710.1016/j.tsf.2006.11.129 ↗
7. Chui · Technical Digest – International Electron Devices Meeting · 2002 · 43710.1109/IEDM.2002.1175872 ↗
8. Nieminen · Applied Surface Science · 2001 · 174 · 15510.1016/S0169-4332(01)00149-0 ↗
9. Triyoso · Journal of Vacuum and Science Technology B · 2005 · 23 · 28810.1116/1.1849217 ↗
10. Kim · Applied Physics Letters · 2007 · 90 · 10310410.1063/1.2709951 ↗
11. Abermann · Journal of the Electrochemical Society · 2009 · 156 · G5310.1149/1.3095475 ↗
12. Mavrou · Applied Physics Letters · 2008 · 103 · 014506
13. Mavrou · Applied Physics Letters · 2008 · 93 · 21290410.1063/1.3033546 ↗
14. Tsoutsou · Microelectronic Engineering · 2009 · 86 · 162610.1016/j.mee.2009.02.037 ↗
15. Tsoutsou · Applied Physics Letters · 2009 · 94 · 05350410.1063/1.3075609 ↗
16. Lamagna · Applied Physics Letters · 2009 · 95 · 12290210.1063/1.3227669 ↗
17. Liu · ECS Transactions · 2008 · 16 · 47110.1149/1.2981628 ↗
18. Lee · Microelectronic Engineering · 2009 · 86 · 165810.1016/j.mee.2009.03.056 ↗
19. Abermann · Applied Physics Letters · 2009 · 94 · 26290410.1063/1.3173199 ↗
20. Chui · IEEE Electron Device Letters · 2004 · 25 · 27410.1109/LED.2004.827285 ↗
21. Deegan · Applied Surface Science · 1998 · 123–124 · 6610.1016/S0169-4332(97)00511-4 ↗
22. Martens · Microelectronic Engineering · 2007 · 84 · 214610.1016/j.mee.2007.04.039 ↗
23. J. R. Hauser and K. Ahmed, Characterization Metrology ULSI Technology, 1998, 230.
24. Tsipas · Applied Physics Letters · 2008 · 93 · 08290410.1063/1.2977555 ↗
25. Thangadurai · Journal of Material Science · 2005 · 40 · 396310.1007/s10853-005-2831-9 ↗
26. Dimoulas · Applied Physics Letters · 2010 · 96 · 01290210.1063/1.3284655 ↗
27. Schroder · 1998
28. Lee · Journal of Crystal Growth · 2009 · 311 · 218710.1016/j.jcrysgro.2008.11.045 ↗