journal article·2019-10Open access

Development and characterization of magnetron sputtered self-lubricating Au-Ni/a-C nano-composite coating on CuCrZr alloy substrate

Zhaoxi Chen, Li Qiao, Julien Hillairet, Yuntao Song, Viviane Turq, Peng Wang, Raphael Laloo, Jean-Michel Bernard, Kun Lu, Yong Cheng, Qingxi Yang, Caroline Hernandez

Abstract

Abstract Compounding Au-Ni with carbon (C) lubricants is a feasible approach to improve its mechanical properties and wear performance. In this study, 3.5 μm-thick Au-Ni/C nanocomposite coatings with a low residual stress on CuCrZr substrates by magnetron sputtering were developed. Face-centered cubic and hexagonal close-packed stacking structures were both confirmed in the composite coatings based on transmission electron microscopy and X-ray diffraction analyses. Amorphous C (a-C) was confirmed to be the structure of C in the composite coatings, and its graphitization transition with an increase in the C content was validated by X-ray photoemission spectra and Raman spectroscopy. By compounding 0.88 wt% a-C, the hardness of the Au-Ni/a-C coating reached 400 HV, which is twice higher than that of the Au-Ni coating. The electrical resistivity of the Au-Ni/a-C coating is relatively stable with an increase in the a-C content. As graphitization occurred on the wear track, the produced composite coatings showed a minimum wear rate of 2.2 × 10−6 mm3/N·m under atmospheric conditions, which is half that of the Au-Ni reference coating. Under vacuum, the wear performance of the produced Au-Ni/a-C composite coatings was similar to that of the Au-Ni reference coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Lubricants and Their Additives

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Development of a new electroplating solution for electrodeposition of Au–Co alloys10.1016/j.surfcoat.2006.02.004 ↗
2. Development of new electrolytic and electroless gold plating processes for electronics applications10.1016/j.stam.2006.05.003 ↗
3. The effect of Tl (I) on the hard gold alloy electrodeposition of Au–Co from acid baths10.1016/j.jelechem.2010.04.013 ↗
4. Fractal analysis of the evolution of friction surfaces of galvanic AuNi coatings10.1134/S106378501205029X ↗
5. Composition, Structure & Hardness of pulse-plated nickel-hardened gold films
6. Application of a Doehlert experimental design to the optimization of an Au–Co plating electrolyte10.1007/s10800-004-1703-3 ↗
7. Mechanical properties and microstructure of Au–Ni–TiO2 nano-composite coatings10.1016/j.matchar.2015.03.008 ↗
8. Characterizations of thermal stability and electrical performance of Au-Ni coating on CuCrZr substrate for high vacuum radio-frequency contact application10.1016/j.tsf.2018.05.035 ↗
9. An electrochemical study of Au–Ni alloy electrodeposition from cyanide–citrate electrolytes10.1016/j.jelechem.2004.10.024 ↗
10. Electrodeposition of amorphous Au–Ni alloy film10.1016/j.electacta.2008.01.018 ↗
11. Mechanical and electrical properties of Au-Ni-C alloy films produced by pulsed current electrodeposition10.1149/2.012311jes ↗
12. Soft gold coatings: influence of additives and pulse plating10.1179/0020296712Z.00000000048 ↗
13. The effect of carbon nanotubes on the corrosion and tribological behavior of electroless Ni–P–CNT composite coating10.1016/j.apsusc.2011.10.067 ↗
14. Electrodeposition and mechanical properties of Ni–carbon nanotube nanocomposite coatings10.1016/j.jpcs.2007.10.049 ↗
15. Preparation and corrosion behavior of Ni and Ni–graphene composite coatings10.1016/j.materresbull.2012.12.064 ↗
16. Carbon nanofiber-copper composites fabricated by electroplating10.1149/1.1644354 ↗
17. Self-lubricating and anti-corrosion amorphous carbon/Fe3C composite coating on M50NiL steel by low temperature plasma carburizing10.1016/j.surfcoat.2016.06.078 ↗
18. Mechanical properties of nanostructured copper-hydrogenated amorphous carbon composite films studied by nanoindentation10.1016/j.surfcoat.2003.10.117 ↗
19. Evaluation of phase, composition, microstructure and properties in TiC/aC:H thin films deposited by magnetron sputtering10.1016/j.apsusc.2004.05.278 ↗
20. Tribological behaviour of titanium carbide/amorphous carbon nanocomposite coatings: from macro to the micro-scale10.1016/j.surfcoat.2008.02.012 ↗
21. Metal carbide/amorphous C-based nanocomposite coatings for tribological applications10.1016/j.surfcoat.2009.05.038 ↗
22. Preparation, biocompatibility, and biotribological properties of TiN-incorporated graphite-like amorphous carbon bio-ceramic composite films10.1016/j.ceramint.2018.01.102 ↗
23. Gradient titanium and silver based carbon coatings deposited on AISI316L10.1016/j.apsusc.2012.12.088 ↗
24. Structural effects of nanocomposite films of amorphous carbon and metal deposited by pulsed-DC reactive magnetron sputtering10.1016/j.diamond.2007.07.012 ↗
25. SEM study of defects in PVD hard coatings10.1016/j.vacuum.2007.07.005 ↗
26. Performance of HIPIMS deposited CrN/NbN nanostructured coatings exposed to 650 °C in pure steam environment10.1016/j.matchemphys.2016.05.017 ↗
27. Numerical evaluation of the exact phase diagram of an empirical Hamiltonian: embedded atom model for the Au-Ni system
28. Comparison of Au and Au–Ni alloys as contact materials for MEMS switches10.1109/JMEMS.2008.2010850 ↗
29. Comparative surface and nano-tribological characteristics of nanocomposite diamond-like carbon thin films doped by silver10.1016/j.apsusc.2008.07.193 ↗
30. Noblest of all metals is structurally unstable at high pressure10.1103/PhysRevLett.98.045503 ↗
31. Synthesis of hexagonal close-packed gold nanostructures10.1038/ncomms1291 ↗
32. Modified Scherrer equation to estimate more accurately nano-crystallite size using XRD10.4236/wjnse.2012.23020 ↗
33. Controlled growth of hexagonal gold nanostructures during thermally induced self-assembling on Ge (001) surface10.1038/srep42420 ↗
34. Yeo · 2017
35. Amorphous self-lubricant MoS2-C sputtered coating with high hardness10.1016/j.apsusc.2015.01.057 ↗
36. Characterization of amorphous and nanocrystalline carbon films10.1016/j.matchemphys.2005.07.048 ↗
37. Lubricated sliding wear mechanism of chromium-doped graphite-like carbon coating10.1016/j.triboint.2014.04.007 ↗
38. Interpretation of Raman spectra of disordered and amorphous carbon10.1103/PhysRevB.61.14095 ↗
39. Effect of carbon content on nanostructural, mechanical and electrochemical characteristics of self-organized nc-ZrCN/a-CN × nanocomposite films10.1016/j.apsusc.2014.11.181 ↗
40. Residual stress and cracking in thin PVD coatings10.1016/S0042-207X(01)00327-X ↗
41. Residual stress determination in thermally sprayed coatings—a comparison of curvature models and X-ray techniques10.1016/j.surfcoat.2005.06.003 ↗
42. State of residual stress in laser-deposited ceramic composite coatings on aluminum alloys10.1016/j.actamat.2006.07.049 ↗
43. Combinatorial study of gradient Ag–Al thin films: microstructure, phase formation, mechanical and electrical properties10.1021/acsami.6b10659 ↗
44. Effect of residual stresses on mechanical properties and interface adhesion strength of SiN thin films10.1016/j.tsf.2009.03.043 ↗
45. Failure modes in scratch adhesion testing10.1016/0257-8972(91)90188-3 ↗
46. Study of tribological performance of ECR–CVD diamond-like carbon coatings on steel substrates: part 2. The analysis of wear mechanism10.1016/j.wear.2004.10.005 ↗