journal article·2011-10

The mechanism of oxide whisker growth and hot corrosion of hot-dipped Al–Si coated 430 stainless steels in air–NaCl(g) atmosphere

Hsiao-Hung Liu, Wei-Jen Cheng, Chaur-Jeng Wang

Applied Surface Science· Volume 257· Issue 24
Publisher page

Abstract

Abstract The mechanisms of oxide whisker growth and hot corrosion of 430 stainless steel (430SS) and aluminide 430 stainless steel hot-dipped in a Al–10 wt.%Si molten bath (430HDAS) were studied at 750 and 850 °C in air mixed with 500 and 990 vppm NaCl(g). The results showed that the loose Cr2O3 scale which formed on the 430SS could not prevent the corrosion of 430SS in a 500 vppm NaCl(g) atmosphere, resulting in the formation of Fe2O3 scale. Fe2O3 whiskers grew at the grain boundary of the Fe2O3 scale. However, no Fe2O3 whiskers formed on the Fe2O3 scale while 430SS was exposed in a 900 vppm NaCl(g) atmosphere. During the initial high-temperature corrosion of 430HDAS in a 500 vppm NaCl(g) atmosphere, a dense Al2O3 scale formed on the surface of the specimens. Also, Al2O3 whiskers grew on the Al2O3 scale. As exposure time increased, cyclic chlorination/oxidation degraded the protective aluminide layer and caused the formation of Fe2O3 scale and Fe2O3 whiskers. The morphology of Fe2O3 whiskers formed at 750 °C is more slender than those formed at 850 °C. The formation and growth of both Fe2O3 and Al2O3 whiskers may be attributed to the chloridation of both the steel substrate and aluminide layer, accelerating the diffusion rate of metallic ions in the oxide scales.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Aluminum Alloy Microstructure Properties · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. NaCl-induced hot corrosion of Fe–Mn–Al–C alloys10.1016/S0254-0584(01)00515-6 ↗
2. NaCl-induced accelerated oxidation of 304 stainless steel and Fe-Mn-Al alloy at 900°C10.1023/A:1025677331351 ↗
3. Corrosion behaviors of low carbon steel, SUS310 and Fe–Mn–Al alloy with hot-dipped aluminum coatings in NaCl-induced hot corrosion10.1016/S0257-8972(02)00588-1 ↗
4. The high-temperature oxidation behavior of hot-dipping Al–Si coating on low carbon steel10.1016/j.surfcoat.2005.11.031 ↗
5. Observation of high-temperature phase transformation in the Si-modified aluminide coating on mild steel using EBSD10.1016/j.matchar.2010.02.001 ↗
6. Analysis of coating layer formed on steel strips during aluminising by hot dipping in Al–Si baths10.1179/mst.1997.13.10.832 ↗
7. On the influence of silicon on the growth of the alloy layer during hot dip aluminizing10.1007/BF00553379 ↗
8. Chemical vapor deposition of smooth α-Al2O3 films on nickel base superalloys as diffusion barriers10.1016/S0257-8972(99)00333-3 ↗
9. Anistropic grain growth in α-Fe2O3-doped alumina10.1016/S0955-2219(96)00091-X ↗
10. Microstructural study of the influence of NaCl vapor on the oxidation of a Ni–Cr–Al alloy at 850°C10.1007/BF00609972 ↗
11. Oxdation of FeCrAl alloy: influence of temperature and atmosphere on scale growth and mechanism10.1016/S0257-8972(00)00989-0 ↗
12. The microstructure of the scale formed during the high temperature oxidation of a Fe–Cr alloy steel10.1016/0010-938X(84)90036-2 ↗
13. The effect of NaCl(g) on the oxidation of NiAl10.1149/1.2131663 ↗
14. The oxidation of incoloy 800 in moist air containing HCl(g) at 800°C10.1016/0010-938X(84)90066-0 ↗
15. Accelerated oxidation rate of chromium induced by sodium chloride10.1007/BF00659274 ↗
16. Deposition and high temperature corrosion in a 10MW straw fired boiler10.1016/S0378-3820(97)00062-3 ↗
17. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
18. Cyclic-oxidation behavior of thermal-barrier coatings exposed to NaCl vapor10.1007/s11085-007-9088-4 ↗
19. Oxidation of FeCrAl alloy: influence of temperature and atmosphere on scale growth rate and mechanism10.1016/S0257-8972(00)00989-0 ↗
20. The microstructure of the scale formed during the high temperature oxidation of a fecralloy steel10.1016/0010-938X(84)90036-2 ↗
21. Pilling–Bedworth ratio for oxidation of alloys10.1007/s100190050008 ↗
22. Accelerated oxidation of chromium by trace of sodium chloride vapor10.2320/matertrans1989.32.969 ↗
23. Khanna · 2002