Nanoscale multilayered and porous carbide interphases prepared by pressure-pulsed reactive chemical vapor deposition for ceramic matrix composites
Source abstract
Abstract
Abstract In Ceramic Matrix Composites (CMCs) reinforced by continuous fibers, a good toughness is achieved by adding a thin film called “interphase” between the fiber and the brittle matrix, which acts as a mechanical fuse by deflecting the matrix cracks. Pyrocarbon (PyC), with or without carbide sub-layers, is typically the material of choice to fulfill this role. The aim of this work was to study PyC-free nanoscale multilayered carbide coatings as interphases for CMCs. Nanoscale multilayered (SiC–TiC) n interphases were deposited by pressure-Pulsed Chemical Vapor Deposition (P-CVD) on single filament Hi-Nicalon fibers and embedded in a SiC matrix sheath. The thicknesses of the carbide interphase sub-layers could be made as low as a few nanometers as evidenced by scanning and transmission electron microscopy. By using the P-ReactiveCVD method (P-RCVD), in which the TiC growth involves consumption of SiC, it was not only possible to obtain multilayered (SiC–TiC) n films but also TiC films with a porous multilayered microstructure as a result of the Kirkendall effect. The porosity in the TiC sequences was found to be enhanced when some PyC was added to SiC prior to total RCVD consumption. Because the porosity volume fraction was still not high enough, the role of mechanical fuse of the interphases could not be evidenced from the tensile curves, which remained fully linear even when chemical attack of the fiber surface was avoided.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. The role of the fiber-matrix interface in ceramic composites
2. Interphase in composite materials10.4028/www.scientific.net/KEM.127-131.583 ↗
3. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
4. Oxidation embrittlement probe for ceramic-matrix composites10.1111/j.1151-2916.1995.tb08621.x ↗
5. Recent developments in fibers and interphases for high temperature ceramic matrix composites10.1016/S1359-835X(98)00131-6 ↗
6. Single- and multilayered interphases in SiC/SiC composites exposed to severe environmental conditions: an overview10.1111/j.1744-7402.2009.02424.x ↗
7. Simultaneous fatigue and combustion exposure of a SiC/SiC ceramic matrix composite10.1177/0021998310373519 ↗
8. Multiple zirconia interphase for SiC/SiCf composites10.1016/j.surfcoat.2010.10.025 ↗
9. Atomic force and scanning electron microscopy study of zirconia-coated silicon carbide fibers10.1016/j.jeurceramsoc.2006.08.016 ↗
10. Low dose irradiation performance of SiC interphase SiC/SiC composites10.1016/S0022-3115(97)00321-8 ↗
11. The effect of neutron irradiation on the fiber/matrix interphase of silicon carbide composites10.1016/j.jnucmat.2008.11.015 ↗
12. Thermophysical and mechanical properties of near-stoichiometric fiber CVI SiC/SiC composites after neutron irradiation at elevated temperatures10.1016/j.jnucmat.2010.06.002 ↗
13. Hi-Nicalon/SiC minicomposites with (Pyrocarbon/SiC)n nanoscale multilayered interphases10.1111/j.1151-2916.1999.tb02105.x ↗
14. Synthesis of highly tailored ceramic matrix composites by pressure-pulsed CVI10.1016/S0167-2738(01)00743-3 ↗
15. Physico-chemistry of interfaces in inorganic-matrix composites10.1016/S0266-3538(00)00107-X ↗
16. SiC/SiC minicomposites with (PyC/TiC)n interphases processed by pressure-pulsed reactive CVI10.1023/B:JMSC.0000007742.34926.65 ↗
17. Reactive chemical vapor deposition (R.C.V.D.) as a method for coating carbon fibre with carbides, 1989 MRS Fall Meeting10.1557/PROC-168-305 ↗
18. Influence of carbide coatings on the oxidation behavior of carbon fibers10.1016/0008-6223(94)00170-5 ↗
19. Formation of carbide coatings on Nicalon fiber by gas-phase transport reactions10.1023/A:1022650907968 ↗
20. Protective ceramic multilayer coatings for carbon fibers10.1016/j.surfcoat.2006.03.046 ↗
21. The chemistry, morphology, topography of titanium carbide modified carbon fibers10.1016/j.carbon.2007.11.019 ↗
22. Which alternative to the pyrocarbon interphase in ceramic matrix composites?10.3166/acsm.30.609-620 ↗
23. Micro/minicomposites: a useful approach to the design and development of non-oxide CMCs10.1016/S1359-835X(98)00147-X ↗
24. Synthesis of TiC from porous carbon coating on Si–C–O (Nicalon) fibres by reactive chemical vapour deposition in pressure-pulsed mode or at atmospheric pressure10.1007/s10853-010-4769-9 ↗
25. The growth of Ti3SiC2 coatings onto SiC by reactive chemical vapor deposition using H2 and TiCl410.1016/j.surfcoat.2006.09.040 ↗
26. Phase equilibria and reactive chemical vapour deposition (RCVD) of Ti3SiC210.1007/s11669-008-9284-1 ↗
27. Thin-film preparation of C/C composites and CMC using the broad argon ion beam method
28. Micromechanical and statistical approach to the behavior of CMC's10.1002/9780470314234.ch50 ↗
29. Formation of nanotubes and hollow nanoparticles based on Kirkendall and diffusion processes: a review10.1002/smll.200700382 ↗
30. Fibers coatings for ceramic matrix composites
31. H.W. Carpenter, J. Bohlen, N.S. Steffier Weak frangible fiber coating with unfilled pores for toughening ceramic fiber-matrix composites, US Patent No. 5.221.578 (1993).