Nanostructured two-phase nc-TiN/a-(TiB2, BN) nanocomposite thin films
Source abstract
Abstract
Abstract Thin films of Ti–B–N with different N contents were deposited on Si(1 0 0) at room temperature by reactive unbalanced close-field dc-magnetron sputtering using three Ti targets and one TiB2 target in an Ar–N2 gas mixture. The effect of N content on bonding structure, microstructure, phase configuration, surface roughness and mechanical properties have been investigated using X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), cross-sectional scanning electron microscopy (SEM), plan-view and cross-sectional high-resolution transmission electron microscopy (HRTEM), atomic force microscopy (AFM) and microindentation measurements. It was found that the N content significantly affected phase segregation and microstructure. The nitrogen-free TiB0.65 films showed an amorphous compound consisting of Ti and TiB2 (Ti–TiB2). After adding about 28 at.% N, Ti was preferentially bonded to N to form TiN, accompanying with formation of small amounts of TiB and BN bonds. At this stage they combined TiB2 to form a two-phase nanocomposite with microstructures comprising of nanocrystalline (nc-) TiN phase in nitrogen-containing amorphous (a-) TiB2 matrix. Addition of more N promoted formation of BN bonding at cost of TiB2, which resulted in formation of nanocomposite nc-TiN/a-(TiB2, BN) thin films. A small grain less than 8 nm in size was found at low N content, and the grain size increased with increasing N content. A low microhardness value of about 20 GPa was obtained in the amorphous Ti–TiB2 compound, and a maximum microhardness value of about 50 GPa was achieved in nc-TiN/a-TiB2. A decrease of microhardness took place after formation of BN (i.e. amorphous matrix composed by both TiB2 and BN) with further increasing N content, and a hardness value of about 35 GPa was followed at high N contents. The surface roughness strongly depended on the phase configuration. The higher the mole fraction of nanocrystalline TiN phase, the rougher the surface became.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Gissler · Surf. Coat. Technol. · 1994 · 68–69 · 55610.1016/0257-8972(94)90217-8 ↗
2. Veprek · J. Vac. Sci. Technol. A · 1999 · 17 · 240110.1116/1.581977 ↗
3. Karvankova · Surf. Coat. Technol. · 2003 · 163–164 · 14910.1016/S0257-8972(02)00492-9 ↗
4. Baker · J. Vac. Sci. Technol. A · 1995 · 13 · 163310.1116/1.579743 ↗
5. Ruby · Surf. Interface Anal. · 2000 · 29 · 82310.1002/1096-9918(200012)29:12<823::AID-SIA933>3.0.CO;2-C ↗
6. Wiedemann · Surf. Coat. Technol. · 1999 · 116–119 · 30210.1016/S0257-8972(99)00130-9 ↗
7. Musil · Surf. Coat. Technol. · 2000 · 125 · 32210.1016/S0257-8972(99)00586-1 ↗
8. Hammer · Surf. Coat. Technol. · 1994 · 68–69 · 19410.1016/0257-8972(94)90159-7 ↗
9. Gissler · Diamond Film Technol. · 1997 · 7 · 165
10. Zhang · Appl. Phys. Lett. · 1996 · 68 · 68
11. Knotek · J. Hard Mater. · 1992 · 3 · 29
12. Baker · J. Vac. Sci. Technol. A · 1997 · 15 · 28410.1116/1.580526 ↗
13. Shirley · Phys. Rev. B · 1972 · 5 · 470910.1103/PhysRevB.5.4709 ↗
14. Lu · Surf. Coat. Technol. · 2004 · 187 · 9810.1016/j.surfcoat.2003.11.024 ↗
15. Carrasco · Mater. Charact. · 2002 · 48 · 8110.1016/S1044-5803(02)00256-5 ↗
16. Dean · 1999
17. Rogl · 1992
18. Krzanowski · Surf. Coat. Technol. · 2004 · 188–189 · 37610.1016/j.surfcoat.2004.08.028 ↗
19. Lu · J. Vac. Sci. Technol. B · 2005 · 23 · 44910.1116/1.1865117 ↗