Investigation of thermally grown oxide on 4H-SiC by a combination of H2O and HNO3 vapor with varied HNO3 solution heating temperature
Source abstract
Abstract
Abstract A new technique of oxidizing n-type 4H-SiC in a combination of H2O and nitric acid (HNO3) vapor at various heating temperatures (60 °C, 70 °C, 80 °C, 90 °C, 100 °C and 110 °C) of HNO3 solution has been introduced in this work. Utilizing secondary ion mass spectroscopy, effects of H+ and N− on the passivation of structural defects at the bulk oxide and partial of the SiC/SiO2 interface have been discussed. The effects of heating temperature of HNO3 solution on structural properties of the SiC substrate; after the oxide has been removed have been systematically investigated. Contact angles and the surface roughness of the substrate were recorded from a Goniometer and an atomic force microscope, respectively. It has been revealed that as compared to oxide grown by conventional wet (H2O vapor only) oxidation technique; this “wet diluted nitridation” technique is able to produce oxide with lower interface-state density and higher breakdown voltage. Physical properties of the substrate after oxide removal show surface roughness reduces as the heating temperature of HNO3 solution increases, which is mainly attributed by the significant reduction of carbon content at the SiC/SiO2 interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. J.H. Zhao, Silicon carbide power field-effect transistors, in: E.L. Fleischer, Advances in Silicon Carbide Electronics, MRS Bulletin, USA, 2005, p. 293.10.1557/mrs2005.76 ↗
2. Silicon carbide benefits and advantages for power electronics circuits and systems10.1109/JPROC.2002.1021562 ↗
3. Investigation of the 4H–SiC surface10.1016/j.apsusc.2008.03.056 ↗
4. S. Dhar, S. Wang, Williams Jr., S.T. Pantelides, L.C. Feldman, Interface passivation for silicon dioxide layers on silicon carbide, in: E.L. Fleischer, Advances in Silicon Carbide Electronics, MRS Bulletin, USA, 2005, pp. 288–290.10.1557/mrs2005.75 ↗
5. Contributions to the density of interface states in SiC MOS structures
6. Alternative techniques to reduce interface traps in n-type 4H-SiC MOS capacitors
7. Oxidation, MOS capacitors and MOSFETs
8. Detection and electrical characterization of defects at the SiO2/4H-SiC interface10.4028/www.scientific.net/MSF.645-648.463 ↗
9. Experimental identification of extra type of charges at SiO2/SiC interface in 4H-SiC10.4028/www.scientific.net/MSF.645-648.519 ↗
10. Trapping of majority carriers in SiO2/4H-SiC structures10.1088/0022-3727/42/12/125301 ↗
11. Interfaces between 4H-SiC and SiO2: microstructure, nanochemistry and near-interface traps10.1063/1.1836004 ↗
12. Reduction of interface-state density in 4H–SiC n-type metal–oxide–semiconductor structures using high-temperature hydrogen annealing10.1063/1.126103 ↗
13. Influence of the post-oxidation process on the MOS interface and MOSFETs properties10.4028/www.scientific.net/MSF.353-356.643 ↗
14. Strong dependence of the inversion mobility of 4H and 6H SiC (0001) MOSFETs on the water content in pyrogenic re-oxidation annealing10.1109/55.974797 ↗
15. Improvement of charge trapping by hydrogen post-oxidation annealing in gate oxide of 4H–SiC metal–oxide–semiconductor capacitors10.1063/1.1289806 ↗
16. Intrinsic SiC/SiO2 interface states10.1002/1521-396X(199707)162:1<321::AID-PSSA321>3.0.CO;2-F ↗
17. Effects of nitridation in gate oxides grown on 4H-SiC10.1063/1.1412579 ↗
18. 4H-SiC MISFET with nitrogen-containing insulators
19. Properties of nitrided oxides on SiC
20. Significant improvement in reliability of thermal oxide on 4H-SiC (0001) face using ammonia post-oxidation annealing10.4028/www.scientific.net/MSF.645-648.685 ↗
21. K. Das Mrinal, Commercially available Cree silicon carbide power devices: historical success of JBS diodes and future power switch prospects, CS MANTECH Conference, Palm Springs: California, 2011.
22. Density of interface states, electron traps, and hole traps as a function of the nitrogen density in SiO2 on SiC10.1063/1.3131845 ↗
23. Increase in oxide hole trap density associated with nitrogen incorporation at the SiO2/SiC interface10.1063/1.2940736 ↗
24. Electrical and physical characterization of gate oxides on 4H-SiC grown in diluted N2O10.1063/1.1555696 ↗
25. Steam-induced interface improvement of N2O-nitrided SiO2 grown on 6H–SiC10.1016/S0038-1101(03)00012-1 ↗
26. Improved electrical properties of SiC-MOS interfaces by thermal oxidation of plasma nitrided 4H-SiC(0001) surfaces10.4028/www.scientific.net/MSF.645-648.507 ↗
27. Kobayashi Formation of atomically smooth SiO2/SiC interfaces at ∼120°C by use of nitric acid oxidation method10.1016/j.susc.2005.11.005 ↗
28. Nitric acid oxidation method to form SiO2/3C–SiC structure at 120°C10.1016/j.apsusc.2007.10.102 ↗
29. Low temperature formation of SiO2/Si structure by nitric acid vapour10.1063/1.2395601 ↗
30. Ultrathin SiO2 layer with a low leakage current density formed with ∼100% nitric acid vapour10.1088/0957-4484/21/11/115202 ↗
31. Band alignment of SiO2/Si structure formed with nitric acid vapour below 500°C10.1016/j.susc.2009.01.026 ↗
32. Effects of Wet N2O Oxidation on Interface Properties of 6H-SiC MOS Capacitors10.1109/LED.2002.1015220 ↗
33. Schroder · 2006
34. Characterization of border trap generation in rapid thermally annealed oxides deposited using silane chemistry10.1063/1.368384 ↗
35. Re-oxidation characteristics of oxynitrides on 3C- and 4H-SiC10.1007/s11664-999-0007-0 ↗
36. Effect of near-interfacial nitrogen on the oxidation behavior of ultrathin silicon oxynitrides10.1063/1.365264 ↗
37. Nelson Martinez · 2009 · 1
38. Study of HF-treated heavily-doped Si surface using contact angle measurements10.1143/JJAP.33.6508 ↗
39. Contact measurement and contact angle interpretation10.1016/S0001-8686(98)00087-6 ↗
40. Wet surface technologies
41. Effects of thermal nitrided gate-oxide thickness on 4H silicon-carbide-based metal-oxide-semiconductor characteristics