The effects of treatment of Si(111) surfaces with NH4F solution on Schottky diode parameters
Source abstract
Abstract
Abstract A study on Al/p-Si(1 1 1) Schottky barrier diodes (SBDs) parameters with and without a thin chemical oxide layer on p-type Si has been performed. The oxide layer has been formed by a wet chemical oxidation in HNO 3 solution. In order to avoid native oxide formation on the sample surface, the silicon dangling bonds have been passivated with hydrogen atoms by dipping in a NH 4 F solution. It is shown that these treatments give almost the same barrier height values. In addition, it has been found that the treatment of the sample back surface in NH 4 F solution reduces the reverse current and the series resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and interfaces · Semiconductor materials and devices · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Infrared spectroscopy study of initial stages of oxidation of hydrogen-terminated Si surfaces stored in air10.1063/1.357627 ↗
2. In situ infrared observation of etching and oxidation processes on Si surfaces in NH4F solution10.1149/1.1393393 ↗
3. Preparation of air-stable, low recombination velocity Si(111) surfaces through alkyl termination10.1063/1.1312203 ↗
4. V.L. Thanh, Low-temperature wet chemical cleaning of Si(001) surfaces for MBE and GSMBE of Si and SiGeC, in: D. Glocken, S.I. Shah, L. Vescan (Eds.), Handbook of Thin Film Process Technology, Institute of Physics Publishing, 2000, pp. G6:1–G6:11.10.1063/1.372403 ↗
5. Surface barrier detectors using aluminium on n- and p-type silicon for α-spectroscopy10.1016/S0168-9002(00)00991-8 ↗
6. The effects of the time-dependent and exposure time to air on Au/epilayer n-Si Schottky diodes10.1051/epjap:1999156 ↗
7. Schottky diodes with high series resistance: limitations of forward I–V methods10.1063/1.357909 ↗
8. S.M. Sze, Physics of Semiconductor Devices, Bell Laboratories, Murray Hill, NJ, 1969, Chapter 8, p. 378.
9. J.H. Werner, U. Rau, in: J.F. Luy, P. Russer (Eds.), Springer Series in Electronics and Photonics, Springer, Berlin, 1994, p. 32.
10. Evaluation of various electrode metals for ultra-high purity P-type Si surface barrier detectors10.1109/TNS.1984.4333272 ↗
11. Initial stage of native oxide growth on hydrogen terminated silicon (111) surfaces10.1063/1.360853 ↗
12. Initial stages of oxidation of hydrogen-terminated Si surface stored in air10.1016/0169-4332(96)00319-4 ↗
13. Fabrication of low noise silicon radiation detectors by the planar process10.1016/0029-554X(80)90948-9 ↗
14. Current and capacitance measurements as a fast diagnostic tool for evaluation of semiconductor parameters10.1016/S0168-9002(99)00929-8 ↗