journal article·2003-06

Improvement of hot-carrier-reliability by deuterium termination of Si/SiO2 interface defects

H. Takahashi, H. Yamada-Kaneta

Applied Surface Science· Volume 216· Issue 1-4
Publisher page

Abstract

Abstract We present the improvement of hot-carrier-reliability by deuterium annealing at the temperatures ranging from 430 to 460 °C in the case of CMOS transistors of the design rule of 0.13 μm. By means of secondary ion mass spectroscopy (SIMS) and ESR measurements, we confirm that this improvement is caused by the termination of the interface defects by deuterium atoms.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Ion-surface interactions and analysis · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (7)

Show source-provided references
1. Lyding · Appl. Phys. Lett. · 1996 · 68 · 252610.1063/1.116172 ↗
2. Van de Walle · Appl. Phys. Lett. · 1996 · 69 · 244110.1063/1.117664 ↗
3. Kizilyalli · IEEE Electron. Device Lett. · 1997 · 18 · 8110.1109/55.556087 ↗
4. Lee · Mater. Res. Soc. Symp. Proc. · 1998 · 510 · 30110.1557/PROC-510-301 ↗
5. Clark · IEEE Electron. Device Lett. · 1999 · 20 · 50110.1109/55.791923 ↗
6. Ference · IEEE Trans. Electron. Devices · 1999 · 46 · 74710.1109/16.753709 ↗
7. Clark · IEEE Electron. Device Lett. · 1999 · 20 · 4810.1109/55.737570 ↗