Abstract
Abstract Well-crystallized and stoichiometric Pb(Zr, Ti)O 3 (PZT) films, typically ∼5 μm thick, with pure perovskite-type rhombohedral structures have been successfully prepared via an electrospray assisted vapour deposition (ESAVD) method. Control of the deposition temperature within a narrow range of 300–400 °C resulted in films with the most desirable phases. PZT films with close stoichiometric match with the expected composition ratio and uniform element distribution were obtained by adding the appropriate levels of excess Pb in the precursor solutions. The annealed films were uniform, dense, compact and adherent to the substrates. The dielectric constant, ɛ r, and loss tangent, tan δ , of the fabricated PZT films measured at 10 kHz were 442 and 0.09, respectively. The ESAVD deposited PZT films showed a remanent polarization, P r , of 15.3 μC/cm 2 and coercive field, E c , of 86.7 kV/cm. These results demonstrate the clear potential of the ESAVD method as a promising technique for the fabrication of thick PZT films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Electronic and Structural Properties of Oxides · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Ferroelectric films10.1023/A:1008758020834 ↗
2. Xu · 1991
3. Electron emission type infrared imaging sensor using ferroelectric thin plate10.1016/S0924-4247(01)00802-0 ↗
4. Micromachining of PZT-based MEMS
5. PZT thin film bi-layer devices for phase controlled actuation in MEMS10.1023/A:1012256108078 ↗
6. Pyroelectric devices and materials10.1088/0034-4885/49/12/002 ↗
7. Preparation and characterization of Pb(Zr0.52Ti0.48)O3 ceramics from high-energy ball milling powders10.1016/S0167-577X(99)00190-1 ↗
8. Preparation of highly oriented Pb(Zr0.52Ti0.48)O3 thin films by sol–gel-hydrothermal process10.1557/JMR.1999.0364 ↗
9. Fabrication and investigation of ultrathin, and smooth Pb(Zr, Ti)O3 films for miniaturization of microelectronic devices10.1063/1.1524307 ↗
10. Crystalline and ferroelectric properties of Pb(Zr, Ti)O3 thin films grown by low-temperature metalorganic chemical vapor deposition10.1143/JJAP.41.6686 ↗
11. AES and XPS study of PZT thin film deposition by the laser ablation technique10.1016/S0272-8842(98)00013-3 ↗
12. Epitaxial growth of a (101) Pb(ZrxTi1−x)O3 film on an epitaxial (110)Ir/(100) ZrN/(100) Si substrate structure10.1143/JJAP.41.6653 ↗
13. Effects of poly(ethylene glycol) additive molecular weight on the microstructure and properties of sol–gel-derived lead zirconate titanate thin films10.1557/JMR.2003.0100 ↗
14. Growth of highly (100)-oriented Zr-rich PZT films on Pt/Ti/SiO2/Si substrates by a sol–gel process10.1080/00150190108016013 ↗
15. Epitaxial PbZr.52Ti.48O3 films on SrTiO3/(001)Si substrates deposited by sol–gel method10.1063/1.1498006 ↗
16. Preparation of Pb(Zr, Ti)O3 thin films by soft chemical route10.1016/S0955-2219(03)00318-2 ↗
17. Pyroelectric and piezoelectric properties of thick PZT films produced by a new sol–gel route10.1016/j.jeurceramsoc.2005.03.090 ↗
18. Multi-layer ferroelectric Pb(Zr0.52Ti0.48)O3 thick films prepared by pulsed laser deposition Integra10.1080/713718247 ↗
19. Jet molding system for realization of three-dimensional micro-structures10.1016/S0924-4247(98)00059-4 ↗
20. Preparation of piezoelectric Pb(Zr,Ti)O3–Pb(Zn1/3Nb2/3)O3 thick films on ZrO2 substrates using low-temperature firing10.1016/S0924-4247(01)00791-9 ↗
21. Screen-printed piezoelectric ceramic thick films with sintering additives introduced through a liquid-phase approach10.1016/j.sna.2004.08.022 ↗
22. Dense PZT thick films derived from sol–gel based nanocomposite process10.1016/S0921-5107(02)00568-8 ↗
23. Some characteristics of PZT films produced by jet molding system
24. PZT ‘composite’ ferroelectric thick films10.1016/S0955-2219(01)00260-6 ↗
25. Choy · 2002
26. Controlled synthesis of gas sensing Cr2–xTixO3 films by electrostatic spray assisted vapour deposition and their structural characterization10.1016/j.tsf.2005.09.169 ↗
27. Influence of Al2O3 diffusion barrier and PbTiO3 seed layer on microstructural and ferroelectric characteristics of PZT thin films by sol–gel spin coating method10.1016/S0040-6090(97)00034-5 ↗
28. Atomic force microscopic investigation of PZT thin films by MOD technology10.1080/00150199708224123 ↗
29. Fatigue of Pb(Zr0.53Ti0.47)O3 ferroelectric thin films10.1063/1.367953 ↗
30. Structural and electrical properties of excess PbO doped Pb(Zr0.52Ti0.48)O3 thin films using rf magnetron sputtering method10.1557/JMR.1998.0467 ↗
31. Effects of excess Pb on structural and electrical properties of Pb(Zr0.48Ti0.52)O3 thin films using MOD process10.1023/A:1017999223329 ↗
32. Raman scattering study of cubic to tetragonal phase transitions of Ti-rich Pb(ZrxTi1−x)O310.1143/JJAP.36.2985 ↗
33. Structural studies of Nd-modified lead zirconate titanate ceramics between 11 and 680K at the morphotropic phase boundary10.1103/PhysRevB.56.221 ↗
34. Polarized Raman scattering in transparent polycrystalline solid10.1103/PhysRevLett.26.1114 ↗
35. Chemical solution deposition of PZT thin layers on silicon: densification and stress development10.1179/096797804225012756 ↗
36. Pb(Zr0.52Ti0.48)O3 ceramics sintered with Li2Co3 and Na2CO3-improvement of characteristics10.1007/BF02431633 ↗
37. Pulsed laser deposition and characterization of PZT thin films10.1016/S0169-4332(99)00415-8 ↗
38. Characterization of sol–gel Pb(Zr0.53Ti0.47)O3 films in the thickness range 0.25–10μm10.1557/JMR.1999.0249 ↗
39. Preparation of PbZrO3–PbTiO3 ferroelectric thin films by the sol–gel process10.1111/j.1151-2916.1991.tb07298.x ↗