Surface modification of a MoSiON phase shift mask to reduce critical dimension variation after exposure to a 193-nm ArF excimer laser

Hyeokseong Choo, Dongwan Seo, Sangwoo Lim

Publisher page

Abstract

Abstract Introduction of a MoSi-based phase shift mask (PSM) improves photolithography resolution by causing light to shift phase by 180° thus canceling the overlap. However, when MoSiON PSM was exposed to an ArF excimer laser ( λ = 193 nm), a significant increase in patterned critical dimension (CD) was observed. It was confirmed that the CD increase resulted from oxidation progression into the MoSiON layer. In this study, N 2 O or NH 3 plasma treatment and thermal annealing in NH 3 effectively suppressed CD variation after ArF laser exposure. While the compositional ratio of Si, N, O, and Mo elements in the MoSiON layer was not changed, an increase in oxygen content only in the top 5 nm was observed. Therefore, it is concluded that slight oxidation of the top surface of MoSiON PSM by introducing either N 2 O or NH 3 plasma treatment or thermal annealing in NH 3 suppresses an increase in the patterned CD of MoSiON PSM after exposure to a 193-nm ArF excimer laser.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Photolithography Techniques · Advanced Surface Polishing Techniques · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Ultrafast high-resolution contact lithography with excimer lasers10.1147/rd.262.0151 ↗
2. Self-developing resist with submicrometer resolution and processing stability10.1063/1.94126 ↗
3. Pushing the limits of lithography10.1038/35023233 ↗
4. Improving resolution in photolithography with a phase-shifting mask10.1109/T-ED.1982.21037 ↗
5. High performance very large scale integrated photomask with a silicide film10.1116/1.583523 ↗
6. Practical attenuated phase-shifting mask with a single-layer absorptive shifter of MoSiO and MoSiON for ULSI fabrication
7. 193-nm radiation durability study of MoSi binary mask and resulting lithographic performance10.1117/12.899173 ↗
8. Study and improvement approach to 193-nm radiation damage of attenuated phase-shift mask10.1117/12.867710 ↗
9. Attenuated phase-shift mask with high tolerance for 193nm radiation damage10.1117/12.898984 ↗
10. XPS study of SiO thin films and SiO–metal interfaces
11. ESCA and SEXAFS investigations of insulating materials for ULSI microelectronics10.1016/0042-207X(90)94025-L ↗
12. Nitrogen 1s charge referencing for Si3N4 and related compounds10.1002/sia.740110611 ↗
13. X-ray photoelectron spectroscopy of thermally treated SiO2 surfaces10.1021/ac00289a033 ↗
14. Interaction of ion beams with surfaces reactions of nitrogen with silicon and its oxides10.1063/1.435869 ↗
15. Characterization of a boro-silicon oxynitride prepared by thermal nitridation of a polyborosiloxane10.1016/0925-8388(95)01982-0 ↗
16. X-ray photoelectron spectroscopy of some silicates10.1016/0009-2614(76)85029-4 ↗
17. Further examination of the Si KLL Auger line in silicon nitride thin films10.1016/0378-5963(81)90068-4 ↗
18. On the surface chemistry of molybdena-alumina catalysts prepared from Mo(CO)610.1016/0021-9517(89)90005-5 ↗
19. Surface studies and catalytic properties of the bifunctional bulk MoO2 system10.1002/sia.1288 ↗
20. A new barium molybdate phase10.1016/0025-5408(87)90052-3 ↗
21. Improved the surface roughness of silicon nanophotonic devices by thermal oxidation method
22. Polycrystalline silicon oxidation method improving surface roughness at the oxide/polycrystalline silicon interface10.1063/1.113948 ↗
23. Reduction of etched AlGaAs sidewall roughness by oxygen-enhanced wet thermal oxidation10.1063/1.2766859 ↗