journal article·2026-04-16Open access

Fabrication of Thin Copper Anode Current Collectors on Ceramic Solid Electrolytes Using Atmospheric Plasma Spraying for Anode-Free Solid-State Batteries

Andre Borchers, Timo Paschen, Manuela Ockel, Florian Vollnhals, Cornelius Dirksen, Martin Muckelbauer, Berik Uzakbaiuly, George Sarau, Jörg Franke, Silke Christiansen

Batteries· Volume 12· Issue 4

Abstract

Metal anodes offer substantially higher specific and volumetric capacities than conventional anode materials such as graphite in lithium-ion batteries or hard carbon in sodium-ion batteries. However, the integration of metal anodes into solid-state batteries poses significant challenges, particularly with respect to processing, interfacial stability, and cell assembly. Anode-free solid-state batteries (AFSSBs) address these challenges by eliminating the pre-installed metal anode, instead forming the metal in situ during the initial charging (formation) step. In anode-free solid-state batteries, the quality of the interfacial contact is particularly critical, as insufficient contact can lead to locally increased current densities. Consequently, the initial metal plating during the formation step plays a decisive role in determining the homogeneity and stability of the anode interface. Furthermore, conventional battery-grade copper foils (~10 µm) are considerably thicker than required for the targeted C-rates and are difficult to use as stand-alone anode-free current collectors, thereby hindering the industrial production of anode-free solid-state batteries. In this publication, we demonstrate the application of atmospheric plasma spraying (APS) to fabricate thin copper current collectors directly on the ceramic solid electrolytes LAGP (lithium aluminium germanium phosphate) and BASE (beta-alumina solid electrolyte) with superior interface contact. No mechanical damage or diffusion of copper into the solid electrolyte nor formation of secondary phases at the interfaces were observed in SEM or EDS despite the elevated process temperature. LAGP with a thickness as low as 300 µm was successfully coated and subsequently used for plating/stripping experiments. Finally, dense sodium metal was plated at the copper-substrate interface of a 1.4 mm thick BASE sample.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Thermal Expansion and Ionic Conductivity

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Fraunhofer Institute for Ceramic Technologies and Systems (IKTS), Äußere Nürnberger Str. 62, 91301 Forchheim, Germany

Friedrich-Alexander-Universität Erlangen-Nürnberg, Fürther Straße 246b, 90429 Nürnberg, Germany

Institut für Nanotechnologie und Korrelative Mikroskopie gGmbH (INAM), Äußere Nürnberger Str. 62, 91301 Forchheim, Germany

Fraunhofer Institute for Ceramic Technologies and Systems (IKTS), Michael-Faraday-Straße 1, 07629 Hermsdorf, Germany

Powerlyze GmbH, Fürther Straße 246b, 90429 Nürnberg, Germany

Funding

Federal Ministry of Research, Technology and Space—BMFTR · Federal Ministry for Economic Affairs and Energy

References (41)

Show source-provided references
1. Toward a Fundamental Understanding of the Lithium Metal Anode in Solid-State Batteries—An Electrochemo-Mechanical Study on the Garnet-Type Solid Electrolyte Li6.25Al0.25La3Zr2O1210.1021/acsami.9b02537 ↗
2. Emerging processing guidelines for solid electrolytes in the era of oxide-based solid-state batteries10.1039/D5CS00358J ↗
3. Enhanced stability and high rate capability of garnet solid-state electrolyte interface through integration of nanoscale Li4Ti5O12 for Li battery applications10.1016/j.jpowsour.2025.237593 ↗
4. High plating currents without dendrites at the interface between a lithium anode and solid electrolyte10.1038/s41560-025-01847-0 ↗
5. Influence of Microstructure on the Material Properties of LLZO Ceramics Derived by Impedance Spectroscopy and Brick Layer Model Analysis10.1021/acsami.3c10060 ↗
6. Guidelines for Impedance Analysis of Parent Metal Anodes in Solid-State Batteries and the Role of Current Constriction at Interface Voids, Heterogeneities, and SEI10.1002/admi.202202354 ↗
7. Extreme lithium-metal cycling enabled by a mixed ion- and electron-conducting garnet three-dimensional architecture10.1038/s41563-023-01627-9 ↗
8. Lithium-Metal Growth Kinetics on LLZO Garnet-Type Solid Electrolytes10.1016/j.joule.2019.06.013 ↗
9. Pressure-Driven Interface Evolution in Solid-State Lithium Metal Batteries10.1016/j.xcrp.2019.100012 ↗
10. Negating interfacial impedance in garnet-based solid-state Li metal batteries10.1038/nmat4821 ↗
11. A 3D Cross-Linking Lithiophilic and Electronically Insulating Interfacial Engineering for Garnet-Type Solid-State Lithium Batteries10.1002/adfm.202007815 ↗
12. A perspective on the design, manufacturing, and energy content of oxide all-solid-state batteries with scaffold-based composite cathodes10.1016/j.jpowsour.2024.234091 ↗
13. Critical Current Density in Solid-State Lithium Metal Batteries: Mechanism, Influences, and Strategies10.1002/adfm.202009925 ↗
14. Stabilizing the Interface of NASICON Solid Electrolyte against Li Metal with Atomic Layer Deposition10.1021/acsami.8b06366 ↗
15. Deposition of Sodium Metal at the Copper-NaSICON Interface for Reservoir-Free Solid-State Sodium Batteries10.1002/aenm.202302729 ↗
16. Enabling “Sodium-Metal-Free” Manufacturing of Solid-State Batteries10.1021/acsenergylett.4c01724 ↗
17. Sputtered Zero-Excess Electrodes with Metallic Seed Layers for Solid-State Sodium Batteries10.1002/batt.202400364 ↗
18. From High- to Low-Temperature: The Revival of Sodium-Beta Alumina for Sodium Solid-State Batteries10.1002/batt.202100131 ↗
19. Dirksen, C.L., Skadell, K., Schulz, M., Fertig, M.P., and Stelter, M. (2021). Influence of 3d transition metal doping on lithium stabilized na-β″-alumina solid electrolytes. Materials, 14.10.3390/ma14185389 ↗
20. Hensel, A., Schwarzer, C., Scheetz, M., Kaloudis, M., and Franke, J. (2018, January 4–7). Investigations of silver sintered interconnections 3-dimensional ceramics with plasma based additive copper metallizations. Proceedings of the 2018 IEEE 20th Electronics Packaging Technology Conference, Singapore.10.1109/EPTC.2018.8654421 ↗
21. Ockel, M., Borchers, A., Frohlich, J., Petersen, M., Paschen, T., Christiansen, S., and Franke, J. (2024, January 5–6). Atmospheric Plasma Spraying for Copper Coating of Ceramic Solid Electrolytes for Anode-Free Solid-State Batteries with Increased Interfacial Contact. Proceedings of the 2024 1st International Conference on Production Technologies and Systems for E-Mobility, Bamberg, Germany.10.1109/EPTS61482.2024.10586742 ↗
22. Microstructures and key properties of cold-sprayed and thermally sprayed copper coatings10.1016/j.surfcoat.2005.05.011 ↗
23. Schwarzer, C., Hensel, A., Roth, F., Franke, J., and Kaloudis, M. (, January June). Investigation of Pressureless Sintered Interconnections on Plasma Based Additive Copper Metallization. Proceedings of the 2020 IEEE 70th Electronic Components and Technology Conference, Orlando, FL, USA.
24. Gökçen, A., Ockel, M., Petersen, M., Thielen, N., Franke, J., and Risch, F. (2025, January 5–8). Optimizing Thin Electric Functional Copper Coatings via Atmospheric Plasma Spray. Proceedings of the International Thermal Spray Conference, Vancouver, BC, Canada.10.31399/asm.cp.itsc2025p0192 ↗
25. Critical Role of Pressure for Chemo-Mechanical-Induced Stability of Sodium Metal Battery Anodes10.1021/acsenergylett.3c00734 ↗
26. High Coulombic Efficiency Plating and Stripping of Sodium for Reservoir-Free Solid-State Batteries at Low Stack Pressure10.1021/acsenergylett.5c01680 ↗
27. Imaging the microstructure of lithium and sodium metal in anode-free solid-state batteries using electron backscatter diffraction10.1038/s41563-024-02006-8 ↗
28. Understanding Li Plating and Stripping Behavior in Zero-Excess Li Metal Batteries Using Operando Dilatometry10.1149/1945-7111/ac5cf1 ↗
29. Influence of contouring the lithium metal/solid electrolyte interface on the critical current for dendrites10.1039/D3EE03322H ↗
30. Analysis of microstructural effects on mechanical properties of copper alloys10.1016/j.jsamd.2016.12.003 ↗
31. Copper Current Collector: The Cornerstones of Practical Lithium Metal and Anode–Free Batteries10.1002/cphc.202400007 ↗
32. Preparing ultra-thin copper foil as current collector for improving the LIBs performances with reduced carbon footprint10.1016/j.mtcomm.2023.105952 ↗
33. Fabricating ultralight and ultrathin copper current collectors for high-energy batteries10.1016/j.esci.2024.100271 ↗
34. Ultralight and fire-extinguishing current collectors for high-energy and high-safety lithium-ion batteries10.1038/s41560-020-00702-8 ↗
35. Reducing the thickness of solid-state electrolyte membranes for high-energy lithium batteries10.1039/D0EE02241A ↗
36. Understanding key limiting factors for the development of all-solid-state-batteries10.1016/j.ceja.2022.100436 ↗
37. High-rate cycling in 3D dual-doped NASICON architectures toward room-temperature sodium-metal-anode solid-state batteries10.1039/D3EE03879C ↗
38. Fast Charging and Low Temperature Capabilities of Sodium Solid-State Batteries Enabled by Thin NASICON Bilayer Architecture10.1021/acsenergylett.5c00575 ↗
39. Spraying Li6PS5Cl and silver-carbon multilayers to facilitate large-scale fabrication of all-solid-state batteries10.1016/j.device.2024.100468 ↗
40. Lithium All-Solid-State Batteries Fabricated at Room Temperature by the Powder Aerosol Deposition Method with Garnet-Type Electrolyte and Graded Composite Cathode10.1002/admt.202400745 ↗
41. Plasma Spray Deposition of Na3Zr2Si2PO12 Electrolyte for High-Performance All-Solid-State Sodium-Ion Battery10.1007/s11666-025-01928-2 ↗