journal article·2019-06-14Open access

Luminescence of Tb3Al5O12 phosphors co-doped with Ce3+/Gd3+ for white light-emitting diodes

Yu-Guo Yang, Lei Wei, Jian-Hua Xu, Hua-Jian Yu, Yan-Yan Hu, Hua-Di Zhang, Xu-Ping Wang, Bing Liu, Cong Zhang, Qing-Gang Li

Abstract

Tb2.96−xCe0.04GdxAl5O12 phosphors were synthesized through solid-state reactions. The influence of Gd3+ on the luminescence was investigated. Under the excitation at 460 nm, Tb2.96Ce0.04Al5O12 shows the characteristic emission band of Ce3+ with a peak wavelength at about 554 nm. After co-doping Gd3+ into Tb2.96Ce0.04Al5O12, the peak wavelength of the Ce3+ emission band shifts to longer wavelengths, which is induced by the increasing crystal field splitting. However, the Ce3+ emission intensity also decreases because the substitution of Tb3+ with Gd3+ causes lattice deformation and generates numerous structural and chemical defects. By comparing the light parameters of white light-emitting diodes (WLEDs) containing Y2.96Ce0.04Al5O12, Tb2.96Ce0.04Al5O12 and Tb2.81Ce0.04Gd0.15Al5O12 phosphors, we can find that the WLED containing the Tb2.81Ce0.04Gd0.15Al5O12 phosphor generates warmer light than the WLEDs containing Y2.96Ce0.04Al5O12 and Tb2.96Ce0.04Al5O12 phosphors. Moreover, the WLEDs fabricated by integrating a blue LED chip and Ce3+/Gd3+-co-doped Tb3Al5O12 phosphors show outstanding colour stability when driven under different currents.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Luminescence Properties of Advanced Materials · Radiation Detection and Scintillator Technologies · Perovskite Materials and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. 10.1109/lpt.2002.80585210.1109/lpt.2002.805852 ↗
2. 10.1016/j.cplett.2017.07.04210.1016/j.cplett.2017.07.042 ↗
3. 10.1038/nmat401210.1038/nmat4012 ↗
4. 10.1111/j.1551-2916.2009.03574.x10.1111/j.1551-2916.2009.03574.x ↗
5. 10.1007/s10854-018-8820-y10.1007/s10854-018-8820-y ↗
6. 10.1166/nnl.2013.168710.1166/nnl.2013.1687 ↗
7. 10.1016/j.mseb.2013.03.01710.1016/j.mseb.2013.03.017 ↗
8. 10.1142/s179329201450008810.1142/s1793292014500088 ↗
9. 10.1039/c4tc00031e10.1039/c4tc00031e ↗
10. 10.1039/c6tc02695h10.1039/c6tc02695h ↗
11. 10.1039/c5tc04133c10.1039/c5tc04133c ↗
12. 10.1039/c7tc02514a10.1039/c7tc02514a ↗
13. 10.1364/ome.7.00045410.1364/ome.7.000454 ↗
14. 10.1007/s10854-017-7323-610.1007/s10854-017-7323-6 ↗
15. 10.1016/j.jlumin.2018.03.05810.1016/j.jlumin.2018.03.058 ↗
16. 10.1021/cm801732d10.1021/cm801732d ↗
17. 10.1016/j.jallcom.2017.08.02310.1016/j.jallcom.2017.08.023 ↗
18. 10.1149/1.336722410.1149/1.3367224 ↗
19. 10.1021/ic501063j10.1021/ic501063j ↗
20. 10.1016/j.materresbull.2017.10.01910.1016/j.materresbull.2017.10.019 ↗
21. 10.1080/17458080.2011.55958910.1080/17458080.2011.559589 ↗
22. 10.1038/srep1151410.1038/srep11514 ↗
23. 10.1016/j.molstruc.2017.09.03710.1016/j.molstruc.2017.09.037 ↗
24. 10.1016/j.jlumin.2017.07.05610.1016/j.jlumin.2017.07.056 ↗
25. 10.1016/j.mseb.2011.10.00510.1016/j.mseb.2011.10.005 ↗
26. 10.1016/j.optmat.2007.07.00510.1016/j.optmat.2007.07.005 ↗
27. 10.1016/j.jlumin.2018.01.04310.1016/j.jlumin.2018.01.043 ↗
28. 10.1016/j.ceramint.2018.02.10410.1016/j.ceramint.2018.02.104 ↗
29. 10.1134/s0030400x0903010210.1134/s0030400x09030102 ↗
30. Robertson · Philips Journal of Research · 1981 · 36 · 15
31. 10.1016/j.jlumin.2018.11.05710.1016/j.jlumin.2018.11.057 ↗
32. 10.1039/c6tc02763f10.1039/c6tc02763f ↗
33. 10.1039/c5dt04909a10.1039/c5dt04909a ↗