Effect of current density on the microstructure and corrosion resistance of microarc oxidized ZK60 magnesium alloy
Source abstract
Abstract
The application of magnesium alloys as biomaterials is limited by their poor corrosion behavior. Microarc oxidation (MAO) treatment was used to prepare ceramic coatings on ZK60 magnesium alloys in order to overcome the poor corrosion resistance. The process was conducted at different current densities (3.5 and 9.0 A/dm2), and the effect of current density on the process was studied. The microstructure, elemental distribution, and phase composition of the MAO coatings were characterized by scanning electron microscopy, energy-dispersive x-ray spectrometry, and x-ray diffraction, respectively. The increment of current density contributes to the increase of thickness. A new phase Mg2SiO4 was detected as the current density increased to 9.0 A/dm2. A homogeneous distribution of micropores could be observed in the coating produced at 3.5 A/dm2, while the surface morphology of the coating formed at 9.0 A/dm2 was more rough and apparent microcracks could be observed. The coating obtained at 3.5 A/dm2 possessed a better anticorrosion behavior.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Shandong University Key Laboratory for Liquid-Solid Structural Evolution and Processing of Materials, Ministry of Education, School of Materials Science and Engineering, , Ji'nan 250061, Shandong, People's Republic of China
Shandong University Key Laboratory of High-Efficiency and Clean Mechanical Manufacture (Shandong University), Ministry of Education, School of Mechanical Engineering, , Ji'nan 250061, Shandong, People's Republic of China
References (32)
Show source-provided references
1. Mater. Sci. Eng., A · 2001 · 302 · 3710.1016/S0921-5093(00)01351-4 ↗
2. Surf. Coat. Technol. · 2010 · 205 · S18210.1016/j.surfcoat.2010.07.045 ↗
3. Adv. Eng. Mater. · 2003 · 5 · 83710.1002/adem.200310405 ↗
4. J. Magn. Alloys · 2013 · 1 · 17710.1016/j.jma.2013.09.003 ↗
5. Acta Biomater. · 2012 · 8 · 244210.1016/j.actbio.2012.04.012 ↗
6. Corros. Sci. · 2006 · 48 · 353110.1016/j.corsci.2006.02.008 ↗
7. Surf. Coat. Technol. · 2006 · 201 · 49210.1016/j.surfcoat.2005.11.081 ↗
8. Corros. Sci. · 2005 · 47 · 276010.1016/j.corsci.2004.11.004 ↗
9. Appl. Surf. Sci. · 2007 · 253 · 449010.1016/j.apsusc.2006.09.064 ↗
10. Trans. Nonferrous Met. Soc. China · 2011 · 21 · 30710.1016/S1003-6326(11)60714-0 ↗
11. Mater. Chem. Phys. · 2008 · 107 · 35610.1016/j.matchemphys.2007.07.027 ↗
12. Appl. Surf. Sci. · 2012 · 261 · 77410.1016/j.apsusc.2012.08.099 ↗
13. J. Mater. Sci. · 2012 · 47 · 519710.1007/s10853-012-6403-5 ↗
14. Acta Biomater. · 2011 · 7 · 188010.1016/j.actbio.2010.11.034 ↗
15. Appl. Surf. Sci. · 2012 · 258 · 611610.1016/j.apsusc.2012.03.016 ↗
16. J. Alloys Compd. · 2012 · 543 · 10910.1016/j.jallcom.2012.07.130 ↗
17. Surf. Coat. Technol. · 2010 · 205 · 178910.1016/j.surfcoat.2010.05.016 ↗
18. Appl. Surf. Sci. · 2010 · 256 · 401710.1016/j.apsusc.2010.01.069 ↗
19. Appl. Surf. Sci. · 2010 · 256 · 392810.1016/j.apsusc.2010.01.052 ↗
20. Corros. Sci. · 2013 · 73 · 18810.1016/j.corsci.2013.03.035 ↗
21. Appl. Surf. Sci. · 2007 · 253 · 693910.1016/j.apsusc.2007.02.010 ↗
22. Curr. Appl. Phys. · 2009 · 9 · 12610.1016/j.cap.2007.12.007 ↗
23. Mater. Chem. Phys. · 2005 · 90 · 12810.1016/j.matchemphys.2004.10.025 ↗
24. Surf. Coat. Technol. · 2010 · 205 · S3210.1016/j.surfcoat.2010.03.032 ↗
25. Electrochim. Acta · 2007 · 53 · 41710.1016/j.electacta.2007.04.030 ↗
26. Electrochem. Soc. · 1999 · 146 · 175710.1149/1.1391838 ↗
27. Appl. Surf. Sci. · 2012 · 259 · 36210.1016/j.apsusc.2012.07.052 ↗
28. J. Alloys Compd. · 2009 · 480 · 46910.1016/j.jallcom.2009.01.102 ↗
29. Electrochim. Acta · 2009 · 54 · 384210.1016/j.electacta.2009.02.004 ↗
30. Appl. Surf. Sci. · 2009 · 255 · 421210.1016/j.apsusc.2008.11.008 ↗
31. Corros. Sci. · 2006 · 48 · 193910.1016/j.corsci.2005.08.004 ↗
32. Corros. Sci. · 2010 · 52 · 57910.1016/j.corsci.2009.10.016 ↗