In vitro and in vivo studies on the degradation of high-purity Mg (99.99wt.%) screw with femoral intracondylar fractured rabbit model
Source abstract
Abstract
High-purity magnesium (HP Mg) takes advantage in no alloying toxic elements and slower degradation rate in lack of second phases and micro-galvanic corrosion. In this study, as rolled HP Mg was fabricated into screws and went through in vitro immersion tests, cytotoxicity test and bioactive analysis. The HP Mg screws performed uniform corrosion behavior in vitro, and its extraction promoted cell viability, bone alkaline phosphatase (ALP) activity, and mRNA expression of osteogenic differentiation related gene, i.e. ALP, osteopontin (OPN) and RUNX2 of human bone marrow mesenchymal stem cells (hBMSCs). Then HP Mg screws were implanted in vivo as load-bearing implant to fix bone fracture and subsequently gross observation, range of motion (ROM), X-ray scanning, qualitative micro-computed tomography (μCT) analysis, histological analysis, bending-force test and SEM morphology of retrieved screws were performed respectively at 4, 8, 16 and 24 weeks. As a result, the retrieved HP Mg screws in fixation of rabbit femoral intracondylar fracture showed uniform degradation morphology and enough bending force. However, part of PLLA screws was broken in bolt, although its screw thread was still intact. Good osseointegration was revealed surrounding HP Mg screws and increased bone volume and bone mineral density were detected at fracture gap, indicating the rigid fixation and enhanced fracture healing process provided by HP Mg screws. Consequently, the HP Mg showed great potential as internal fixation devices in intra-articular fracture operation.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Orthopaedic implants and arthroplasty · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. The history of biodegradable magnesium implants: a review10.1016/j.actbio.2010.02.028 ↗
2. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
3. In vivo corrosion of four magnesium alloys and the associated bone response10.1016/j.biomaterials.2004.09.049 ↗
4. In vitro and in vivo corrosion measurements of magnesium alloys10.1016/j.biomaterials.2005.07.037 ↗
5. The in vivo and in vitro corrosion of high-purity magnesium and magnesium alloys WZ21 and AZ9110.1016/j.corsci.2013.06.019 ↗
6. The development of binary Mg-Ca alloys for use as biodegradable materials within bone10.1016/j.biomaterials.2007.12.021 ↗
7. Research on an Mg-Zn alloy as a degradable biomaterial10.1016/j.actbio.2009.06.028 ↗
8. In vitro and in vivo studies on a Mg-Sr binary alloy system developed as a new kind of biodegradable metal10.1016/j.actbio.2012.02.018 ↗
9. Corrosion behaviour of a nominally high purity Mg ingot produced by permanent mould direct chill casting10.1016/j.corsci.2012.04.030 ↗
10. Biodegradable metals10.1016/j.mser.2014.01.001 ↗
11. In vitro degradation and cytotoxicity response of Mg-4% Zn-0.5% Zr (ZK40) alloy as a potential biodegradable material10.1016/j.actbio.2013.07.001 ↗
12. Corrosion fatigue behaviors of two biomedical Mg alloys - AZ91D and WE43-In simulated body fluid10.1016/j.actbio.2010.07.026 ↗
13. Degradable biomaterials based on magnesium corrosion10.1016/j.cossms.2009.04.001 ↗
14. Preparation and assessment of revised simulated body fluids10.1002/jbm.a.10482 ↗
15. Proliferation and osteoblastic differentiation of human bone marrow-derived stromal cells on akermanite-bioactive ceramics10.1016/j.biomaterials.2006.07.027 ↗
16. Intra-articular injection of hyaluronic acid for the reduction in joint adhesion formation in a rabbit model of knee injury10.1007/s00167-013-2547-3 ↗
17. International Cartilage Repair Society (ICRS) and Oswestry macroscopic cartilage evaluation scores validated for use in Autologous Chondrocyte Implantation (ACI) and microfracture10.1016/j.joca.2007.05.005 ↗
18. Long-term in vivo degradation behaviour and biocompatibility of the magnesium alloy ZEK100 for use as a biodegradable bone implant10.1016/j.actbio.2012.08.028 ↗
19. Effect of fracture gap on stability of compression plate fixation: a finite element study10.1002/jor.20990 ↗
20. Bone-implant interface strength and osseointegration: biodegradable magnesium alloy versus standard titanium control10.1016/j.actbio.2010.08.020 ↗
21. Osteogenic evaluation of calcium/magnesium-doped mesoporous silica scaffold with incorporation of rhBMP-2 by synchrotron radiation-based muCT10.1016/j.biomaterials.2011.07.090 ↗
22. Bioactive ceramic coating of cancellous screws improves the osseointegration in the cancellous bone
23. In vivo assessment of the host reactions to the biodegradation of the two novel magnesium alloys ZEK100 and AX30 in an animal model10.1186/1475-925X-11-14 ↗
24. Stress-enhanced ion release–the effect of static loading10.1016/0142-9612(91)90108-M ↗
25. Effect of mechanical stability on fracture healing–an update10.1016/j.injury.2007.02.005 ↗
26. Mechanical stimulation promotes osteogenic differentiation of human bone marrow stromal cells on 3-D partially demineralized bone scaffolds in vitro10.1007/s00223-003-0104-7 ↗
27. In vitro studies of biomedical magnesium alloys in a simulated physiological environment: a review10.1016/j.actbio.2010.12.004 ↗
28. A novel model to study metaphyseal bone healing under defined biomechanical conditions10.1007/s00402-008-0692-9 ↗
29. Magnesium alloys as a biomaterial for degradable craniofacial screws10.1016/j.actbio.2013.12.040 ↗
30. Corrosion of magnesium alloy AZ31 screws is dependent on the implantation site10.1016/j.mseb.2011.02.010 ↗
31. Biomechanical characterisation of a degradable magnesium-based (MgCa0.8) screw10.1007/s10856-011-4544-8 ↗
32. In vitro mechanical integrity of hydroxyapatite coated magnesium alloy10.1088/1748-6041/6/4/045003 ↗
33. The biology of fracture healing10.1016/j.injury.2011.03.031 ↗
34. Loss of mechanical properties in vivo and bone-implant interface strength of AZ31B magnesium alloy screws with Si-containing coating10.1016/j.actbio.2013.12.020 ↗
35. Shape and site dependent in vivo degradation of Mg-Zn pins in rabbit femoral condyle10.3390/ijms15022959 ↗
36. Bone and metal: an orthopaedic perspective on osseointegration of metals10.1016/j.actbio.2014.06.004 ↗
37. Randomized controlled trial of osteoconductive fixation screws for anterior cruciate ligament reconstruction: a comparison of the Calaxo and Milagro screws10.1016/j.arthro.2012.10.021 ↗
38. Biomechanical testing and degradation analysis of MgCa0.8 alloy screws: a comparative in vivo study in rabbits10.1016/j.actbio.2010.10.031 ↗
39. Local release of magnesium from mesoporous TiO2 coatings stimulates the peri-implant expression of osteogenic markers and improves osteoconductivity in vivo10.1016/j.actbio.2014.08.011 ↗
40. Cytocompatibility, degradation, mechanical property retention and ion release profiles for phosphate glass fibre reinforced composite rods10.1016/j.msec.2012.12.089 ↗
41. The effect of loading on peri-implant bone: a critical review of the literature10.1111/joor.12195 ↗
42. Stress shielding and bone resorption in shoulder arthroplasty10.1067/mse.2003.22 ↗
43. Numerical evaluation of reduction of stress shielding in laser coated hip prostheses10.1590/S1516-14392011005000043 ↗
44. A comparison of the results of anterior cruciate ligament reconstruction using bioabsorbable versus metal interference screws: a meta-analysis10.2106/JBJS.J.00269 ↗
45. Bioabsorbable fixation devices in trauma and bone surgery: current clinical standing10.1586/17434440.1.2.229 ↗