journal article·2005-12

Corrosion behavior of titanium in the presence of calcium phosphate and serum proteins

Xiaoliang Cheng, Sharon G. Roscoe

Biomaterials· Volume 26· Issue 35
Publisher page

Abstract

The effect of calcium phosphate surface deposit and the surface adsorption of the serum proteins, bovine serum albumin (BSA) and fibrinogen, on the corrosion resistance and electrochemical behavior of (cp)titanium in phosphate buffer saline solution (pH 7.4) was investigated at physiological temperature, 37 degrees C, using electrochemical impedance spectroscopy and dc electrochemical polarization techniques. The formation of calcium phosphate deposit on the Ti surface decreased both the corrosion rate at the open circuit potential (OCP) and the anodic reaction current in the high anodic potential range (>2.6 V). Addition of BSA significantly moved the OCP towards a more negative (cathodic) potential and inhibited the cathodic corrosion reaction, but did not significantly change the corrosion resistance at the OCP. Addition of fibrinogen showed a similar, but less pronounced effect than BSA. The possible mechanisms leading to these observed effects are discussed.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. In vitro human monocyte response to wear particles of titanium alloy containing vanadium or niobium10.1302/0301-620X.79B2.0790311 ↗
2. Characterization of implant materials in fetal bovine serum and sodium sulfate by electrochemical impedance spectroscopy. I. Mechanically polished samples10.1002/jbm.10329 ↗
3. Study of the corrosion behavior of titanium and some of its alloys for biomedical and dental implant applications10.1016/S0022-0728(99)00260-0 ↗
4. Modifying the properties of titanium surface with the aim of improving its bioactivity and corrosion resistance10.1016/S0924-0136(03)00398-4 ↗
5. In vitro corrosion resistance of titanium made using different fabrication methods10.1016/S0142-9612(98)00160-4 ↗
6. Electrochemical characterization of cast titanium alloys10.1016/S0142-9612(02)00293-4 ↗
7. Measurement and evaluation of galvanic corrosion between titanium/Ti6Al4V implants and dental alloys by electrochemical techniques and auger spectrometry10.1016/S0142-9612(98)00248-8 ↗
8. Surface oxide films on titanium alloys regenerated in Hanks’ solution10.2320/matertrans.43.3000 ↗
9. In-vitro corrosion and wear of titanium alloys in the biological environment10.1016/0142-9612(96)00029-4 ↗
10. Characterisation of a duplex TiO2/CaP coating on Ti6Al4V for hard tissue replacement10.1016/j.biomaterials.2004.04.022 ↗
11. Corrosion resistance of implant alloys in pseudo physiological solution and role of alloying elements in passive films10.2320/matertrans1989.38.78 ↗
12. Interactions between calcium, phosphate, and albumin on the surface of titanium10.1002/1097-4636(200104)55:1<45::AID-JBM70>3.0.CO;2-0 ↗
13. Preparation of calcium phosphate coatings on titanium implant materials by simple chemistry10.1002/(SICI)1097-4636(199808)41:2<227::AID-JBM7>3.0.CO;2-K ↗
14. An in vitro study of Ti- and Ti-alloys coated with sol–gel derived hydroxyapatite coatings10.1016/S0257-8972(02)00732-6 ↗
15. The electrochemical behavior of Ti–6Al–7Nb alloy with and without plasma-sprayed hydroxyapatite coating in Hank's solution10.1002/jbm.10351 ↗
16. In vitro corrosion behavior of bioceramic, metallic, and bioceramic-metallic coated stainless steel dental implants10.1016/S0109-5641(02)00029-5 ↗
17. Corrosion resistance of titanium CP in saline physiological solutions with calcium phosphate and proteins10.1016/0267-6605(93)90015-Y ↗
18. The corrosion behavior of Ti–6Al–4V, Ti–6Al–7Nb and Ti–13Nb–13Zr in protein solutions10.1016/S0142-9612(98)00217-8 ↗
19. Conjoint corrosion and wear of titanium alloys10.1016/S0142-9612(98)00229-4 ↗
20. The effects of proteins on metallic corrosion10.1002/jbm.820160205 ↗
21. Effect of fluoride and albumin concentration on the corrosion behavior of Ti6Al4V alloy10.1016/S0142-9612(02)00315-0 ↗
22. The influence of albumin on corrosion resistance of titanium in fluoride solution10.4012/dmj.22.359 ↗
23. Corrosion behavior and surface characterization of titanium in solution containing fluoride and albumin10.1016/j.biomaterials.2004.03.025 ↗
24. Electrochemical studies on the influence of proteins on the corrosion of implant alloys10.1016/0142-9612(88)90119-6 ↗
25. Electrochemical studies of the adsorption behavior of Bovine Serum Albumin on stainless steel10.1021/la990474f ↗
26. Electrochemical corrosion in saline and serum, Journal of Biomedical Materials Research10.1002/jbm.820140208 ↗
27. Isolation of serum-protein organometallic corrosion products from 316ss and HS-21 invitro and invivo10.1002/jbm.820180110 ↗
28. Interfacial behavior of beta-lactoglobulin at a stainless steel surface: An electrochemical impedance spectroscopy study10.1006/jcis.2000.6913 ↗
29. Electrochemical studies of the adsorption behavior of serum proteins on titanium10.1021/la991497x ↗
30. Electrochemical and XPS studies of titanium for biomaterial applications with respect to the effect of hydrogen peroxide10.1002/jbm.820280115 ↗
31. Electrochemical studies on the stability and corrosion resistance of titanium-based implant materials10.1016/S0142-9612(00)00309-4 ↗
32. Electrochemical characterization of passive films on Ti alloys under simulated biological conditions10.1016/S0013-4686(02)00029-4 ↗
33. EIS characterization of a Ti-dental implant in artificial saliva media: dissolution process of the oxide barrier10.1016/j.jelechem.2004.01.011 ↗
34. Passive dissolution kinetics of titanium in vitro10.1007/BF00120380 ↗
35. Structure and composition of passive titanium oxide films10.1016/S0921-5107(97)00043-3 ↗
36. Hydrogen evolution and oxygen reduction at a titanium sonotrode10.1039/a800801i ↗
37. The passivity and breakdown of beryllium in aqueous solutions10.1149/1.1838717 ↗