Use of vitamin E to protect cross-linked UHMWPE from oxidation
Source abstract
Abstract
Wear and oxidative degradation may limit the life span of UHMWPE implants. Cross-linking and stabilisation by vitamin E are proposed to overcome wear and degradation. The present investigation takes a close look to the oxidative behaviour of cross-linked and stabilised UHMWPE. First, the consolidated vitamin E stabilised UHMWPE was qualified in terms of microstructure and homogeneity of the distribution of the additive to be suitable for oxidation profiles over the entire section. Then cross-linked samples with five different concentrations of vitamin E (nil to 1.0%) underwent two different ageing protocols. The first was under pressurized oxygen at 70 degrees C, as defined in the ASTM F 2003 standard with a prolonged period of 60 days, the second was in 5% aqueous hydrogen peroxide solution with iron (III) chloride as catalyst at 50 degrees C. The first accelerated ageing protocol showed that a vitamin E concentration as low as 0.05% is effective to protect irradiated highly cross-linked UHMWPE against oxidation when exposed direct to oxygen. Vitamin E stabilised, highly cross-linked UHMWPE exhibits therefore no oxidation potential origination from the irradiation treatment. Analysis of samples treated by the second chemical ageing yielded, that vitamin E is effective to prolong initial stability against a supplementary attack of hydrogen peroxide and reactive radicals. The time period of stability against the aggressive hydrogen peroxide solution increases with increasing vitamin E content. However, even 0.05% have a marked stabilisation effect. Therefore, such small additions of vitamin E are effective to protect the UHMWPE material against a supplementary exposure to in vivo oxidation after the irradiation treatment. In conclusion, vitamin E shields cross-linked UHMWPE for orthopaedic application against oxidation in the heat of consolidation, during irradiation treatment and finally while implanted in the human body.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Total Knee Arthroplasty Outcomes · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Osteolysis in alloarthroplasty of the hip. The role of ultra-high molecular weight polyethylene wear particles10.1097/00003086-199009000-00013 ↗
2. A literature review of the association between wear rate and osteolysis in total hip arthroplasty10.1054/arth.2002.33664 ↗
3. In vivo UHMWPE biodegradation of retrieved prosthesis10.1016/S0142-9612(98)00013-1 ↗
4. Vitamin E blended UHMWPE biomaterials
5. The effects of high dose irradiation on cross-linking of vitamin E-blended UHMWPE10.1016/j.biomaterials.2008.05.004 ↗
6. A second generation highly cross-linked UHMWPE: vitamin E stabilisation does not adversely affect the wear rate of irradiated acetabular liners
7. The effect of irradiation, annealing temperature and artificial aging on the oxidation, mechanical properties and fractures mechanisms of UHMWPE10.1002/jbm.a.10090 ↗
8. Luisetto Y. Degradation mechanism and effects of vitamin E addition in UHMWPE hip implants. Ph.D. thesis, Lund University, Lund/Sweden; 2003.
9. Trace concentrations of vitamin E protects radiation crosslinked UHMWPE from oxidative degradation10.1002/jbm.a.32122 ↗
10. Accelerated ageing experiments with crosslinked and conventional UHMWPE stabilised with alpha-tocopherol for total joint arthroplasty10.1007/s10856-006-0608-6 ↗
11. Lidgren L, Bengtsson P, Sjövall P, Wesslen B. A method for the preparation of UHMWPE doped with an antioxidant and an implant made thereof. Eur Patent EP1161489B1; 2004.
12. Accelerated aging studies of UHMWPE. II. Virgin UHMWPE is not immune to oxidative degeneration10.1002/jbm.10136 ↗
13. Wear resistance and mechanical properties of highly cross-linked, UHMWPE doped With Vitamin E10.1016/j.arth.2005.07.009 ↗
14. Ticona GmbH Kelsterbach/Germany · 2009
15. Property changes of UHMWPE hip cup endoprostheses during implantation10.1002/jbm.820180915 ↗
16. Gamma sterilisation of UHMWPE articular implants: an analysis of the oxidation problem10.1016/0142-9612(95)00349-5 ↗
17. Can accelerated aqueous aging simulate in vivo oxidation of gamma-sterilized UHMWPE?10.1002/jbm.b.30514 ↗
18. Significance of in vivo degradation for polyethylene in total hip arthroplasty10.1097/01.blo.0000246547.18187.0b ↗