Degradation of mechanical behavior in UHMWPE after natural and accelerated aging
Source abstract
Abstract
Ultra-high molecular weight polyethylene (UHMWPE) is known to degrade during natural (shelf) aging following gamma irradiation in air, but the mechanical signature of degradation remains poorly understood. Accelerated aging methods have been developed to reproduce the natural aging process as well as to precondition total joint replacement components prior to joint simulator wear testing. In this study, we compared the mechanical behavior of naturally (shelf) aged and accelerated aged tibial inserts using a previously validated miniature specimen testing technique known as the small punch test. Tibial inserts made-of GUR 1120 and sterilized with 25 to 40 kGy of gamma radiation (in air) in 1988, 1993, and 1997 were obtained; a subset of the 1997 implants were subjected to 4 weeks of accelerated aging in air at 80 degrees C. To determine the spatial variation of mechanical properties within each insert, miniature disk shaped specimens were machined from the surface and subsurface regions of the inserts. Analysis of variance of the test data showed that aging significantly affected the small punch test measures of elastic modulus, initial load, ultimate load, ultimate displacement, and work to failure. The accelerated aging protocol was unable to reproduce the spatial mechanical profile seen in shelf aged components, but it did mechanically degrade the surface of GUR 1120 tibial components to an extent comparable to that seen after 10 years of natural aging. Test specimens showed a fracture morphology consistent with the decreased ductility and toughness which was corroborated by the small punch test metrics of this study. Our data support the hypothesis that UHMWPE undergoes a spatially nonuniform change towards a less ductile (more brittle) mechanical behavior after gamma irradiation in air and shelf aging.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Advanced materials and composites · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Advances in the processing, sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty10.1016/S0142-9612(99)00053-8 ↗
2. Gamma sterilization of UHMWPE articular implants10.1016/0142-9612(95)00349-5 ↗
3. Sanford WM, Saum KA. Accelerated oxidative aging testing of UHMWPE. Presented at the Annual Meeting of the Transactions of the 41st Orthopedic Research Society, Orlando, FL, February 13–16, 1995.
4. McKellop H, Yeom B, Sun DC, Sanford WM. Accelerated aging of irradiated UHMW polyethylene for wear evaluations. Presented at the Annual Meeting of the 42nd Orthopedic Research Society, Atlanta, GA, February 19–22, 1996.
5. Development of an accelerated aging method for evaluation of long-term irradiation effects on UHMWPE implants
6. Di Maio WG, Lilly WB, Moore WC, Saum KA. Low wear, low oxidation radiation crosslinked UHMWPE. Presented at the annual Meeting of the Transactions of the 44th Orthopedic Research Society, New Orleans, LA, February 21–24, 1998.
7. Sun DC, Wang A, Stark C, Dumbleton JH. The concept of stabilization in UHMWPE. Presented at the annual Meeting of the Transactions of the Fifth World Biomaterials Congress, San Francisco, CA, March 18–22, 1996.
8. Study of fatigue resistance of chemical and radiation crosslinked medical grade ultrahigh molecular weight polyethylene10.1002/(SICI)1097-4636(19990915)46:4<573::AID-JBM16>3.0.CO;2-A ↗
9. Greer KW, Schmidt MB, Hamilton JV. The hip simulator wear of gamma-vacuum, gamma-air, and ethylene oxide sterilized UHMWPE following a severe oxidative challenge. Presented at the Annual Meeting of the Transactions of the 44th Orthopedic Research Society, New Orleans, LA, February 21–24, 1998.
10. Sanford WM, Moore WC, McNulty D, Frisinger C, Schmalzried TP. Hip simulator study of the effect of sterilization and oxidation on UHMWPE wear. Presented at the Annual Meeting of the Transactions of the 43rd Orthopedic Research Society, San Francisco, CA, February 9–13, 1997.
11. Sun DC, Scmidig G, Stark C, Dumbleton JH. A simple accelerated aging method for simulations of long-term oxidative aging effects in UHMWPE implants. Presented at the Annual Meeting of the Transactions of the 42nd Orthopedic Research Society, Atlanta, GA, February 19–22, 1996.
12. Evolution of morphology in UHMWPE following accelerated aging10.1002/(SICI)1097-4636(199907)46:1<112::AID-JBM13>3.0.CO;2-U ↗
13. Plasticity-induced damage layer is a precursor to wear in radiation-crosslinked UHMWPE acetabular components for total hip replacement10.1016/S0883-5403(99)90086-4 ↗
14. Edidin AA, Kurtz SM. The influence of mechanical behavior on the wear of four clinically relevant polymeric biomaterials in a hip simulator. J Arthroplasty, 2000;15:in press.10.1016/S0883-5403(00)90647-8 ↗
15. Validation of a small punch testing technique to characterize the mechanical behavior of ultra-high molecular weight polyethylene10.1016/S0142-9612(97)00124-5 ↗
16. Kurtz SM, Jewett CW, Foulds JR, Edidin AA. A miniature-specimen mechanical testing technique scaled to the articulating surface of polyethylene components for total joint arthroplasty. J Biomed Mater Res (Appl Biomater) 1999;48:75–81.10.1002/(SICI)1097-4636(1999)48:1<75::AID-JBM13>3.0.CO;2-H ↗
17. Impact of gamma sterilization on clinical performance of polyethylene in the hip
18. Effects of sterilization on wear in total knee arthroplasty10.1097/00003086-199610000-00023 ↗
19. Impact of gamma sterilization on clinical performance of polyethylene in the knee10.1016/S0883-5403(96)80026-X ↗
20. An analysis of Hylamer and polyethylene bearings from retrieved acetabular components10.3928/0147-7447-19980801-09 ↗
21. Radiation and peroxide crosslinking promote strain hardening behavior and molecular alignment in UHMWPE during multiaxial loading conditions10.1016/S0142-9612(99)00038-1 ↗
22. The natural history of ultra high molecular weight polyethylene
23. Degradation rate of ultra-high molecular weight polyethylene10.1002/jor.1100150109 ↗
24. The relationship between the clinical performance and large deformation mechanical behavior of retrieved UHMWPE tibial inserts10.1016/S0142-9612(99)00178-7 ↗
25. Wunderlich B. Cormier CM. Heat of fusion of polyethylene. J Polymer Sci Part A-2 1967;5:987-988.10.1002/pol.1967.160050514 ↗
26. Kurtz SM, Muratoglu OK, Mounib L, Currier B, Gsell R, Hastings B, Shen F, Yau S-S, Urian C. Interlaboratory validation of a standard for determining the oxidation index of UHMWPE. Presented at the Annual Meeting of the Transactions of the 45th Orthopedic Research Society, Anaheim, CA, February 9–13, 1999.
27. Effect of radiation sterilization and aging on ultrahigh molecular weight polyethylene10.1002/jbm.820150209 ↗
28. Analysis of retrieved implants10.1002/jbm.820160408 ↗
29. Property changes of UHMW polyethylene hip cup endoprostheses during implantation10.1002/jbm.820180915 ↗
30. Radiation-induced crystallinity changes in linear polyethylene10.1002/app.1983.070280236 ↗
31. Radiation-induced crystallinity changes in linear polyethylene10.1080/00222349008212332 ↗
32. Radiation-induced crystallinity changes in polyethylene blends10.1007/BF00553046 ↗
33. Radiation sterilization and the wear rate of polyethylene10.1002/jor.1100020412 ↗
34. Post-irradiation aging of ultra-high molecular weight polyethylene10.2106/00004623-199407000-00014 ↗
35. Exponential model for the tensile true stress-strain behavior of as-irradiated and oxidatively degraded ultra high molecular weight polyethylene10.1002/jor.1100140512 ↗
36. A predictive model for the tensile true stress-strain behavior of chemically and mechanically degraded ultra-high molecular weight polyethylene10.1002/(SICI)1097-4636(199823)43:3<241::AID-JBM4>3.0.CO;2-N ↗
37. Martell JM. Personal Communication, September 1999.