Abstract
To prolong the life of total joint replacements, highly crosslinked ultra-high molecular weight polyethylenes (UHMWPEs) have been introduced to improve the wear resistance of the articulating surfaces. However, there are concerns regarding the loss of ductility and potential loss in fatigue crack propagation (FCP) resistance. The objective of this study was to evaluate the effects of gamma radiation-induced crosslinking with two different post-irradiation thermal treatments on the FCP resistance of UHMWPE. Two highly crosslinked and one virgin UHMWPE treatment groups (ram-extruded, orthopedic grade, GUR 1050) were examined. For the two highly crosslinked treatment groups, UHMWPE rods were exposed to 100 kGy and then underwent post-irradiation thermal processing either above the melt temperature or below the melt temperature (2 h-150 degrees C, 110 degrees C). Compact tension specimens were cyclically loaded to failure and the fatigue crack growth rate, da/dN, vs. cyclic stress intensity factor, DeltaK, behavior was determined and compared between groups. Scanning electron microscopy was used to examine fracture surface characteristics. Crosslinking was found to decrease the ability of UHMWPE to resist crack inception and propagation under cyclic loading. The findings also suggested that annealing as a post-irradiation treatment may be somewhat less detrimental to FCP resistance of UHMWPE than remelting. Scanning electron microscopy examination of the fracture surfaces demonstrated that the virgin treatment group failed in a more ductile manner than the two highly crosslinked treatment groups.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Advanced materials and composites · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Advances in the processing, sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty10.1016/S0142-9612(99)00053-8 ↗
2. Alternative bearing surfaces in hip replacement
3. Thermomechanical behavior of virgin and highly crosslinked ultra-high molecular weight polyethylenes used in total joint replacements10.1016/S0142-9612(02)00102-3 ↗
4. Effect of sterilization method and other modifications on the wear resistance of acetabular cups made of ultra-high molecular weight polyethylene. A hip-simulator study10.2106/00004623-200012000-00004 ↗
5. Duus LC, Walsh HA, Gillis AM, Noisiez E, Li S. A comparison of the fracture toughness of crosslinked UHMWPE made from different resins, manufacturing methods, and sterilization conditions. Transaction on Sixth World Biomaterials Congress, 2000.
6. Development and validation of the small punch test for UHMWPE used in total joint replacements
7. The effects of degree of crosslinking on the fatigue crack initiation and propagation resistance of orthopedic-grade polyethylene10.1002/jbm.a.10606 ↗
8. Gamma irradiation alters fatigue-crack behavior and fracture toughness in 1900H and GUR 1050 UHMWPE10.1002/jbm.10335 ↗
9. ASTM, E 399-Standard Test Method for Plane-Strain Fracture Toughness of Metallic Materials. In: Annual Book of ASTM Standards. 1990.
10. ASTM, E 647-Standard Test Method for Measurement of Fatigue Crack Growth Rates. In: Annual Book of ASTM Standards. 1995.
11. Dowling · 1999
12. A rational analytic theory of fatigue
13. Kleinbaum · 1998
14. Study of fatigue resistance of chemical and radiation crosslinked medical grade ultrahigh molecular weight polyethylene10.1002/(SICI)1097-4636(19990915)46:4<573::AID-JBM16>3.0.CO;2-A ↗
15. Compression and tension fatigue resistance of medical grade ultra high molecular weight polyethylene: the effect of morphology, sterilization, aging, and temperature10.1016/S0032-3861(99)00199-8 ↗
16. Fatigue crack propagation behavior of ultrahigh molecular weight polyethylene10.1002/jor.1100020202 ↗
17. Review: structure and plastic deformation of polyethylene10.1007/BF01162485 ↗
18. Rimnac · 1989
19. Fatigue crack propagation resistance of highly crosslinked polyethylene10.1097/01.blo.0000150124.34906.34 ↗
20. Time resolved simultaneous small- and wide-angle X-ray scattering during polyethylene deformation-II. Cold drawing of linear polyethylene10.1016/S0032-3861(97)00226-7 ↗
21. Bhattacharyya · 2004
22. Failure micromechanisms during uniaxial tensile fracture of conventional and highly crosslinked ultra-high molecular weight polyethylenes used in total joint replacements10.1016/S0142-9612(03)00277-1 ↗