Fatigue and cyclic deformation behaviour of surface-modified titanium alloys in simulated physiological media
Source abstract
Abstract
In this investigation, the cyclic deformation behaviour of the binary titanium alloys Ti-6Al-4V and Ti-6Al-7Nb was characterized in axial stress-controlled constant amplitude and load increase tests as well as in rotating bending tests. The influence of different clinically relevant surface treatments (polishing, corundum grit blasting, thermal and anodic oxidizing) on the fatigue behaviour was investigated. All tests were realized in oxygen-saturated Ringer's solution. The cyclic deformation behaviour was characterized by mechanical hysteresis measurements. In addition, the change of the free corrosion potential and the corrosion current during testing in simulated physiological media indicated surface damages such as slip bands, intrusions and extrusions or finally microcracks. Microstructural changes on the specimen surfaces were examined by scanning electron microscopy (SEM).
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Hydrogen embrittlement and corrosion behaviors in metals · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Crystal structure of the surface oxide layer on titanium and its changes arising from immersion10.1002/jbm.820290111 ↗
2. Structure and composition of passive titanium oxide films10.1016/S0921-5107(97)00043-3 ↗
3. Passive film on orthopedic TiAlV alloy formed in physiological solution10.1016/S0142-9612(00)00145-9 ↗
4. The implant material Ti6Al7Nb: surface, microstructure, composition and properties
5. Anodic oxidation of titanium in 1m H2SO4, studied by Ruther-ford backscattering10.1016/0039-6028(93)90934-C ↗
6. Preparation of TiO2 layers on cp-Ti and Ti-6Al-4V by thermal and anodic oxidation and by sol–gel coating techniques and their characterisation10.1002/jbm.1212 ↗
7. Anodic plasma-chemical treatment of CP titanium surfaces for biomedical applications10.1016/S0142-9612(03)00560-X ↗
8. Effect of thermal oxidation on corrosion and corrosion-wear behaviour of a Ti-6Al-4V alloy10.1016/j.biomaterials.2003.10.009 ↗
9. Fatigue characteristics of bioactive glass-ceramic-coated Ti-29Nb-13Ta-4.6Zr for biomedical application10.1016/j.biomaterials.2003.09.108 ↗
10. The effect of sandblasting treatment on endurance properties of titanium alloy hip prostheses10.1046/j.1525-1594.2000.06486.x ↗
11. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
12. Fatigue crack initiation and fatigue life prediction of Ti-6Al-4V ELI
13. The cyclic deformation behaviour and fatigue induced surface damage of the implant alloy TiAl6Nb7 in simulated physiological media10.1016/j.ijfatigue.2004.01.001 ↗
14. Characterization of the cyclic deformation behaviour and fatigue crack initiation on titanium in physiological media by electrochemical techniques10.3139/146.017972 ↗
15. Corrosion monitoring system based on measurement and analysis of electrochemical noise10.5006/1.3293594 ↗
16. Use of electrochemical noise to detect stress corrosion crack initiation in simulated BWR environments10.1002/(SICI)1521-4176(199809)49:9<651::AID-MACO651>3.0.CO;2-M ↗
17. Localized corrosion and electrochemical noise analysis10.1002/1521-4176(200106)52:6<430::AID-MACO430>3.0.CO;2-3 ↗
18. Cyclic response—electrochemical Interaction in mono and polycrystalline AISI 316L stainless steel in H2SO4 solution, part I–III10.1016/0956-7151(93)90003-B ↗
19. Development of the electrochemical fatigue sensor
20. Cyclic deformation behaviour of (a+b) titanium alloys under complex mechanical and physiological loading conditions10.3139/146.020620 ↗
21. Longitudinal-optical phonons in TiO2 (rutile) thin-film spectra10.1103/PhysRevB.3.2086 ↗
22. Infrared reflection-absorption spectra of oxide films on titanium10.1016/0040-6090(76)90209-1 ↗
23. Structural and microstructural study of glasses in the LiO–TiO2–SiO2-system10.1007/BF01178435 ↗
24. Some physical properties of silicate glasses containing TiO2 in relation to their structure
25. Fatigue behaviour of shot peened TiAl6V4 in the temperature range 20°C<T<450°C
26. Optimizing of the bending fatigue behaviour of TiAl6V4 by shot peening
27. Characterization of mechanically induced surface damage on the implant alloy TiAl6Nb7 in quasi-physiological media10.1002/1521-4052(200208)33:8<442::AID-MAWE442>3.0.CO;2-K ↗